# US 2022/0010395 A1 · High surface compressive stress for through hardening

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0010395 A1
- Document ID: US20220010395A1
- Status: Published application
- Kind: A1
- Application number: 17/291,861
- Filed: 2019-04-12
- Published: 2022-01-13
- Earliest claimed: 2018-11-19
- Assignees: The Timken Company
- Applicants: The Timken Company
- Inventors: Mohan Chand Paladugu
- Web page: https://patentgrep.com/patent/US20220010395A1

## CPC

- C21D 9/40: for rings; for bearing races
- C21D 1/20: Isothermal quenching, e.g. bainitic hardening
- C21D 1/78: Combined heat-treatments not provided for above
- C21D 1/785: {Thermocycling}
- C21D 9/36: for balls; for rollers
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/008: Martensite
- F16C 2204/64: Medium carbon steel, i.e. carbon content from 0.4 to 0,8 wt%
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS

## Abstract

A heat treatment process for through hardening results in high surface compressive stresses. The method includes heating a steel component to a first temperature, quenching the steel component to a second temperature, maintaining the steel component at the second temperature for a first duration of time, heating the steel component to a third temperature, maintaining the steel component at the third temperature for a second duration of time, and quenching the steel component to a fourth temperature when austenite to martensite+bainite or bainite transformation is at least 10% but less than 85% complete.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A method of through hardening steel with at least 0.7% weight of carbon, the method comprising:
heating a steel component to a first temperature;
quenching the steel component to a second temperature;
maintaining the steel component at the second temperature for a first time interval;
heating the steel component to a third temperature;
maintaining the steel component at the third temperature for a second time interval; and
quenching the steel component to a fourth temperature when austenite to martensite+bainite or bainite transformation is at least 20% but less than 80% complete;
wherein the steel component, after quenching to the fourth temperature, has a residual compressive stress of at least 100 MPA in a surface region of the steel component and
wherein the steel component, after quenching to the fourth temperature, includes at least 20% retained austenite.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first temperature is 800 degrees Celsius to 1100 degrees Celsius.

### Claim 16 (depends on 14)

The method of claim 14, wherein the second temperature is from 0.6 times a martensite start temperature to 1.2 times the martensite start temperature.

### Claim 17 (depends on 14)

The method of claim 14, wherein the third temperature is greater than the second temperature by at least 5 degrees Celsius.

### Claim 18 (depends on 17)

The method of claim 17, wherein the third temperature is greater than the second temperature by no more than 200 degrees Celsius.

### Claim 19 (depends on 14)

The method of claim 14, wherein the fourth temperature is equal to or less than 100 degrees Celsius.

### Claim 20 (depends on 14)

The method of claim 14, wherein first time interval is from 20 minutes to 180 minutes.

### Claim 21

(canceled)

### Claim 22 (depends on 14)

The method of claim 14, wherein the second time interval is from 20 minutes to 180 minutes.

### Claim 23

(canceled)

### Claim 24 (depends on 14)

The method of claim 14, further including tempering the steel component after quench to the fourth temperature by reheating the steel component to a fifth temperature of 100 degrees Celsius to 350 degrees Celsius and quenching the component to an ambient temperature.

### Claim 25 (depends on 14)

The method of claim 14, wherein the steel component, after quenching to the fourth temperature, has a through hardness of at least 50 HRC.

### Claim 26 (depends on 14)

The method of claim 14, further comprising tempering the steel component after quenching to the fourth temperature, and wherein the steel component, after tempering, has a through hardness of at least 50 HRC.

### Claim 27 (depends on 14)

The method of claim 14, wherein the steel component, after quenching to the fourth temperature, has a microstructure of at least 30% martensite in a surface region of the steel component and a microstructure of at least 30% bainite in a core of the steel component.

### Claim 28

(canceled)

### Claim 29 (depends on 14)

The method of claim 14, wherein the steel component is quenched to the fourth temperature when austenite to martensite+bainite or bainite transformation is at least 20% but less than 65% complete.

### Claim 30

A steel component comprising a surface, a core, and a surface region extending from the surface toward the core to a depth up to 1000 micrometers below the surface:
an overall microstructure of the steel component including at least 20% retained austenite;
the core of the steel component having a microstructure including at least 30% bainite; and
the surface region of the steel component having a microstructure including at least 30% martensite, and wherein a through hardness of the steel component is at least 50 HRC;
wherein the surface region has a residual compressive stress of at least 100 MPa.

### Claim 31 (depends on 30)

The steel component of claim 30, wherein the microstructure of the steel component includes less than 40% retained austenite.

### Claim 32 (depends on 30)

The steel component of claim 30, wherein the core has a microstructure of at least 50% bainite.

### Claim 33 (depends on 30)

The steel component of claim 30, wherein the surface region has a microstructure of at least 50% martensite.

### Claim 34

(canceled)

### Claim 35 (depends on 30)

The steel component of claim 30, wherein the microstructure between the surface region and the core is graded such that the microstructure gradually transforms from at least 30% martensite at the surface to at least 30% bainite at the core.

### Claim at position 24

36-41. (canceled)