# US 2021/0343843 A1 · Metal Oxide Film and Semiconductor Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343843 A1
- Document ID: US20210343843A1
- Status: Published application
- Kind: A1
- Application number: 17/370,221
- Filed: 2021-07-08
- Published: 2021-11-04
- Earliest claimed: 2015-12-29
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Yasuharu Hosaka; Toshimitsu Obonai; Yukinori Shima; Masami Jintyou; Daisuke Kurosaki; Takashi Hamochi; Junichi Koezuka; Kenichi Okazaki; Shunpei Yamazaki
- Web page: https://patentgrep.com/patent/US20210343843A1

## CPC

- H10D 62/80: characterised by the materials
- C03C 17/245: by deposition from the vapour phase
- C04B 35/01: based on oxide ceramics
- C04B 35/453: based on zinc, tin, or bismuth oxides or solid solutions thereof with other oxides, e.g. zincates, stannates or bismuthates
- C04B 35/62218: {obtaining ceramic films, e.g. by using temporary supports}
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- C23C 14/5853: {Oxidation}
- H10D 30/473: {having confinement of carriers by multiple heterojunctions, e.g. quantum well HEMT}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 30/6734: {having gate electrodes arranged on both top and bottom sides of the channel, e.g. dual-gate TFTs}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 62/875: {being semiconductor metal oxide, e.g. InGaZnO (Group II-VI materials H10D62/86; Group I-VI materials H10D62/871; Pb compounds or alloys H10D62/874)}
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/60: wherein the TFTs are in active matrices
- C03C 2217/23: Mixtures
- C03C 2218/151: by vacuum evaporation
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3284: Zinc oxides, zincates, cadmium oxides, cadmiates, mercury oxides, mercurates or oxide forming salts thereof
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/3293: Tin oxides, stannates or oxide forming salts thereof, e.g. indium tin oxide [ITO]
- C04B 2235/787: Oriented grains
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A metal oxide film includes indium, M, (M is Al, Ga, Y, or Sn), and zinc and includes a region where a peak having a diffraction intensity derived from a crystal structure is observed by X-ray diffraction in the direction perpendicular to the film surface. Moreover, a plurality of crystal parts is observed in a transmission electron microscope image in the direction perpendicular to the film surface. The proportion of a region other than the crystal parts is higher than or equal to 20% and lower than or equal to 60%.

## Claims

### Claim 1

A semiconductor device comprising:
a first conductive film over a substrate;
a first insulating film over the first conductive film;
an oxide semiconductor layer over the first insulating film;
a second insulating film over the oxide semiconductor layer;
a second conductive film over the second insulating film;
a third conductive film over the second conductive film; and
a third insulating film over the third conductive film,
wherein the oxide semiconductor layer comprises indium, an element M, and zinc,
wherein the element M is Al, Ga, Y, or Sn,
wherein a plurality of crystal parts is observed in a transmission electron microscope image in a direction perpendicular to a surface of the oxide semiconductor layer,
wherein a proportion of a region other than the plurality of crystal parts is higher than or equal to 20% and lower than or equal to 60%, and
wherein the third insulating film has a region in contact with a top surface of the oxide semiconductor layer and a top surface of the first insulating film.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1,
wherein the plurality of crystal parts has a higher proportion of crystal parts in which c-axes are aligned in a thickness direction of the oxide semiconductor layer than crystal parts aligned in other directions.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1,
wherein a first image is an image obtained by subjecting a cross-sectional TEM image to fast Fourier transform,
wherein a second image is obtained by subjecting the first image to inverse fast Fourier transform after mask treatment by which a periodic region remains,
wherein in the second image, the proportion of the remaining area subtracted from an original image is more than or equal to 20% and less than 60%.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein the proportion of the region other than the plurality of crystal parts is higher than or equal to 30% and lower than or equal to 50%.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1,
wherein when electron diffraction with a probe diameter of 50 nm or more is performed on a slice of the oxide semiconductor layer having a thickness of greater than or equal to 10 nm and less than or equal to 50 nm in the direction perpendicular to its cross section, a first electron diffraction pattern that includes a ring-like diffraction pattern and two first spots overlapping with the ring-like diffraction pattern is observed, and
wherein when electron diffraction with a probe diameter of greater than or equal to 0.3 nm and less than or equal to 5 nm is performed thereon, a second electron diffraction pattern that includes the two first spots and a plurality of second spots distributed in a circumferential direction is observed.

