# US 2021/0344058 A1 · Process for recovering lithium and transition metals from waste cathode of spent lithium ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0344058 A1
- Document ID: US20210344058A1
- Status: Published application
- Kind: A1
- Application number: 17/230,937
- Filed: 2021-04-14
- Published: 2021-11-04
- Earliest claimed: 2020-05-01
- Assignees: XProEM Ltd.
- Applicants: XProEM Ltd.
- Inventors: Xintong LIU; Chattopadhyay KINNOR
- Web page: https://patentgrep.com/patent/US20210344058A1

## CPC

- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- C22B 5/10: by solid carbonaceous reducing agents
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 7/008: {by an alkaline or ammoniacal leaching}
- C22B 15/0052: {Reduction smelting or converting}
- C22B 15/0056: {Scrap treating}
- C22B 23/0476: {Separation of nickel from cobalt}
- C22B 26/12: Obtaining lithium
- C22B 47/00: Obtaining manganese
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention is a process for directly recovering lithium and valuable transition metals such as cobalt, nickel and manganese from waste cathode and anode powder of spent lithium ion batteries into high grade products through a cascade reduction reaction scheme, followed by digestion and precipitation circuit using CO2 as media, and a series of physical separation procedures.

## Claims

### Claim 1

A process for recovering lithium and transition metals, namely cobalt and nickel for spent NCM LIBs, from Black Mass powders physically separated from other parts and materials of used battery packs, comprising:
I. partial reduction of Black Mass with added carbon in a reducing atmosphere facilitated by gas mixture of CO and CO2;
II. separating residual carbon from other substances from partially reduced Black Mass using gravity separation;
III. digestion of lithium carbonate and cobalt oxide in a cooled aqueous solution facilitated by CO2 injection and carbonate-bicarbonate ionic system;
IV. filtering nickel oxide and manganese oxide from leachate solution containing soluble lithium and cobalt species
V. complete reduction of nickel oxide with added carbon in a reducing atmosphere facilitated by gas mixture of CO and CO2
VI. separating magnetic metallic nickel from non-magnetic tailing using wet magnetic separation;
VII. precipitation of lithium carbonate and cobalt carbonate hydrate from the leachate solution via evaporative crystallization;
VIII. calcination of precipitated crystal mixture to form cobalt oxide and lithium carbonate.

### Claim 2 (depends on 1)

A process according to claim 1 wherein the cobalt oxide and lithium carbonate mixture is reduced in a reducing atmosphere facilitated by gas mixture of CO and CO2 to form metallic cobalt.

### Claim 3 (depends on 2)

A process according to claim 2 wherein the products from cobalt reduction are separated using magnetic separation into metallic cobalt and a slurry stream containing lithium carbonate.

### Claim 4 (depends on 3)

A process according to claim 3 wherein the abovementioned slurry stream is dried to obtain lithium carbonate crystal.

### Claim 5 (depends on 1)

A process according to claim 1 wherein the cobalt oxide and lithium carbonate mixture is washed using cold water to remove lithium carbonate from cobalt oxide.

### Claim 6 (depends on 5)

A process according to claim 5 wherein the lithium carbonate precipitates from the abovementioned washing water using evaporative crystallization.

### Claim 7 (depends on 1)

A process according to claim 1 wherein the source of carbon comprises of lignite coal, anthracite charcoal, activated carbon or a type of carbon-bearing substance with limited amounts of volatile and low impurity level.

### Claim 8 (depends on 1)

A process according to claim 1 wherein the CO/CO2 volumetric ratio in gas stream added to partial reduction is from 1:2 to 2:1.

### Claim 9 (depends on 1)

A process according to claim 1 wherein the CO/CO2 volumetric ratio in gas stream added to complete reduction is from 1:1 to 4:1.

### Claim 10 (depends on 1)

A process according to claim 1 wherein the temperature of partial reduction of Black Mass from spent NCM LIB is 400-600 degrees Celsius.

### Claim 11 (depends on 1)

A process according to claim 1 wherein the temperature of complete reduction of nickel oxide from abovementioned partially reduced Black Mass is 650-800 degrees Celsius.

### Claim 12 (depends on 1)

A process according to claim 1 wherein the temperature of decomposition of cobalt carbonate hydrate from abovementioned precipitated crystal mixture is 400-700 degrees Celsius.

### Claim 13 (depends on 2)

A process according to claim 2 wherein the temperature of complete reduction of cobalt oxide is 600-750 degrees Celsius.

### Claim 14 (depends on 1)

A process according to claim 1 wherein reaction time for partial reduction of Black Mass is 1-4 hours.

### Claim 15 (depends on 1)

A process according to claim 1 wherein reaction time for complete reduction of nickel oxide is 2-8 hours.

### Claim 16 (depends on 1)

A process according to claim 1 wherein reaction time for decomposition of cobalt carbonate hydrate is 1-4 hours.

### Claim 17 (depends on 2)

A process according to claim 2 wherein reaction time for complete reduction of cobalt oxide is 2-8 hours.

### Claim 18 (depends on 1)

A process according to claim 1 wherein inert gas such as Argon or Nitrogen is applied during heating or cooling.

### Claim 19 (depends on 1)

A process according to claim 1 wherein magnetic strengths in wet magnetic separation for a two-pass practice are 100-200 mT and 200-400 mT.

### Claim 20 (depends on 1)

A process according to claim 1 wherein magnetic strength in wet magnetic separation for one-pass practice is 100-200 mT.

### Claim 21 (depends on 1)

A process according to claim 1 wherein demineralized water added for lithium carbonate (and cobalt oxide as applicable) digestion is cooled to 0-5 degrees Celsius, and temperature of entire digestion process is maintained at 0-5 degrees Celsius.

### Claim 22 (depends on 1)

A process according to claim 1 wherein digestion of lithium carbonate and cobalt oxide is carried out with CO2 gas injection.

### Claim 23 (depends on 1)

A process according to claim 1 wherein the time for digestion of lithium carbonate and cobalt oxide is 1-6 hours.

### Claim 24 (depends on 1)

A process according to claim 1 wherein the temperature for evaporative crystallization of lithium carbonate is 60-80 degrees Celsius.

### Claim 25 (depends on 1)

A process according to claim 1 wherein the holding time for evaporative crystallization of lithium carbonate is 4-12 hours.