# US 2021/0343930 A1 · Semiconductor memory structure and method for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343930 A1
- Document ID: US20210343930A1
- Status: Published application
- Kind: A1
- Application number: 16/861,224
- Filed: 2020-04-29
- Published: 2021-11-04
- Earliest claimed: 2020-04-29
- Assignees: HeFeChip Corporation Limited
- Applicants: HeFeChip Corporation Limited
- Inventors: Hong-Hui Hsu; Wei-Chuan Chen; Qinli Ma; Shu-Jen Han
- Web page: https://patentgrep.com/patent/US20210343930A1

## CPC

- H10N 50/80: Constructional details
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H01F 10/3272: {by use of anti-parallel coupled [APC] ferromagnetic layers, e.g. artificial ferrimagnets [AFI], artificial [AAF] or synthetic [SAF] anti-ferromagnets}
- H01F 10/3286: {Spin-exchange coupled multilayers having at least one layer with perpendicular magnetic anisotropy}
- H01F 41/32: for applying conductive, insulating or magnetic material on a magnetic film {, specially adapted for a thin magnetic film}
- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N 50/85: Materials of the active region
- H01F 10/123: {having a L10 crystallographic structure, e.g. [Co,Fe][Pt,Pd] thin films}
- H01F 10/3236: {made of a noble metal, e.g.(Co/Pt) n multilayers having perpendicular anisotropy (H01F10/3286 takes precedence)}
- H01F 41/325: {applying a noble metal capping on a spin-exchange-coupled multilayer, e.g. spin filter deposition}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor memory structure includes a substrate, a magnetic tunneling junction (MTJ) stack disposed on the substrate, and an encapsulation layer surrounding the MTJ stack. The encapsulation layer comprises an outer silicon oxynitride layer with a composition of SiOx1Ny1 and an inner silicon oxynitride layer with a composition of SiOx2Ny2, wherein x1/y1>x2/y2.

## Claims

### Claim 1

A semiconductor memory structure, comprising:
a substrate;
a magnetic tunneling junction (MTJ) stack disposed on the substrate; and
an encapsulation layer surrounding the MTJ stack, wherein the encapsulation layer comprises an outer silicon oxynitride layer with a composition of SiOx1Ny1 and an inner silicon oxynitride layer with a composition of SiOx2Ny2, wherein x1/y1>x2/y2.

### Claim 2 (depends on 1)

The semiconductor memory structure according to claim 1, wherein the MTJ stack comprises a reference layer, a tunnel barrier layer on the reference layer, and a free layer on the tunnel barrier layer.

### Claim 3 (depends on 2)

The semiconductor memory structure according to claim 2, wherein the reference layer is comprised of RL_PL1|AFC-spacer|RL_PL2|metal-spacer|PEL, wherein the RL_PL1 and RL_PL2 are ferromagnetic layers having strong perpendicular magnetic anisotropy, which comprise [Co/Pt]n, [Co/Pd]n, [Co/Ni]n multilayers, [Co/Ir]n and [Fe/Rh]n; FePt, CoPt, FePd, TeFeCo, GdCo, MnGa, MnGe, MnSi, alloys thereof, or any combination thereof, wherein the metal-spacer comprises metal having amorphous texture, wherein the metal-spacer comprises Ta, Mo, W, Ir, Rh, Zr, Nb, Hf, Cr, V, Bi or any combination thereof, wherein the PEL is ferromagnet having high spin polarization and acquiring PMA at the interface of the metal-spacer and tunnel barrier layer, wherein the PEL comprises Fe, Co, Ni, Mn, B, Al, Si, CoFeB, CoFeAl, or CoMnSi, wherein the AFC-spacer is metal that provides antiferromagnetic coupling between the RL_PL and the PEL and comprises Ru, Ir, Rh, Cr or Re.

### Claim 4 (depends on 2)

The semiconductor memory structure according to claim 2, wherein the tunnel barrier layer comprises MgO, AlOx, TiOx, HfOx, MgAlOx, MgZnOx, TaOx, VOx, or any combination thereof.

### Claim 5 (depends on 2)

The semiconductor memory structure according to claim 2, wherein the free layer comprises Fe, CoFe, CoFeB, CoFeAl, CoMnSi, CoPt, FePt, CoPd, FePd, TeFeCo, GdCo, MnGa, MnGe, MnAl, MnSi or combinations thereof, with a thickness of 10 to 50 angstroms, wherein there is non-magnetic metal layer introduced in the free layer to improve retention, and wherein the non-magnetic metal layer comprises Ta, W, Mo, Nb, Mg, Al, C, V, Hf, Ir, Rh, Zr, Cr, Bi, or combinations thereof.

