# US 2022/0010419 A1 · Multi-process hardening method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0010419 A1
- Document ID: US20220010419A1
- Status: Published application
- Kind: A1
- Application number: 17/473,814
- Filed: 2021-09-13
- Published: 2022-01-13
- Earliest claimed: 2016-09-16
- Applicants: Karsten Manufacturing Corporation
- Inventors: Matthew W. Simone
- Web page: https://patentgrep.com/patent/US20220010419A1

## CPC

- C22F 1/183: {of titanium or alloys based thereon}
- A63B 53/0416: {Heads having an impact surface provided by a face insert}
- A63B 53/042: {the face insert consisting of a material different from that of the head}
- C22C 14/00: Alloys based on titanium
- C22F 1/002: {by rapid cooling or quenching; cooling agents used therefor}
- A63B 53/0408: {characterised by specific dimensions, e.g. thickness}
- A63B 53/0466: {wood-type}
- A63B 53/047: {iron-type}
- A63B 2209/00: Characteristics of used materials
- B23K 10/02: Plasma welding
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

Embodiments of multi-process hardened golf club heads and methods of multi-process hardening of golf club heads are generally described herein. Other embodiments and methods may be described and claimed.

## Claims

### Claim 1

A method of a club head assembly, the method comprising:
(a) providing a golf club head having a recess, and providing a faceplate, wherein the golf club head and the faceplate are formed from an α-β Ti alloy, the α-β Ti alloy comprising between 5.5 wt % to 6.75 wt % aluminum (Al), between 3.5 wt % to 4.5 wt % vanadium (V), a maximum of 0.08 wt % carbon (C), a maximum of 0.03 wt % silicon (Si), a maximum of 0.3 wt % iron (Fe), a maximum of 0.2 wt % oxygen (O), a maximum of 0.015 wt % tin (Sn), and a trace of molybdenum (Mo);
(b) aligning the faceplate with the recess of the golf club head;
(c) welding the faceplate to the golf club head;
(d) heat treating the club head assembly to a temperature just below the β-transus temperature of the α-β Ti alloy for a predetermined amount of time;
(e) quenching the club head assembly to room temperature;
(f) aging the club head assembly to a temperature just below the Ti3Al solution temperature; and
(g) reducing the temperature of the club head assembly to room temperature by increments of at most 400° C. every hour.

### Claim 2 (depends on 1)

The method of claim 1, wherein the club head assembly of step (d) is heat treated in an α-β Ti alloy solution between 825° C. and 950° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the quenching of the club head assembly of step (e) comprises fluids selected from the group consisting of straight oils, water, water, water soluble fluid, micro-dispersion oils, and synthetic or semi-synthetic fluids.

### Claim 4 (depends on 1)

The method of claim 1, wherein the club head assembly of step (e) is quenched at a quenching rate of at least 550° C. per second.

### Claim 5 (depends on 1)

The method of claim 1, wherein the club head assembly of step (f) is aged by induction heat with induction heating coils.

### Claim 6 (depends on 1)

The method of claim 1, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in increments of at most 175° C. every hour.

### Claim 7 (depends on 1)

The method of claim 1, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in increments of at most 350° C. every hour.

### Claim 8 (depends on 1)

The method of claim 1, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in a time span range from 5 hours to 7 hours.

### Claim 9 (depends on 1)

The method of claim 1, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in a time span range from 2 hours to 6 hours.

### Claim 10 (depends on 1)

The method of claim 1, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in a time span range from 3 hours to 8 hours.

### Claim 11

A method of a club head assembly, the method comprising:
(a) providing a golf club head having a recess, and providing a faceplate, wherein the golf club head and the faceplate are formed from an α-β Ti alloy, the α-β Ti alloy comprising between 6 wt % Al, 6 wt % V, and 2 wt % Sn;
(b) aligning the faceplate with the recess of the golf club head;
(c) welding the faceplate to the golf club head;
(d) heat treating the club head assembly to a temperature just below the β-transus temperature of the α-β Ti alloy for a predetermined amount of time;
(e) quenching the club head assembly to room temperature
(f) aging the club head assembly to a temperature just below the Ti3Al solution temperature; and
(g) reducing the temperature of the club head assembly to room temperature by increments of at most 400° C. every hour.

### Claim 12 (depends on 11)

The method of claim 11, wherein the club head assembly of step (d) is heat treated in an α-β Ti alloy solution between 400° C. and 630° C.

### Claim 13 (depends on 11)

The method of claim 11, wherein the quenching of the club head assembly of step (e) comprises fluids selected from the group consisting of straight oils, water, water, water soluble fluid, micro-dispersion oils, and synthetic or semi-synthetic fluids.

### Claim 14 (depends on 11)

The method of claim 11, wherein the club head assembly of step (e) is quenched at a quenching rate of at least 2000° C. per second.

### Claim 15 (depends on 11)

The method of claim 11, wherein the club head assembly of step (f) is aged by induction heating with induction heating coils.

### Claim 16 (depends on 11)

The method of claim 11, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in increments of at most 125° C. every hour.

### Claim 17 (depends on 11)

The method of claim 11, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in increments of at most 275° C. every hour.

### Claim 18 (depends on 11)

The method of claim 11, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in a time span range from 5 hours to 7 hours.

### Claim 19 (depends on 11)

The method of claim 11, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in a time span range from 7 hours to 8 hours.

### Claim 20 (depends on 11)

The method of claim 11, wherein the temperature of the club head assembly of step (g) is reduced to room temperature in a time span range from 3 hours to 8 hours.