# US 2022/0008983 A1 · Process for making an erosion and wear resistant shot chamber for die casting application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0008983 A1
- Document ID: US20220008983A1
- Status: Published application
- Kind: A1
- Application number: 16/926,714
- Filed: 2020-07-12
- Published: 2022-01-13
- Earliest claimed: 2020-07-12
- Assignees: Qingyou Han
- Inventors: Qingyou Han
- Web page: https://patentgrep.com/patent/US20220008983A1

## CPC

- B22C 9/061: {Materials which make up the mould}
- B22D 17/10: with horizontal press motion
- B22D 17/2023: {Nozzles or shot sleeves}
- B22D 17/203: {Injection pistons (B22D17/2053 takes precedence; for plastics B29C45/53)}
- B22D 17/2209: {Selection of die materials (for permanent moulds B22C9/061)}
- B22D 17/229: {with exchangeable die part (B22D17/2245 takes precedence)}
- B22D 17/30: Accessories for supplying molten metal, e.g. in rations (supplying molten metal in ration in general B22D39/00)
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/12: Aluminium or alloys based thereon
- C23C 2/32: using vibratory energy applied to the bath or substrate (C23C2/14 takes precedence)
- C23C 6/00: Coating by casting molten material on the substrate
- C23C 10/44: Siliconising
- C23C 10/48: Aluminising
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- B22C 9/06: Permanent moulds for shaped castings (moulds for ingots B22D7/06)
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A process of forming an erosion, oxidation, and wear resistant shot chamber, either a gooseneck or a shot sleeve, is provided. The process utilizes a self-healing erosive wear resistant coating on a liner of refractory metal to serve as the working surfaces of a shot chamber. Such a shot chamber is expected to have an improved service life for die casting of corrosive metals and alloys, including hot chamber die casting of aluminum alloys. An improved hot dipping process using stirring in the motel metal bath is also disclosed.

## Claims

### Claim 1

A method for forming an erosion, oxidation, and wear resistant composite die casting shot chamber, the method comprising of the steps of:
preparing a liner made of refractory metallic materials with melting temperatures higher than 1600° C.;
coating the liner with a self-healing coating which has a metallurgical bond to the liner, wherein the coating is also capable of promoting the formation of a metallurgical bond between ferrous alloy and the liner in a casting process;
placing the coated liner in a mold cavity and using it as a core for forming the working surfaces of the shot chamber;
pouring a ferrous liquid alloy into the mold cavity to bond the coated liner with a metallurgical bond and to form a solid composite shot chamber after the liquid alloy is solidified on the coated liner;
machining the solid composite shot chamber to its final dimensions; and
covering the outside surfaces of the ferrous alloy with a conventional thick coating used in the casting industry.

### Claim 2 (depends on 1)

A method of claim 1, wherein the shot chamber includes, but is not limited to gooseneck, shot sleeve, and components that are associated with the shot chamber such as plunger, ram, nozzle, and die insert.

### Claim 3 (depends on 1)

A method of claim 1, wherein the refractory metallic material is niobium, molybdenum, rhenium, tantalum, titanium, tungsten, or its alloy.

### Claim 4 (depends on 1)

A method of claim 1, wherein the said coating on the liner is an aluminizing coating using hot plating, cementation-packing, laser-printing, thermal spring, arc surface alloying, or other techniques.

### Claim 5 (depends on 1)

A method of claim 1, wherein the said coating on the liner is a silicide coating.

### Claim 6

A method of claim, 1 wherein the said coating on the liner is a zinc coating.

### Claim 7 (depends on 1)

A method of claim 1, wherein the said coating on the liner is an oxidation resistant coating conventionally used for protecting a refractory metal from oxidation.

### Claim 8 (depends on 1)

A method of claim 1, wherein the coating on the liner is a carbide, nitride, silicide, or a TiAlN type of coating that can be applied using a physical vapor deposition process or a chemical vapor deposition process.

### Claim 9 (depends on 1)

A method of claim 1, wherein the said ferrous alloy is cast iron.

### Claim 10 (depends on 1)

A method of claim 1, wherein the said ferrous alloy is steel.

### Claim 11 (depends on 1)

A method of claim 1, wherein the coating covering the outside surfaces of the ferrous alloy can also be part of the liner that is placed in the mold cavity to form the surfaces of the shot chamber contacting molten metal during die casting process.

### Claim 12

A method for forming an erosion, oxidation, and wear resistant composite shot chamber for die casting processes, the method comprising the steps of:
preparing a refractory metal liner in the form of a tube coated with a layer of oxidation resistant coating;
coating the outer surface of the coated refractory metal tube with a solder material;
preparing a ferrous alloy shot chamber and heating it up to desired temperatures; and
shrink fitting the shot chamber on the liner tube while the heat of the shot chamber melts the said solder material and bond the shot chamber with the liner tube.

### Claim 13 (depends on 12)

A method of claim 12, wherein the refractory metallic material is niobium, molybdenum, rhenium, tantalum, titanium, tungsten, or its alloy.

### Claim 14 (depends on 12)

A method of claim 12, wherein the solder material is, but is not limited to, a metallic solder that has its melting temperature higher than 500° C.

### Claim 15 (depends on 12)

A method of claim 12, wherein the inside diameter of the ferrous alloy shot chamber is slightly larger than the outside diameter of the coated liner at the said desired temperatures but is smaller than the outside diameter of the coated liner at room temperatures.

### Claim 16

A method for coating a solid metallic article with a layer of intermetallic compounds from a molten metallic material, the method comprising the steps of:
preparing a solid article with clean surfaces;
preparing a metallic bath at a temperature at least 20° C. higher than the liquidus of the material;
submerging the solid article in a molten metallic bath;
stiffing the molten metallic bath to enhance the chemical reaction between the material of the solid article and the molten metallic material at their interfaces; and
removing the solid article out of the metallic bath after a layer of intermetallic phases have been formed on the solid article.

### Claim 17 (depends on 16)

A method of claim 16, wherein the stiffing is caused by using a plurality of sonotrodes submerged in the bath with each sonotrode vibrating at a frequency in the range of about 15 kHz to about 80 kHz and power in the range of 100 to 100,000 watts.

### Claim 18 (depends on 16)

A method of claim 16, wherein the stiffing is caused by mechanical means including using a plurality of stirrers.

### Claim 19 (depends on 16)

A method of claim 16, wherein the stiffing is caused by a physical alternating or pulsed field such as an electrical, magnetic, electromagnetic field.

### Claim 20 (depends on 16)

A method according to claim 16 wherein the molten bath comprises of a metallic metal or its alloy with melting temperatures lower than 1100° C., including an aluminum alloy bath.