# US 2021/0344008 A1 · Secondary battery and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0344008 A1
- Document ID: US20210344008A1
- Status: Published application
- Kind: A1
- Application number: 17/259,722
- Filed: 2019-02-21
- Published: 2021-11-04
- Earliest claimed: 2018-07-27
- Assignees: Panasonic Intellectual Property Management Co., Ltd.
- Applicants: Panasonic Intellectual Property Management Co., Ltd.
- Inventors: Takayuki Nakatsutsumi; Kazuhiro Iida; Atsushi Fukui
- Web page: https://patentgrep.com/patent/US20210344008A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/0447: {of complete cells or cells stacks}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/5835: {Comprising fluorine or fluoride salts}
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0567: characterised by the additives
- H01M 10/0569: characterised by the solvents
- H01M 10/058: Construction or manufacture
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0034: Fluorinated solvents
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A secondary battery includes a positive electrode containing a positive electrode active material; a negative electrode; and an electrolyte. The electrolyte contains a solvent, a lithium salt dissolved in the solvent, and a film forming compound. The film forming compound includes fluorine and an unsaturated bond between carbons. A surface of the positive electrode active material is at least partially covered with a film containing lithium, oxygen, carbon, and fluorine.

## Claims

### Claim 1

A secondary battery comprising:
a positive electrode containing a positive electrode active material; a negative electrode; and an electrolyte,
wherein the electrolyte contains a solvent, a lithium salt dissolved in the solvent, and a film forming compound,
the film forming compound includes fluorine and an unsaturated bond between carbons and is a compound to be reduced at a potential of +2.0 V or more with reference to Li, and
a surface of the positive electrode active material is at least partially covered with a film containing lithium, oxygen, carbon, and fluorine.

### Claim 2 (depends on 1)

The secondary battery according to claim 1,
wherein the film forming compound is at least one of a cyclic acid anhydride and a cyclic carbonate compound.

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The secondary battery according to claim 1,
wherein the film forming compound includes trifluoromethyl maleic anhydride.

### Claim 5 (depends on 1)

The secondary battery according to claim 1,
wherein the film containing fluorine contains a reductively decomposed product of the film forming compound.

### Claim 6 (depends on 1)

The secondary battery according to claim 1,
wherein the negative electrode contains a lithium-containing substance which has a lithium-ion discharge potential in a range of +2.0 V to +3.5 V with reference to Li.

### Claim 7 (depends on 6)

The secondary battery according to claim 6,
wherein the lithium-containing substance contains at least one of a phosphoric salt which belongs to the space group Pnma and which contains lithium and a transition metal element MA and a composite oxide which belongs to the space group Immm and which contains lithium and a transition metal element MB.

### Claim 8 (depends on 1)

The secondary battery according to claim 1,
wherein the positive electrode active material contains a lithium nickel composite oxide represented by LiaNibM11-bO2,
M1 is at least one selected from the group consisting of Mn, Co, and Al, and
0.95≤a≤1.2 and 0.5≤b≤1 are satisfied.

### Claim 9 (depends on 8)

The secondary battery according to claim 8,
wherein the lithium nickel composite oxide is represented by LiaNibMncCo1-b-cO2, and
0.1≤c≤0.4 is satisfied.

### Claim 10 (depends on 8)

The secondary battery according to claim 8,
wherein the lithium nickel composite oxide is composed of particles having a compression strength of 250 MPa to 1,500 MPa.

### Claim 11 (depends on 1)

The secondary battery according to claim 1,
wherein the solvent contains a fluorinated solvent containing fluorine, oxygen, and carbon, and
a rate of the fluorinated solvent with respect to 100 parts by mass of the solvent is 30 to 100 parts by mass.

### Claim 12 (depends on 11)

The secondary battery according to claim 11,
wherein the fluorinated solvent includes at least one selected from the group consisting of fluoroethylene carbonate, methyl 3,3,3-trifluoropropionate, and 2,2,2-trifluoroethyl acetate.

### Claim 13

A method for manufacturing a secondary battery, comprising:
a step of assembling a secondary battery including a positive electrode, a negative electrode, and an electrolyte; and
a film forming step of dipping the positive electrode in a solution containing a lithium salt and a film forming compound which includes fluorine and an unsaturated bond between carbons to cover a surface of the positive electrode with a film formed by reductive decomposition of the film forming compound.

### Claim 14 (depends on 13)

The method for manufacturing a secondary battery according to claim 13,
wherein the solution is the electrolyte, and
the film forming step includes, after the step of assembling a secondary battery, a step of performing an overdischarge treatment on the secondary battery until the potential of the positive electrode reaches to a reduction potential of the film forming compound or less.