# US 2022/0009853 A1 · Gas generant composition, preparation method therefor, and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0009853 A1
- Document ID: US20220009853A1
- Status: Published application
- Kind: A1
- Application number: 17/478,013
- Filed: 2021-09-17
- Published: 2022-01-13
- Earliest claimed: 2020-05-15
- Assignees: Hubei Hangpeng Chemical Power Technology Co., Ltd.
- Applicants: Hubei Hangpeng Chemical Power Technology Co., Ltd.
- Inventors: Yunqiang LUO; Xiangning REN; Tao DU; Jun ZHANG; Xiaochen SHEN
- Web page: https://patentgrep.com/patent/US20220009853A1

## CPC

- C06D 5/06: by reaction of two or more solids
- B60R 21/2644: {using only solid reacting substances, e.g. pellets, powder}
- C06B 29/22: the salt being ammonium perchlorate
- C06B 31/00: Compositions containing an inorganic nitrogen-oxygen salt
- C06D: MEANS FOR GENERATING SMOKE OR MIST; GAS-ATTACK COMPOSITIONS; GENERATION OF GAS FOR BLASTING OR PROPULSION (CHEMICAL PART) (fuels C10)
- B60R: VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISE PROVIDED FOR
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})

## Abstract

Provided are a gas generant composition, a preparation method, and a gas generator containing the composition. The gas generant composition includes components having the following contents, in percent by mass: 40% to 60% of guanidine nitrate, 25% to 50% of basic copper nitrate, 0% to 7% of ammonium perchlorate, 1% to 10% of a slag-forming agent, and 0.05% to 5% of a release agent/lubricant, the slag-forming agent is used as a form-retaining agent, so that the tablets can retain their form before combustion very well after combustion, thereby completely avoiding burning of an inflatable bag due to melting and splashing of the combusted tablets. Moreover, ammonium perchlorate is used as auxiliary oxidizers, thereby reducing the amount of basic cupric nitrate used and reducing molten copper residues. The gas generant composition is mainly used in a gas generator for vehicle airbag.

## Claims

### Claim 1

A gas generant composition, comprising guanidine nitrate, basic copper nitrate and ammonium perchlorate, further comprising a slag-forming agent and a lubricant, wherein the slag-forming agent is at least one zirconate, at least one silicate or a mixture of at least one zirconate and at least one silicate,
wherein contents, in percent by mass, of respective components are as follows:
guanidine nitrate
40% to 60%;
basic copper nitrate
25% to 50%;
ammonium perchlorate
0% to 7%;
slag-forming agent
1% to 10%;
and
lubricant
0.05% to 5%.

### Claim 2 (depends on 1)

The gas generant composition according to claim 1, wherein the zirconate is one of strontium zirconate, barium zirconate and calcium zirconate, or a combination therefrom.

### Claim 3 (depends on 1)

The gas generant composition according to claim 1, wherein the silicate is one of zirconium silicate and calcium silicate, or a combination therefrom.

### Claim 4 (depends on 1)

The gas generant composition according to claim 1, wherein the slag-forming agent is the mixture of at least one zirconate and at least one silicate, in which a mass ratio of zirconate to silicate is 1:0.5-3.

### Claim 5 (depends on 4)

The gas generant composition according to claim 4, wherein the slag-forming agent is a mixture of strontium zirconate, zirconium silicate and calcium silicate in a mass ratio of 1:0.2-1.5:0.3-1.5.

### Claim 6 (depends on 1)

The gas generant composition according to claim 1, wherein the slag-forming agent is a mixture of strontium zirconate and barium zirconate in a mass ratio of 1:0.5-3.

### Claim 7 (depends on 1)

The gas generant composition according to claim 1, wherein the lubricant is one of talc, graphite, calcium stearate, magnesium stearate, molybdenum disulfide and boron nitride, or a combination therefrom.

### Claim 8 (depends on 1)

The gas generant composition according to claim 1, wherein the ammonium perchlorate has a particle size D90 not greater than 20 μm; and the slag-forming agent has a particle size D90 not greater than 5 μm.