### Claim 6 (depends on 5)

The semiconductor device according to claim 5,
wherein the two first spots are symmetric with respect to a center,
wherein an angle between a first straight line and the direction of a normal vector of the surface of the oxide semiconductor layer is more than or equal to 0° and less than or equal to 10°, and
wherein the first straight line passes through the center and a point at which a luminance of the two first spots is the highest.

### Claim 7 (depends on 6)

The semiconductor device according to claim 6,
wherein in the first electron diffraction pattern, the luminance of the ring-like diffraction pattern is lower than that of the two first spots at a point of intersection of the ring-like diffraction pattern and a second straight line that intersects with the first straight line.

### Claim 8 (depends on 7)

The semiconductor device according to claim 7,
wherein the luminance of the two first spots is greater than 1 time and less than or equal to 9 times the luminance of the ring-like diffraction pattern at the point of intersection of the ring-like diffraction pattern and the second straight line.

### Claim 9

A semiconductor device comprising:
a first conductive film over a substrate;
a first insulating film over the first conductive film;
an oxide semiconductor layer over the first insulating film;
a second insulating film over the oxide semiconductor layer;
a second conductive film over the second insulating film;
a third conductive film over the second conductive film; and
a third insulating film over the third conductive film,
wherein the oxide semiconductor layer comprises indium, an element M, and zinc,
wherein the element M is Al, Ga, Y, or Sn,
wherein a plurality of crystal parts is observed in a transmission electron microscope image in a direction perpendicular to a surface of the oxide semiconductor layer,
wherein a proportion of a region other than the plurality of crystal parts is higher than or equal to 20% and lower than or equal to 60%,
wherein the third insulating film has a region in contact with a top surface of the oxide semiconductor layer and a top surface of the first insulating film, and
wherein a length of the second insulating film is longer than a length of the second conductive film in a cross sectional view of the semiconductor device.

### Claim 10 (depends on 9)

The semiconductor device according to claim 9,
wherein the plurality of crystal parts has a higher proportion of crystal parts in which c-axes are aligned in a thickness direction of the oxide semiconductor layer than crystal parts aligned in other directions.

### Claim 11 (depends on 9)

The semiconductor device according to claim 9,
wherein a first image is an image obtained by subjecting a cross-sectional TEM image to fast Fourier transform,
wherein a second image is obtained by subjecting the first image to inverse fast Fourier transform after mask treatment by which a periodic region remains,
wherein in the second image, the proportion of the remaining area subtracted from an original image is more than or equal to 20% and less than 60%.

### Claim 12 (depends on 9)

The semiconductor device according to claim 9, wherein the proportion of the region other than the plurality of crystal parts is higher than or equal to 30% and lower than or equal to 50%.

### Claim 13 (depends on 9)

The semiconductor device according to claim 9,
wherein when electron diffraction with a probe diameter of 50 nm or more is performed on a slice of the oxide semiconductor layer having a thickness of greater than or equal to 10 nm and less than or equal to 50 nm in the direction perpendicular to its cross section, a first electron diffraction pattern that includes a ring-like diffraction pattern and two first spots overlapping with the ring-like diffraction pattern is observed, and
wherein when electron diffraction with a probe diameter of greater than or equal to 0.3 nm and less than or equal to 5 nm is performed thereon, a second electron diffraction pattern that includes the two first spots and a plurality of second spots distributed in a circumferential direction is observed.

### Claim 14 (depends on 13)

The semiconductor device according to claim 13,
wherein the two first spots are symmetric with respect to a center,
wherein an angle between a first straight line and the direction of a normal vector of the surface of the oxide semiconductor layer is more than or equal to 0° and less than or equal to 10°, and
wherein the first straight line passes through the center and a point at which a luminance of the two first spots is the highest.

### Claim 15 (depends on 14)

The semiconductor device according to claim 14,
wherein in the first electron diffraction pattern, the luminance of the ring-like diffraction pattern is lower than that of the two first spots at a point of intersection of the ring-like diffraction pattern and a second straight line that intersects with the first straight line.

### Claim 16 (depends on 15)

The semiconductor device according to claim 15,
wherein the luminance of the two first spots is greater than 1 time and less than or equal to 9 times the luminance of the ring-like diffraction pattern at the point of intersection of the ring-like diffraction pattern and the second straight line.