# US 2022/0010393 A1 · Gradient steel material having surface layer with ferrite and inner layer with ferrite + pearlite and manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0010393 A1
- Document ID: US20220010393A1
- Status: Published application
- Kind: A1
- Application number: 17/413,781
- Filed: 2019-12-27
- Published: 2022-01-13
- Earliest claimed: 2018-12-28
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Suoquan ZHANG; Sihai JIAO; Jianhua DING; Xiaojun LIANG
- Web page: https://patentgrep.com/patent/US20220010393A1

## CPC

- C21D 1/28: Normalising
- C21D 8/0247: characterised by the heat treatment
- C21D 1/84: Controlled slow cooling (cooling-beds for metal rolling B21B43/00)
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C21D 2211/005: Ferrite
- C21D 2211/009: Pearlite
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are a gradient steel material having a surface layer with ferrite and an inner layer with ferrite+pearlite, and a manufacturing method, the weight percentages of the components are: C≤0.15%, Si≤1%, Mn≤1.5%, the balance of Fe and inevitable impurities, and the surface layer of the steel material is ferrite, the inner layer is ferrite+pearlite. The manufacturing method thereof includes: smelting, casting, rolling, heat treatment; wherein, in the heat treatment step, the steel material is heated above the austenitizing temperature Ac3, and hold at the temperature more than 3 min to ensure that the material is completely austenitized; subsequently, it is cooled to a temperature below Ar1 at a cooling rate lower than 0.5° C./s. The present steel material does not need to be obtained by means of the compound preparation of different materials, and is only processed and prepared by a single material, the process is short, the procedure is simple, and the cost is low.

## Claims

### Claim 1

A gradient steel material having a surface layer with ferrite and an inner layer with ferrite+pearlite, comprising the following components in percentage by weight: 0<C≤0.15%, 0<Si≤1%, 0<Mn≤1.5%, and the balance of Fe and inevitable impurities, the surface layer of the gradient steel material is a ferrite with good plasticity, and the inner layer is a ferrite+pearlite.

### Claim 2 (depends on 1)

The gradient steel material having a surface layer with ferrite and an inner layer with ferrite+pearlite according to claim 1, characterized in that the surface layer of the gradient steel material is a ferrite with a carbon content not higher than 0.02 wt %; and the carbon content of the surface layer of the gradient steel material is lower than the carbon content of the inner layer of the gradient steel material.

### Claim 3 (depends on 1)

A manufacturing method of a gradient steel material having a surface layer with ferrite and an inner layer with ferrite+pearlite according to claim 1, characterized by including: smelting, casting, rolling and heat treatment; wherein in the heat treatment step, a steel material is heated above the austenitizing temperature Ac3, and the temperature is kept above 3 min to ensure that the material is completely austenitized; and subsequently, it is cooled to a temperature below Ar1 at a cooling rate of less than 0.5° C./s.