# US 2021/0343831 A1 · Semiconductor structure and method for forming same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343831 A1
- Document ID: US20210343831A1
- Status: Published application
- Kind: A1
- Application number: 17/101,209
- Filed: 2020-11-23
- Published: 2021-11-04
- Earliest claimed: 2020-04-30
- Assignees: Semiconductor Manufacturing International (Shanghai) Corporation; Semiconductor Manufacturing International (Beijing) Corporation
- Applicants: Semiconductor Manufacturing International (Shanghai) Corporation; Semiconductor Manufacturing International (Beijing) Corporation
- Inventors: Lian Feng HU
- Web page: https://patentgrep.com/patent/US20210343831A1

## CPC

- H10D 1/68: Capacitors having no potential barriers
- H10D 1/696: {comprising multiple layers, e.g. comprising a barrier layer and a metal layer (barrier layers to prevent diffusion of hydrogen or oxygen in perovskite based capacitors H10D1/688)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/496: {Capacitor integral with wiring layers}
- H10D 1/684: {the dielectrics comprising multiple layers, e.g. comprising buffer layers, seed layers or gradient layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor structure and a method for forming same are provided. In some implementations, a forming method includes: providing a base; forming a first electrode layer on the base; and forming a capacitor dielectric layer with a stacked structure on the first electrode layer and a second electrode layer on the capacitor dielectric layer, the capacitor dielectric layer including a bottom high-k dielectric layer, a leakage-proof dielectric layer, and a top high-k dielectric layer that are sequentially stacked from bottom to top, wherein the bottom high-k dielectric layer and the top high-k dielectric layer have a preset total deposition thickness, and wherein a proportion of a deposition thickness of the bottom high-k dielectric layer to the preset total deposition thickness is greater than a proportion of a deposition thickness of the top high-k dielectric layer to the preset total deposition thickness. In implementations of the present disclosure, the respective proportions of the bottom high-k dielectric layer and the top high-k dielectric layer to the preset total deposition thickness are adjusted, so that effective thicknesses of the bottom high-k dielectric layer and the top high-k dielectric layer are both relatively small, thereby alleviating the crystallization problem of the bottom high-k dielectric layer and the top high-k dielectric layer, and further improving reliability of a capacitor structure.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
providing a base;
forming a first electrode layer on the base; and
forming a capacitor dielectric layer with a stacked structure on the first electrode layer and a second electrode layer on the capacitor dielectric layer, the capacitor dielectric layer comprising:
a bottom high-k dielectric layer,
a leakage-proof dielectric layer, and
a top high-k dielectric layer that are sequentially stacked from a bottom to a top,
wherein the bottom high-k dielectric layer and the top high-k dielectric layer have a preset total deposition thickness, and
wherein a proportion of a deposition thickness of the bottom high-k dielectric layer to the preset total deposition thickness is greater than a proportion of a deposition thickness of the top high-k dielectric layer to the preset total deposition thickness.

### Claim 2 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein:
after the first electrode layer is formed on the base and before the capacitor dielectric layer with a stacked structure is formed on the first electrode layer and a second electrode layer on the capacitor dielectric layer is formed, the forming method further comprises:
forming a capacitor dielectric film covering the stacked structure of the first electrode layer, the capacitor dielectric film comprising a bottom high-k dielectric film, a leakage-proof dielectric film, and a top high-k dielectric film that are sequentially stacked from a bottom to a top,
wherein the bottom high-k dielectric film and the top high-k dielectric film have a preset total deposition thickness, and
wherein a proportion of a deposition thickness of the bottom high-k dielectric film to the preset total deposition thickness is greater than a proportion of a deposition thickness of the top high-k dielectric film to the preset total deposition thickness;
the step of forming the second electrode layer comprises:
forming an electrode film covering the capacitor dielectric film; and
patterning the electrode film to form a second electrode layer above a part of the first electrode layer; and
the step of forming the capacitor dielectric layer comprises: after the second electrode layer is formed, removing the capacitor dielectric film exposed from the second electrode layer, and retaining, as the capacitor dielectric layer, the capacitor dielectric film remaining between the second electrode layer and the first electrode layer.

### Claim 3 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein a process for forming the capacitor dielectric layer comprises an atomic layer deposition process or a plasma chemical vapor deposition process.

### Claim 4 (depends on 2)

The method for forming a semiconductor structure according to claim 2, wherein the step of removing the capacitor dielectric film exposed from the second electrode layer comprises: etching the capacitor dielectric film exposed from the second electrode layer using an anisotropic dry etching process.