### Claim 9 (depends on 1)

The gas generant composition according to claim 1, wherein the basic copper nitrate and the lubricant each have a particle size D90 not greater than 5 μm.

### Claim 10 (depends on 1)

The gas generant composition according to claim 1, wherein a sum of water contents in the respective components of the gas generant composition is not more than 1 of a total mass of the respective components.

### Claim 11 (depends on 1)

The gas generant composition according to claim 1, wherein the gas generant composition is molded as a circular or elliptical sheet structure, a circular or elliptical columnar structure, a special-shaped sheet or columnar structure, a circular or elliptical monoporous structure, a circular or elliptical porous structure, or a special-shaped monoporous or porous structure.

### Claim 12 (depends on 11)

The gas generant composition according to claim 11, wherein the circular sheet structure has a diameter of 3 to 15 mm and a height of 2 to 5 mm; the circular columnar structure has a diameter of 3 to 15 mm and a height of 5 to 15 mm; the circular monoporous structure has an inner diameter of 0.5 to 2.5 mm, an outer diameter of 3 to 15 mm and a height of 3 to 15 mm; and the elliptical monoporous structure has an inner diameter of 0.5 to 2.5 mm, a major diameter of 3 to 20 mm, a minor diameter of 2 to 12 mm and a height of 3 to 15 mm.

### Claim 13 (depends on 1)

A method for preparing the gas generant composition according to claim 1, wherein the gas generant composition is prepared by wet granulation, spray granulation or dry granulation, wherein a preparation method for the wet granulation comprises steps of:
(1) mixing guanidine nitrate, basic copper nitrate, ammonium perchlorate and the slag-forming agent to obtain a first material;
(2) performing wet mixing on the first material by adding water, to obtain a second material, wherein an amount of water added is 5% to 15% of a total mass of the first material;
(3) making the second material pass through a sieve of 10 to 40 meshes to obtain a third material;
(4) drying the third material to a water content less than 0.5% of a total mass of the third material, and making the third material pass through a sieve of 10 to 40 meshes again to obtain a fourth material; and
(5) adding a lubricant to the fourth material and molding the material.

### Claim 14 (depends on 13)

The method for preparing the gas generant composition according to claim 13, wherein in the step (1), the first material is obtained by mixing guanidine nitrate, basic copper nitrate, ammonium perchlorate and the slag-forming agent in a mixing device for a mixing duration larger than or equal to 5 min.

### Claim 15 (depends on 13)

The method for preparing the gas generant composition according to claim 13, wherein the wet mixing in the step (2) is performed for a duration of 20 min to 60 min; and the wet mixing is performed by a device selected from a kneader and a mixer.

### Claim 16 (depends on 1)

A method for preparing the gas generant composition according to claim 1, wherein the gas generant composition is prepared by wet granulation, and a preparation method comprises steps of:
(1) mixing guanidine nitrate, basic copper nitrate, ammonium perchlorate, the slag-forming agent and the lubricant to obtain a first material;
(2) performing wet mixing on the first material by adding water, to obtain a second material, wherein an amount of water added is 5% to 15% of a total mass of the first material;
(3) making the second material pass through a sieve of 10 to 40 meshes to obtain a third material;
(4) drying the third material to a water content less than 0.5% of a total mass of the third material, and making the third material pass through a sieve of 10 to 40 meshes again to obtain a fourth material; and
(5) molding the fourth material.

### Claim 17 (depends on 16)

The method for preparing the gas generant composition according to claim 16, wherein in the step (1), the first material is obtained by mixing guanidine nitrate, basic copper nitrate, ammonium perchlorate, the slag-forming agent and the lubricant in a mixing device for a mixing duration larger than or equal to 5 min.

### Claim 18 (depends on 16)

The method for preparing the gas generant composition according to claim 16, wherein the wet mixing in the step (2) is performed for a duration of 20 min to 60 min; and the wet mixing is performed by a device selected from a kneader and a mixer.

### Claim 19 (depends on 1)

The gas generant composition according to claim 1, wherein the zirconate is barium zirconate.

### Claim 20 (depends on 1)

The gas generant composition according to claim 1, wherein the basic copper nitrate has a specific surface area of 1.0-8.0 m2/g.