# US 2022/0009022 A1 · Joining method and joined body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0009022 A1
- Document ID: US20220009022A1
- Status: Published application
- Kind: A1
- Application number: 17/413,680
- Filed: 2019-12-13
- Published: 2022-01-13
- Earliest claimed: 2018-12-21
- Assignees: NHK Spring Co., Ltd.
- Applicants: NHK Spring Co., Ltd.
- Inventors: Toshihiko Hanamachi; Daisuke Fujino; Masaru Takimoto; Yoshihito Araki; Masahiro Fujii
- Web page: https://patentgrep.com/patent/US20220009022A1

## CPC

- B23K 20/02: by means of a press {; Diffusion bonding}
- B23K 20/023: {Thermo-compression bonding}
- B23K 20/002: {specially adapted for particular articles or work (B23K20/129 takes precedence)}
- B23K 20/2336: {both layers being aluminium}
- B23K 2101/14: Heat exchangers
- B23K 2103/10: Aluminium or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A joining method of joins a main body and a cover, the main body being a flat plate and made of aluminum or an aluminum alloy and including a passage through which a medium for promoting heat exchange is circulated, and the cover being a flat plate and made of aluminum or an aluminum alloy and configured to cover the passage of the main body. The method includes: a covering step of covering the main body with the cover; and a diffusion bonding step of joining the main body and the cover by diffusion bonding under a condition in which a joining temperature is 500° C. or higher and 640° C. or lower, and a joining surface pressure is 0.7 MPa or higher. Each of a joining surface of the main body and a joining surface of the cover has a flatness of 0.2 or less.

## Claims

### Claim at position 1

1-5. (canceled)

### Claim 6

A joining method of joining a main body and a cover, the main body being a flat plate and made of aluminum or an aluminum alloy and including a passage through which a medium for promoting heat exchange is circulated, and the cover being a flat plate and made of aluminum or an aluminum alloy and configured to cover the passage of the main body, the method comprising:
a covering step of covering the main body with the cover; and
a diffusion bonding step of joining the main body and the cover by diffusion bonding under a condition in which a joining temperature is 500° C. or higher and 640° C. or lower, and a joining surface pressure is 0.7 MPa or higher,
wherein each of a joining surface of the main body and a joining surface of the cover has a flatness of 0.2 or less.

### Claim 7 (depends on 6)

The joining method according to claim 6, wherein each of a joining surface of the main body and a joining surface of the cover has a surface roughness greater than zero and equal to or less than Ra 0.4.

### Claim 8

A joined body comprising:
a main body made of aluminum or an aluminum alloy and including a passage through which a medium for promoting heat exchange is circulated, the main body being a flat plate; and
a cover made of aluminum or an aluminum alloy and configured to cover the passage of the main body, the cover being a flat plate, wherein
each of a joining surface of the main body and a joining surface of the cover has a flatness of 0.2 or less, and
the main body and the cover are diffusion-joined.

### Claim 9 (depends on 8)

The joined body according to claim 8, wherein the main body and the cover are made of aluminum alloy No. 6061, and have a tensile strength of 125 MPa or greater.