### Claim 5 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein in the step of forming a capacitor dielectric layer with a stacked structure on the first electrode layer, a proportion of the deposition thickness of the top high-k dielectric layer to the deposition thickness of the bottom high-k dielectric layer is 0.5 to 0.9.

### Claim 6 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein in the step of forming a capacitor dielectric layer with a stacked structure on the first electrode layer, the deposition thickness of the bottom high-k dielectric layer is 1.5 nanometers to 4 nanometers.

### Claim 7 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein a front layer metal interconnect structure is formed in the base, a top surface of the front layer metal interconnect structure being exposed from the base, wherein:
before the first electrode layer is formed, the forming method further comprises:
forming an etch stop layer on the base, the etch stop layer covering the front layer metal interconnect structure; and
forming an interlayer dielectric layer on the etch stop layer; and
in the step of forming the first electrode layer, the first electrode layer is formed on the interlayer dielectric layer.

### Claim 8 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein:
the bottom high-k dielectric layer is made of a material comprising titanium oxide, cobalt oxide, nickel oxide, copper oxide, zinc oxide, zirconium oxide, hafnium oxide, tantalum oxide, tungsten oxide, strontium titanate, strontium zirconate, or strontium ruthenate; and
the top high-k dielectric layer is made of a material comprising titanium oxide, cobalt oxide, nickel oxide, copper oxide, zinc oxide, zirconium oxide, hafnium oxide, tantalum oxide, tungsten oxide, strontium titanate, strontium zirconate, or strontium ruthenate.

### Claim 9 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the leakage-proof dielectric layer is made of a material comprising aluminum oxide, silicon oxide, or silicon nitride.

### Claim 10 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the first electrode layer is made of nitrided metal.

### Claim 11 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the first electrode layer is made of a material comprising TiN, TaN, or WN.

### Claim 12

A semiconductor structure, comprising:
a base;
a first electrode layer located on the base;
a capacitor dielectric layer with a stacked structure located on the first electrode layer, the capacitor dielectric layer comprising:
a bottom high-k dielectric layer,
a leakage-proof dielectric layer, and
a top high-k dielectric layer that are sequentially stacked from a bottom to a top,
wherein the bottom high-k dielectric layer and the top high-k dielectric layer have a preset total deposition thickness, and
wherein a proportion of a deposition thickness of the bottom high-k dielectric layer to the preset total deposition thickness is greater than a proportion of a deposition thickness of the top high-k dielectric layer to the preset total deposition thickness; and
a second electrode layer located on the capacitor dielectric layer.

### Claim 13 (depends on 12)

The semiconductor structure according to claim 12, wherein a proportion of the deposition thickness of the top high-k dielectric layer to the deposition thickness of the bottom high-k dielectric layer is 0.5 to 0.9.

### Claim 14 (depends on 12)

The semiconductor structure according to claim 12, wherein the deposition thickness of the bottom high-k dielectric layer is 1.5 nanometers to 4 nanometers.

### Claim 15 (depends on 12)

The semiconductor structure according to claim 12, wherein:
a front layer metal interconnect structure is formed in the base, a top surface of the front layer metal interconnect structure being exposed from the base,
the semiconductor structure further comprises:
an etch stop layer located on the base, where the etch stop layer covers the front layer metal interconnect structure; and
an interlayer dielectric layer located on the etch stop layer,
the first electrode layer being located on the interlayer dielectric layer.

### Claim 16 (depends on 12)

The semiconductor structure according to claim 12, wherein:
the bottom high-k dielectric layer is made of a material comprising titanium oxide, cobalt oxide, nickel oxide, copper oxide, zinc oxide, zirconium oxide, hafnium oxide, tantalum oxide, tungsten oxide, strontium titanate, strontium zirconate, or strontium ruthenate; and
the top high-k dielectric layer is made of a material comprising titanium oxide, cobalt oxide, nickel oxide, copper oxide, zinc oxide, zirconium oxide, hafnium oxide, tantalum oxide, tungsten oxide, strontium titanate, strontium zirconate, or strontium ruthenate.

### Claim 17 (depends on 12)

The semiconductor structure according to claim 12, wherein the leakage-proof dielectric layer is made of a material comprising aluminum oxide, silicon oxide, or silicon nitride.

### Claim 18 (depends on 12)

The semiconductor structure according to claim 12, wherein the first electrode layer is made of nitrided metal.

### Claim 19 (depends on 12)

The semiconductor structure according to claim 12, wherein the first electrode layer is made of a material comprising TiN, TaN, or WN.