# US 2021/0344001 A1 · Zinc electrode improvements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0344001 A1
- Document ID: US20210344001A1
- Status: Published application
- Kind: A1
- Application number: 17/375,381
- Filed: 2021-07-14
- Published: 2021-11-04
- Earliest claimed: 2019-07-19
- Assignees: The Government of the United States of America, as represented by the Secretary of the Navy
- Applicants: The Government of the United States of America, as represented by the Secretary of the Navy
- Inventors: Brandon J. Hopkins; Joseph F. Parker; Jeffrey W. Long; Debra R. Rolison
- Web page: https://patentgrep.com/patent/US20210344001A1

## CPC

- H01M 4/30: Pressing
- B22F 3/1007: {Atmosphere (B22F3/1021 takes precedence)}
- B22F 3/11: Making porous workpieces or articles
- B22F 3/1134: {Inorganic fillers (carbonaceous or paper filler B22F3/1121)}
- B22F 3/1143: {involving an oxidation, reduction or reaction step}
- B22F 3/1146: {After-treatment maintaining the porosity (B22F3/114 takes precedence)}
- H01M 4/0433: {Molding}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/244: {Zinc electrodes}
- H01M 4/38: of elements or alloys
- H01M 10/24: Alkaline accumulators
- B22F 2301/30: Low melting point metals, i.e. Zn, Pb, Sn, Cd, In, Ga
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- H01M 4/366: {as layered products}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are methods of making porous zinc electrodes. Taken together, the steps are: forming a mixture of water, a soluble compound that increases the viscosity of the mixture, an insoluble porogen, and metallic zinc powder; placing the mixture in a mold to form a sponge; optionally drying the sponge; placing the sponge in a metal mesh positioned to allow air flow through substantially all the openings in the mesh; heating the sponge in an inert atmosphere at a peak temperature of 200 to 420° C. to fuse the zinc particles to each other to form a sintered sponge; and heating the sintered sponge in an oxygen-containing atmosphere at a peak temperature of 420 to 700° C. to form ZnO on the surfaces of the sintered sponge. The heating steps burn out the porogen.

## Claims

### Claim 1

A method comprising:
forming a mixture comprising:
water;
a water-soluble compound that increases the viscosity of the mixture;
water-insoluble porogen particles; and
metallic zinc powder;
placing the mixture in a mold to form a sponge;
optionally drying the sponge;
heating the sponge in an inert atmosphere at a temperature that fuses the zinc particles to each other to form a sintered sponge; and
heating the sintered sponge in an oxygen-containing atmosphere at a temperature that forms ZnO on the surfaces of the sintered sponge;
wherein the heating steps burn out the porogen.

### Claim 2 (depends on 1)

The method of claim 1, wherein the mixture further comprises an organic liquid.

### Claim 3 (depends on 1)

The method of claim 1, wherein the water-soluble compound is a water-soluble carboxymethyl cellulose resin.

### Claim 4 (depends on 1)

The method of claim 1, wherein the porogen is corn starch.

### Claim 5 (depends on 1)

The method of claim 1, wherein the heating steps are performed with the sponge in a metal mesh positioned to allow air flow through substantially all the openings in the mesh.

### Claim 6 (depends on 5)

The method of claim 5;
wherein the mesh is cylindrical in shape; and
wherein the mesh is placed horizontally on a substrate that touches the mesh at most on two lines along the length of the mesh.

### Claim 7 (depends on 1)

The method of claim 1, wherein heating the sponge in an inert atmosphere is performed at a peak temperature of 200 to 420° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein heating the sintered sponge in an oxygen-containing atmosphere is performed at a peak temperature of 420 to 700° C.

### Claim 9 (depends on 1)

A zinc electrode made by the method of claim 1.

### Claim 10 (depends on 9)

The zinc electrode of claim 9, wherein the zinc electrode has a density of at least 1.0 g cm−3.

### Claim 11 (depends on 9)

The zinc electrode of claim 9, wherein the zinc electrode comprises no more than 99 wt. % ZnO.

### Claim 12 (depends on 9)

An electrochemical cell comprising:
an anode current collector;
the zinc electrode of claim 9 in electrical contact with the anode current collector;
an electrolyte;
a cathode current collector;
a cathode in electrical contact with the cathode current collector; and
a separator between the zinc electrode and the cathode.

### Claim 13

A method comprising:
providing a sponge comprising zinc particles and porogen particles;
placing the sponge in a metal mesh positioned to allow air flow through substantially all the openings in the mesh;
heating the sponge in an inert atmosphere at a temperature that fuses the zinc particles to each other to form a sintered sponge; and
heating the sintered sponge in an oxygen-containing atmosphere at a temperature that forms ZnO on the surfaces of the sintered sponge;
wherein the heating steps burn out the porogen.

### Claim 14 (depends on 13)

The method of claim 13, wherein heating the sponge in an inert atmosphere is performed at a peak temperature of 200 to 420° C.

### Claim 15 (depends on 13)

The method of claim 13, wherein heating the sintered sponge in an oxygen-containing atmosphere is performed at a peak temperature of 420 to 700° C.

### Claim 16 (depends on 15)

The method of claim 15, wherein heating the sintered sponge produces a zinc electrode comprising no more than 99 wt. % ZnO.

### Claim 17

A method comprising:
providing a sponge comprising zinc particles and porogen particles;
heating the sponge in an inert atmosphere at a peak temperature of 200 to 420° C. to fuse the zinc particles to each other to form a sintered sponge; and
heating the sintered sponge in an oxygen-containing atmosphere at a peak temperature of 420 to 700° C. to form ZnO on the surfaces of the sintered sponge;
wherein the heating steps burn out the porogen.

### Claim 18 (depends on 17)

The method of claim 17, wherein heating the sintered sponge produces a zinc electrode comprising no more than 99 wt. % ZnO.