# US 2022/0010422 A1 · Dielectric film, method for producing same and optical member using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0010422 A1
- Document ID: US20220010422A1
- Status: Published application
- Kind: A1
- Application number: 17/312,925
- Filed: 2019-10-31
- Published: 2022-01-13
- Earliest claimed: 2018-12-21
- Assignees: Konica Minolta, Inc.
- Applicants: Konica Minolta, Inc.
- Inventors: Jinichi KASUYA; Kazunari TADA
- Web page: https://patentgrep.com/patent/US20220010422A1

## CPC

- C23C 14/10: Glass or silica
- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/081: {of aluminium, magnesium or beryllium}
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/221: {Ion beam deposition (C23C14/46, C23C14/48 take precedence)}
- C23C 14/30: by electron bombardment
- C23C 14/34: Sputtering
- G02B 1/113: using inorganic layer materials only
- G02B 1/115: Multilayers
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 1/16: having an anti-static effect, e.g. electrically conducting coatings
- G02B 1/18: Coatings for keeping optical surfaces clean, e.g. hydrophobic or photo-catalytic films (G02B1/16 takes precedence)
- G02B 27/0006: {with means to keep optical surfaces clean, e.g. by preventing or removing dirt, stains, contamination, condensation (G02B1/18 takes precedence; cleaning in general B08B)}
- G02B 2207/107: Porous materials, e.g. for reducing the refractive index
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A dielectric film is provided on a transparent substrate. The dielectric film has at least one low refractive index layer. An uppermost layer of the dielectric film contains SiO2 and has a film density of 92% or more. The uppermost layer contains an element having an electronegativity smaller than Si.

## Claims

### Claim 1

A dielectric film provided on a transparent substrate, wherein the dielectric film has at least one low refractive index layer, and an uppermost layer of the dielectric film contains SiO2 and has a film density of 92% or more, and the uppermost layer contains an element having an electronegativity smaller than Si.

### Claim 2 (depends on 1)

The dielectric film described in claim 1, wherein the uppermost layer contains an element selected from the group consisting of sodium, calcium, potassium and magnesium.

### Claim 3 (depends on 1)

The dielectric film described in claim 1, wherein a content of sodium, calcium, potassium, and magnesium in the uppermost layer is in the range of 0.5 to 10% by mass, and a layer thickness of the uppermost layer is 1 μm or less.

### Claim 4 (depends on 1)

The dielectric film described in claim 1, wherein the uppermost layer has a film density of 98% or more.

### Claim 5 (depends on 1)

The dielectric film described in claim 1, wherein a water contact angle of the uppermost layer is 30° or less after being stored for 1000 hours in an environment of 85° C. and 85% RH.

### Claim 6 (depends on 1)

The dielectric film described in claim 1, wherein a functional layer containing a metal oxide having a photocatalytic function as a main component is further provided on a transparent substrate side of the uppermost layer.

### Claim 7 (depends on 6)

The dielectric film described in claim 6, wherein the uppermost layer has a plurality of pores that partially expose a surface of the functional layer.

### Claim 8

A method of producing a dielectric film provided on a transparent substrate, comprising the steps of: forming at least one low refractive index layer; and forming an uppermost layer containing SiO2 and an element selected from the group consisting of sodium, calcium, potassium, and magnesium.

### Claim 9 (depends on 8)

The method of producing a dielectric film described in claim 8, further comprising the steps of: forming a functional layer containing a metal oxide having a photocatalytic function as a main component on a transparent substrate side of the uppermost layer; and forming a plurality of pores in the uppermost layer, the pores partially exposing a surface of the functional layer.

### Claim 10 (depends on 8)

The method of producing a dielectric film described in claim 8, comprising the step of forming the dielectric film by an ion assisted deposition method or a sputtering method.

### Claim 11 (depends on 1)

An optical member comprising the dielectric film described in claim 1.

### Claim 12 (depends on 11)

The optical member described in claim 11, wherein the optical member is an in-vehicle lens.