# US 2022/0009830 A1 · Production method of chemically strengthened glass, and chemically strengthened glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0009830 A1
- Document ID: US20220009830A1
- Status: Published application
- Kind: A1
- Application number: 17/487,421
- Filed: 2021-09-28
- Published: 2022-01-13
- Earliest claimed: 2018-01-19
- Assignees: AGC Inc.
- Applicants: Agc Inc.
- Inventors: Izuru KASHIMA; Kaname SEKIYA; Akio SHIZUKAI; Yositeru IKEDA; Shogo SUEDA
- Web page: https://patentgrep.com/patent/US20220009830A1

## CPC

- C03C 3/095: containing rare earths
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/093: containing zinc or zirconium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention relates to a method for producing a chemically strengthened glass, the method including, performing a chemical strengthening treatment including the following steps (1) to (3) to a glass having a specific composition, (1) a step of bringing the glass into contact with an inorganic salt composition including 70 mass % or more of potassium nitrate to perform ion exchange; (2) a step of bringing the glass having been ion-exchanged in step (1) into contact with an inorganic salt composition including 50 mass % or more of sodium nitrate to perform ion exchange; and (3) a step of bringing the glass having been ion-exchanged in step (2) into contact with an inorganic salt composition including 70 mass % or more of potassium nitrate to perform ion exchange.

## Claims

### Claim at position 1

1: A method for producing a chemically strengthened glass, the method comprising
(1) contacting a glass with an inorganic salt composition comprising 70 mass % or more of potassium nitrate to perform ion exchange;
(2) contacting the glass obtained in (1) with an inorganic salt composition comprising 50 mass % or more of sodium nitrate to perform ion exchange; and
(3) contacting the glass obtained in (2) with an inorganic salt composition comprising 70 mass % or more of potassium nitrate to perform ion exchange,
wherein the glass comprises, in mole percentage based on oxides, from 50 to 80% of SiO2, from 2 to 25% of Al2O3, from 0.1 to 20% of Li2O, from 0.1 to 18% of Na2O, from 0 to 10% of K2O, from 0 to 15% of MgO, from 0 to 5% of CaO, from 0 to 5% of P2O5, from 0 to 6% of B2O3, from 0 to 5% of Y2O3, and from 0 to 5% of ZrO2.

### Claim at position 2 (depends on 1)

2: The method of claim 1, satisfying at least one of the following (a1) to (a3):
(a1) in (1), the contact between the glass and the inorganic salt composition is performed at 350 to 480° C. for 0.5 to 20 hours;
(a2) in (2), the contact between the glass and the inorganic salt composition is performed at 340 to 480° C. for 0.5 to 20 hours; and
(a3) in (3), the contact between the glass and the inorganic salt composition is performed at 350 to 480° C. for 0.5 to 20 hours.

### Claim at position 3 (depends on 1)

3: The method of claim 1, satisfying at least one of the following (b1) to (b3):
(b1) the inorganic salt composition in (1) is an inorganic salt composition comprising 80 mass % or more of potassium nitrate;
(b2) the inorganic salt composition in (2) is an inorganic salt composition comprising 65 mass % or more of sodium nitrate; and
(b3) the inorganic salt composition in (3) is an inorganic salt composition comprising 80 mass % or more of potassium nitrate.

### Claim at position 4 (depends on 1)

4: The method of claim 1, satisfying at least one of the following (c1) to (c3):
(c1) in (1), the contact between the glass and the inorganic salt composition is performed at 360 to 470° C.;
(c2) in (2), the contact between the glass and the inorganic salt composition is performed at 350 to 470° C.; and
(c3) in (3), the contact between the glass and the inorganic salt composition is performed at 360 to 470° C.

### Claim at position 5 (depends on 1)

5: The method of claim 1, satisfying at least one of the following (d1) to (d3):
(d1) in (1), the contact between the glass and the inorganic salt composition is performed for 0.5 to 15 hours;
(d2) in (2), the contact between the glass and the inorganic salt composition is performed for 1 to 15 hours; and
(d3) in (3), the contact between the glass and the inorganic salt composition is performed for 0.5 to 15 hours.

### Claim at position 6 (depends on 1)

6: The method of claim 1, wherein:
Na ion is ion-exchanged with K ion in (1);
Li ion is ion-exchanged with Na ion in (2); and
Na ion is ion-exchanged with K ion in (3).