# US 2022/0010405 A1 · Method and device for producing direct reduced metal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0010405 A1
- Document ID: US20220010405A1
- Status: Published application
- Kind: A1
- Application number: 17/599,506
- Filed: 2020-03-31
- Published: 2022-01-13
- Earliest claimed: 2019-04-01
- Assignees: Greeniron H2 AB
- Applicants: Greeniron H2 AB
- Inventors: Hans MURRAY
- Web page: https://patentgrep.com/patent/US20220010405A1

## CPC

- C22B 5/12: by gases
- C21B 13/004: {in a continuous way by reduction from ores}
- C21B 13/0073: {Selection or treatment of the reducing gases}
- C21B 13/10: in hearth-type furnaces
- C21B 13/12: in electric furnaces
- C21B 2100/64: Controlling the physical properties of the gas, e.g. pressure or temperature
- C21B 2100/66: Heat exchange
- C21C 2100/04: Recirculation of the exhaust gas
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS

## Abstract

Method for producing direct reduced metal material, comprising the steps: a) charging metal material to be reduced into a furnace space (120); b) evacuating an existing atmosphere from the furnace space (120) so as to achieve an underpressure inside the furnace space (120); c) providing, in a main heating step, heat and hydrogen gas to the furnace space (120), so that heated hydrogen gas heats the charged metal material to a temperature high enough so that metal oxides present in the metal material are reduced, in turn causing water vapour to be formed; and d) condensing and collecting the water vapour formed in step c in a condenser (160) below the charged metal material; The invention is characterised in that said hydrogen gas in step c is provided without recirculation of the hydrogen gas, and in that the method further comprises the subse 15 quently performed step of removing the reduced metal material from the furnace space (120), and storing and/or transporting the reduced metal material under an inert atmosphere.

## Claims

### Claim 1

A method for producing direct reduced metal material, comprising the steps:
a) charging metal material to be reduced into a furnace space;
b) evacuating an existing atmosphere from the furnace space so as to achieve an underpressure inside the furnace space;
c) providing, in a main heating step, heat and hydrogen gas to the furnace space, so that heated hydrogen gas heats the charged metal material to a temperature high enough so that metal oxides present in the metal material are reduced, in turn causing water vapour to be formed; and
d) condensing and collecting the water vapour formed in step c in a condenser below the charged metal material;
wherein said hydrogen gas in step c is provided without recirculation of the hydrogen gas, and wherein the method further comprises the subsequently performed step of removing the reduced metal material from the furnace space, and storing and/or transporting the reduced metal material under an inert atmosphere.

### Claim 2 (depends on 1)

The method according to claim 1, wherein steps c and d are performed at least until a hydrogen atmosphere overpressure has been reached inside the furnace space, and wherein no hydrogen gas is evacuated from the furnace space until said overpressure has been reached.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the material charged in step a is at the most 50 tonnes, preferably at the most 25 tonnes, preferably between 5 and 10 tonnes of such material.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the method steps a-d are performed in a system provided directly at a mining site, whereby direct reduced metal material is produced at said mining site using said steps, thereafter packaged under a protecting atmosphere and thereafter transported to a different site for further processing.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the method further comprises cooling the charged material, after step d, by circulating said hydrogen gas past the charged material, whereby the hydrogen gas is heated by the charged material and cooled by heat exchange using a heat exchanger.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the cooling of the charged material is performed until the charged material reaches a temperature of below 100° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein said inert atmosphere is a nitrogen atmosphere.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the method further comprises the step of providing the reduced metal material into a first transport container which is filled with inert gas, wherein several such first transport containers are provided into a second transport container, in turn being filled with inert gas in the space surrounding said first transport containers.

### Claim 9 (depends on 1)

The method according to claim 1, wherein step c further comprises, in an initial heating step, providing heat and hydrogen gas to the furnace space, so that heated hydrogen gas heats the charged metal material to a temperature above the boiling temperature of water contained in the metal material, causing said contained water to evaporate.

### Claim 10 (depends on 1)

The method according to claim 1, wherein hydrogen gas to be provided in step c is preheated in a heat exchanger, which heat exchanger is arranged to transfer thermal energy from the evaporated water to the hydrogen gas to be provided in step c.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the main heating step of step c and the condensing in step d are performed until a predetermined pressure has been reached.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the main heating step in step c and the condensing in step d are performed until a steady state is reached, in terms of it no longer being necessary to provide more hydrogen gas in order to maintain a reached steady state gas pressure inside the furnace space.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the main heating step in step c and the condensing in step d are performed until the charged metal material to be reduced has reached a predetermined temperature.

### Claim 14 (depends on 1)

The method according to claim 1, wherein, during the performing of step c, there is a net flow downwards of water vapour through the charged metal material.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the method further comprises the steps of
e) after steps c and d are finished, cooling the hydrogen atmosphere to at the most 100° C.; and
f) after step e is finished, evacuating the hydrogen atmosphere from the furnace space and collecting the hydrogen gas of the evacuated hydrogen atmosphere.

### Claim 16 (depends on 1)

The method according to claim 1, wherein steps c and d are performed during at least 0.25 hours.