### Claim 6 (depends on 2)

The semiconductor memory structure according to claim 2 further comprising a capping layer on the free layer.

### Claim 7 (depends on 6)

The semiconductor memory structure according to claim 6, wherein the capping layer comprises an amorphous layer, a light-element sink layer, and a diffusion-stop layer.

### Claim 8 (depends on 6)

The semiconductor memory structure according to claim 6 further comprising a hard mask layer on the capping layer.

### Claim 9 (depends on 8)

The semiconductor memory structure according to claim 8, wherein the hard mask layer comprises Ru, TiN, TaN or combinations thereof and functions as a top electrode.

### Claim 10 (depends on 1)

The semiconductor memory structure according to claim 1, wherein the inner silicon oxynitride layer is in direct contact with a sidewall of the MTJ stack.

### Claim 11

A method for fabricating a semiconductor memory structure, comprising:
providing a substrate;
forming a magnetic tunneling junction (MTJ) stack on the substrate; and
forming an encapsulation layer surrounding the MTJ stack, wherein the encapsulation layer comprises an outer silicon oxynitride layer with a composition of SiOx1Ny1 and an inner silicon oxynitride layer with a composition of SiOx2Ny2, wherein x1/y1>x2/y2.

### Claim 12 (depends on 11)

The method according to claim 11, wherein said forming the MTJ stack comprises:
forming a reference layer on the substrate;
forming a tunnel barrier layer on the reference layer; and
forming a free layer on the tunnel barrier layer.

### Claim 13 (depends on 12)

The semiconductor memory structure according to claim 12, wherein the reference layer is comprised of RL_PL1|AFC-spacer|RL_PL2|metal-spacer|PEL, wherein the RL_PL1 and RL_PL2 are ferromagnetic layers having strong perpendicular magnetic anisotropy, which comprise [Co/Pt]n, [Co/Pd]n, [Co/Ni]n multilayers, [Co/Ir]n and [Fe/Rh]n; FePt, CoPt, FePd, TeFeCo, GdCo, MnGa, MnGe, MnSi, alloys thereof, or any combination thereof, wherein the metal-spacer comprises metal having amorphous texture, wherein the metal-spacer comprises Ta, Mo, W, Ir, Rh, Zr, Nb, Hf, Cr, V, Bi or any combination thereof, wherein the PEL is ferromagnet having high spin polarization and acquiring PMA at the interface of the metal-spacer and tunnel barrier layer, wherein the PEL comprises Fe, Co, Ni, Mn, B, Al, Si, CoFeB, CoFeAl, or CoMnSi, wherein the AFC-spacer is metal that provides antiferromagnetic coupling between the RL_PL and the PEL and comprises Ru, Ir, Rh, Cr and Re.

### Claim 14 (depends on 12)

The semiconductor memory structure according to claim 12, wherein the tunnel barrier layer comprises MgO, AlOx, TiOx, HfOx, MgAlOx, MgZnOx, TaOx, VOx, or any combination thereof.

### Claim 15 (depends on 12)

The semiconductor memory structure according to claim 12, wherein the free layer comprises Fe, CoFe, CoFeB, CoFeAl, CoMnSi, CoPt, FePt, CoPd, FePd, TeFeCo, GdCo, MnGa, MnGe, MnAl, MnSi or combinations thereof, with a thickness of 10 to 50 angstroms, wherein there is non-magnetic metal layer introduced in free layer to improve retention, and wherein the non-magnetic metal layer comprises Ta, W, Mo, Nb, Mg, Al, C, V, Hf, Ir, Rh, Zr, Cr, Bi, or combinations thereof.

### Claim 16 (depends on 12)

The method according to claim 12 further comprising:
forming a capping layer on the free layer.

### Claim 17 (depends on 16)

The method according to claim 16 further comprising:
forming a hard mask layer on the capping layer.

### Claim 18 (depends on 11)

The method according to claim 11, wherein forming encapsulation layer surrounding the MTJ stack comprises:
depositing a silicon-rich SiN layer on a sidewall of the MTJ stack; and
subjecting the silicon-rich SiN layer to a post-treatment, thereby transforming an outer portion of the encapsulation layer into the outer silicon oxynitride layer, while an inner part of the encapsulation layer is still the silicon-rich SiN layer.

### Claim 19 (depends on 18)

The method according to claim 18, wherein a Si content of the silicon-rich SiN layer exceeds that of stoichiometric Si3N4.

### Claim 20 (depends on 18)

The method according to claim 18, wherein the post-treatment comprises an oxygen plasma treatment.