# US 2021/0363610 A1 · Nano dispersion copper alloy with high air-tightness and low free oxygen content and brief manufacturing process thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0363610 A1
- Document ID: US20210363610A1
- Status: Published application
- Kind: A1
- Application number: 16/627,979
- Filed: 2019-03-15
- Published: 2021-11-25
- Earliest claimed: 2019-01-29
- Assignees: Central South University
- Applicants: Central South University
- Inventors: Zhou Li; Wenting Qiu; Zhu Xiao; Shen Gong
- Web page: https://patentgrep.com/patent/US20210363610A1

## CPC

- C22C 1/0425: {Copper-based alloys}
- B22F 3/172: {Continuous compaction, e.g. rotary hammering (with axial pressure and without reduction of section B22F3/204)}
- B22F 3/20: by extruding
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- B22F 9/22: using gaseous reductors
- C22C 1/05: Mixtures of metal powder with non-metallic powder (C22C1/08 takes precedence)
- C22C 1/1078: {by internal oxidation of material in solid state}
- C22C 9/00: Alloys based on copper
- C22C 32/0021: {Matrix based on noble metals, Cu or alloys thereof}
- B22F 2009/043: {by ball milling}
- B22F 2301/10: Copper
- B22F 2302/253: Aluminum oxide (Al2O3)
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

Disclosed is a nano dispersion copper alloy with high air-tightness and low free oxygen content and a brief manufacturing process thereof, wherein alloy comprises the following components: Al2O3, Ca and La. The manufacturing process comprises the following steps of: preparing Cu—Al2O3 alloy powder by an internal oxidation method; mixing the Cu—Al2O3 alloy powder with Cu—Ca—La alloy powder; sheathing the mixed powder under protection of argon; performing hot extrusion and then rotary forging; vacuumizing the sheath after the rotary forging; and sealing and placing the sheath in a nitrogen atmosphere with a temperature of 450° C. to 550° C. and a pressure intensity of 40 Mpa to 60 Mpa for 3 hours to 5 hours. The dispersion copper prepared by the present disclosure has the advantages of low free oxygen content (≤15 ppm), high dimensional stability, good air-tightness and an air leakage rate≤1.0×10−10 Pa m3/s after hydrogen annealing.

## Claims

### Claim 1

A nano dispersion copper alloy with high air-tightness and low free oxygen content, comprising the following components in percentage by mass:
0.05 wt. % to 1.61 wt. % of Al2O3,
0.008 wt. % to 0.012 wt. % of Ca,
0.008 wt. % to 0.012 wt. % of La, and the balance of Cu.

### Claim 2

A brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content, comprising the following steps of: preparing Cu—Al2O3 alloy powder by an internal oxidation method; mixing the Cu—Al2O3 alloy powder with Cu—Ca—La alloy powder; sheathing the mixed powder under protection of argon; performing hot extrusion at 900° C. to 920° C. and then rotary forging; vacuumizing the sheath to be less than or equal to 10−3 Pa after the rotary forging; and sealing and placing the sheath in a nitrogen atmosphere with a temperature ranging from 450° C. to 550° C. and a pressure intensity ranging from 40 Mpa to 60 Mpa for 3 hours to 5 hours.

### Claim 3 (depends on 2)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 2, wherein the internal oxidation method for preparing the Cu—Al2O3 alloy powder comprises the following steps of:
first step: powder preparation
smelting Al and Cu to prepare a Cu—Al alloy melt with an Al content of 0.03 wt. % to 0.8 wt. %, and atomizing the melt to prepare powder;
second step: ball-milling activation
mixing the powder prepared in the first step with an oxidant for ball-milling activation;
third step: graded internal oxidation
performing two-grade internal oxidation on the mixture obtained in the second step at 380° C. to 400° C. and 880° C. to 900° C. in a protective atmosphere; and
fourth step: reduction
crushing the internally oxidized powder obtained in the third step and then reducing with hydrogen to obtain the Cu—Al2O3 alloy powder.

### Claim 4 (depends on 3)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 3, wherein in the first step, a smelting temperature of the alloy is 1200° C. to 1230° C.; and the alloy melt is pulverized by pure nitrogen atomization, and a purity of nitrogen is more than or equal to 99.9%.

### Claim 5 (depends on 3)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 3, wherein in the second step, alloy powder with a particle diameter less than 40 meshes is mixed with the oxidant for ball-milling; an addition amount of the oxidant accounts for 0.5 wt % to 9.5 wt % of a mass of the alloy powder; and a ball-milling process is as follows: a ratio of ball and material is 3:1 to 10:1, a rotating speed is 50 rpm to 300 rpm, a ball milling time is 120 minutes to 600 minutes, and an atmosphere is air.

### Claim 6 (depends on 3)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 3, wherein in the third step, parameters of the internal oxidation process are as follows: the ball-milled powder is heated to 380° C. to 400° C. in an argon or nitrogen atmosphere and held for 2 hours to 4 hours, and then the ball-milled power is continuously heated to 880° C. to 900° C. and held for 2 hours to 4 hours.

### Claim 7 (depends on 3)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 3, wherein in the fourth step, the internally oxidized powder is sieved through a 40-mesh sieve after crushing, and the sieved powder is heated to 880° C. to 900° C. and reduced by hydrogen for 4 hours to 8 hours.

### Claim 8 (depends on 2)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 2, wherein the preparation method of the Cu—Ca—La alloy powder comprises the following steps of: heating and smelting Cu, Cu—Ca intermediate alloy and La to prepare a Cu—Ca—La alloy melt with a Ca content of 0.08 wt. % to 0.12 wt. % and a La content of 0.08 wt. % to 0.12 wt. %; atomizing the melt with high-purity nitrogen to prepare powder; sieving the powder with a 200-mesh sieve; and performing ball-milling on the sieved powder until a particle diameter of the powder is less than 20 microns to obtain superfine powder; wherein a purity of the high-purity nitrogen is more than or equal to 99.9%.

### Claim 9 (depends on 2)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according to claim 2, wherein the Cu—Ca—La alloy powder and the Cu—Al alloy powder prepared by the internal oxidation method are mixed according to a mass ratio ranging from 1:10 to 1:15, subjected to cold isostatic pressing, sheathed by pure copper in an argon chamber, subjected to water sealing and hot extrusion at 900° C. to 920° C., with an extrusion ratio greater than or equal to 15, then subjected to rotary forging after extrusion; a rotationally forged bar is placed in a new sheath, then the sheath is vacuumized to 10−3 Pa, sealed, and placed in a nitrogen atmosphere with a pressure intensity ranging from 40 Mpa to 60 Mpa at 450° C. to 550° C. for 3 hours to 5 hours.

### Claim 10 (depends on 9)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according claim 9, wherein the prepared nano dispersion copper alloy has a tensile strength of 330 MPa to 580 MPa at room temperature, an electric conductivity greater than 80% to 97% of IACS, a free oxygen content less than or equal to 15 ppm, and an air leakage rate less than or equal to 1.0×10−10 Pa m3/s.

### Claim 11 (depends on 9)

The brief manufacturing process of the nano dispersion copper alloy with high air-tightness and low free oxygen content according claim 9, wherein the diameter of prepared nano dispersion copper alloy of φ20 mm is changed by 0.00 μm before and after annealing with hydrogen at 900° C. for 1 hour through measurement by a spiral micrometer.