# US 2021/0343840 A1 · Manufacturing method of trench mosfet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343840 A1
- Document ID: US20210343840A1
- Status: Published application
- Kind: A1
- Application number: 17/377,408
- Filed: 2021-07-16
- Published: 2021-11-04
- Earliest claimed: 2019-12-25
- Assignees: Excelliance MOS Corporation
- Applicants: Excelliance MOS Corporation
- Inventors: Chu-Kuang Liu; Yi-Lun Lo
- Web page: https://patentgrep.com/patent/US20210343840A1

## CPC

- H10D 62/371: {Inactive supplementary semiconductor regions, e.g. for preventing punch-through, improving capacity effect or leakage current}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 30/0217: {forming self-aligned punch-through stoppers or threshold implants under gate regions}
- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/105: {by having particular doping profiles, shapes or arrangements of PN junctions; by having supplementary regions, e.g. junction termination extension [JTE] (IGFETs having LDD or drain extension regions H10D30/601)}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 32/1406: {by ion implantation}
- H10P 32/171: {being group IV material}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A manufacturing method of a trench MOSFET includes forming a trench gate in an epitaxial layer having a first conductivity type on a substrate, performing implantations of a dopant having a second conductivity type on the epitaxial layer in which an implantation dose is gradually reduced toward the substrate, performing a first drive-in step to diffuse the dopant having the second conductivity type in an upper half of the epitaxial layer to form a body region, implanting a dopant having the first conductivity type on a surface of the epitaxial layer, performing a second drive-in step to diffuse the dopant having the first conductivity type to form a source region, comprehensively implanting the dopant having the second conductivity type at an interface of the body region and the source region to form an anti-punch through region having a doping concentration higher than that of the body region.

## Claims

### Claim 1

A manufacturing method of a trench MOSFET, comprising:
forming a trench gate in an epitaxial layer having a first conductivity type on a substrate;
performing a plurality of implantations of a dopant having a second conductivity type on the epitaxial layer in a manner that an implantation dose is gradually reduced toward a direction of the substrate;
performing a first drive-in step to diffuse the dopant having the second conductivity type in an upper half of the epitaxial layer to form a body region having the second conductivity type;
implanting a dopant having the first conductivity type on a surface of the epitaxial layer;
performing a second drive-in step to diffuse the dopant having the first conductivity type to form a source region; and
comprehensively implanting the dopant having the second conductivity type at an interface of the body region and the source region after the source region is formed to form an anti-punch through region, wherein a doping concentration of the anti-punch through region is higher than a doping concentration of the body region.

### Claim 2 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein a step of performing the plurality of implantations of the dopant having the second conductivity type comprises performing two or three implantations of the dopant having the second conductivity type.

### Claim 3 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein the doping concentration of the anti-punch through region is between 5E+16 atoms/cm3 and 5E+17 atoms/cm3.

### Claim 4 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein the first conductivity type is N-type and the second conductivity type is P-type.

### Claim 5 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein the first conductivity type is P-type and the second conductivity type is N-type.

### Claim 6 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein an energy of implanting the dopant having the first conductivity type is between 20 KeV and 45 KeV.

### Claim 7 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein the second drive-in step comprises rapid thermal processing (RTP).

### Claim 8 (depends on 1)

The manufacturing method of the trench MOSFET of claim 1, wherein the step of forming the trench gate comprises:
forming a trench in the epitaxial layer;
forming a gate oxide layer on a surface of the trench; and
depositing a conductor in the trench as a gate.