# US 2021/0343583 A1 · Method of manufacturing epitaxy substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343583 A1
- Document ID: US20210343583A1
- Status: Published application
- Kind: A1
- Application number: 17/375,008
- Filed: 2021-07-14
- Published: 2021-11-04
- Earliest claimed: 2018-04-03
- Assignees: GlobalWafers Co., Ltd.
- Applicants: GlobalWafers Co., Ltd.
- Inventors: Ying-Ru Shih; Chih-Yuan Chuang; Chi-Tse Lee; Chun-I Fan; Wen-Ching Hsu
- Web page: https://patentgrep.com/patent/US20210343583A1

## CPC

- H10P 90/1914: {using bonding}
- B32B 3/02: characterised by features of form at particular places, e.g. in edge regions {(non-uniform thickness B32B3/263)}
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- C04B 37/001: {directly with other burned ceramic articles}
- C04B 37/003: {by means of an interlayer consisting of a combination of materials selected from glass, or ceramic material with metals, metal oxides or metal salts}
- C04B 37/005: {consisting of glass or ceramic material}
- H10D 62/10: Shapes, relative sizes or dispositions of the regions of the semiconductor bodies; Shapes of the semiconductor bodies
- H10D 62/40: Crystalline structures
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- H10P 90/00: Preparation of wafers not covered by a single main group of this subclass, e.g. wafer reinforcement
- H10P 90/128: {by edge treatment, e.g. chamfering}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- B32B 2250/02: 2 layers
- B32B 2307/20: having particular electrical or magnetic properties, e.g. piezoelectric
- C04B 2237/062: based on silica or silicates
- C04B 2237/08: Non-oxidic interlayers
- C04B 2237/16: Silicon interlayers
- C04B 2237/36: Non-oxidic
- C04B 2237/365: Silicon carbide
- C04B 2237/366: Aluminium nitride
- C04B 2237/52: Pre-treatment of the joining surfaces, e.g. cleaning, machining
- C04B 2237/704: of one or more of the ceramic layers or articles
- C04B 2237/76: Forming laminates or joined articles comprising at least one member in the form other than a sheet or disc, e.g. two tubes or a tube and a sheet or disc
- C04B 2237/80: Joining the largest surface of one substrate with a smaller surface of the other substrate, e.g. butt joining or forming a T-joint
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing an epitaxy substrate is provided. A handle substrate is provided. A beveling treatment is performed on an edge of a device substrate such that a bevel is formed at the edge of the device substrate, wherein a thickness of the device substrate is greater than 100 μm and less than 200 μm. An ion implantation process is performed on a first surface of the device substrate to form an implantation region within the first surface. A second surface of the device substrate is bonded to the handle substrate for forming the epitaxy substrate, wherein a bonding angle greater than 90° is provided between the bevel of the device substrate and the handle substrate, and a projection length of the bevel toward the handle substrate is between 600 μm and 800 μm.

## Claims

### Claim 1

A method of manufacturing an epitaxy substrate, the method comprising:
providing a handle substrate;
performing a beveling treatment on an edge of a device substrate such that a bevel is formed at the edge of the device substrate, wherein a thickness of the device substrate is greater than 100 μm and less than 200 μm;
performing an ion implantation process on a first surface of the device substrate to form an implantation region within the first surface; and
bonding a second surface of the device substrate to the handle substrate to form the epitaxy substrate, wherein a bonding angle greater than 90° is provided between the bevel of the device substrate and the handle substrate, and a projection length of the bevel toward the handle substrate is between 600 μm and 800 μm.

### Claim 2 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a distance between the implantation region and the first surface is 10 nm to 95 nm.

### Claim 3 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a method of providing the handle substrate comprises doping carbon, nitrogen or a combination thereof during crystal growth.

### Claim 4 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, further comprising, after providing the handle substrate, forming a protective layer on a surface of the handle substrate that is not bonded to the device substrate.

### Claim 5 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a method of bonding the second surface of the device substrate to the handle substrate further comprises performing the bonding between the second surface of the device substrate and the handle substrate through a bonding layer.

### Claim 6 (depends on 5)

The method of manufacturing an epitaxy substrate of claim 5, further comprising, before bonding the second surface of the device substrate to the handle substrate, forming a charge trapping layer on a surface of the handle substrate that is bonded to the device substrate.

### Claim 7 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a resistivity of the device substrate is greater than 100 ohm-cm.

### Claim 8 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein an error value of crystal orientation of the device substrate is less than ±0.05 degree.

### Claim 9 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein the bonding angle is 100° to 170°.

### Claim 10 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein the oxygen content of the device substrate is less than 5 ppma.

### Claim 11 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a resistivity of the device substrate is greater than a resistivity of the handle substrate.

### Claim 12 (depends on 11)

The method of manufacturing an epitaxy substrate of claim 11, wherein after annealing at 450° C. for one hour, the resistivity of the device substrate is greater than the resistivity of the handle substrate.

### Claim 13 (depends on 11)

The method of manufacturing an epitaxy substrate of claim 11, wherein after a heat treatment at 720° C. for two minutes, the resistivity of the device substrate is greater than the resistivity of the handle substrate.

### Claim 14 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a diameter of the handle substrate and a diameter of the second surface of the device substrate are different by 0.2 mm or more.

### Claim 15 (depends on 1)

The method of manufacturing an epitaxy substrate of claim 1, wherein a maximum deformation amount of the handle substrate is less than 6.5 mm.