# US 2021/0343534 A1 · Method for manufacturing semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343534 A1
- Document ID: US20210343534A1
- Status: Published application
- Kind: A1
- Application number: 17/373,914
- Filed: 2021-07-13
- Published: 2021-11-04
- Earliest claimed: 2020-02-28
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Taoyan YAN
- Web page: https://patentgrep.com/patent/US20210343534A1

## CPC

- H10W 20/047: {by introducing additional elements therein}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/01125: {the silicides being formed by chemical reaction with the semiconductor after the contact hole formation}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/054: {by selectively removing parts thereof (H10W20/034 takes precedence)}
- H10W 20/066: {by forming silicides of refractory metals}
- H10W 20/0698: {Local interconnections}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/083: {the openings being via holes penetrating underlying conductors}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Some examples of this disclosure relate to the field of the semiconductor technology, and disclose a method for manufacturing a semiconductor structure. The method for manufacturing of the semiconductor structure includes: providing a base, wherein the base includes a metal layer and an oxide located in the metal layer or on a surface of the metal layer; and performing heat treatment on the base, wherein a reducing gas is introduced during the heat treatment, and the metal layer is converted into a metal compound layer after the heat treatment. This disclosure can improve the performance of the semiconductor structure.

## Claims

### Claim 1

A method for manufacturing a semiconductor structure, comprising:
providing a base, wherein the base comprises a metal layer and an oxide located on a surface of the metal layer; and
performing heat treatment on the base, wherein a reducing gas is introduced during the heat treatment, and the metal layer is converted into a metal compound layer after the heat treatment.

### Claim 2 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein the reducing gas comprises NH3, and a gas flow of the reducing gas ranges from 5 slm to 30 slm.

### Claim 3 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein a material of the oxide comprises a silicon oxide.

### Claim 4 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein a material of the metal layer comprises Co, Ni, Ta or Ti.

### Claim 5 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein the heat treatment comprises:
performing a first heat treatment step, wherein the reducing gas and a first auxiliary gas is introduced, and the base is heated to a first temperature and maintained at the first temperature for a first period of time; and
performing a second heat treatment step after the first heat treatment step, wherein a second auxiliary gas is introduced, and the base is heated to a second temperature and maintained at the second temperature for a second period of time, wherein the second temperature is greater than the first temperature.

### Claim 6 (depends on 5)

The method for manufacturing the semiconductor structure of claim 5, wherein the first auxiliary gas or the second auxiliary gas comprises N2, He, Ar or Ne, and a gas flow of the first auxiliary gas or the second auxiliary gas ranges from 5 slm to 50 slm.

### Claim 7 (depends on 5)

The method for manufacturing the semiconductor structure of claim 5, wherein a process pressure of the first heat treatment step and a process pressure of the second heat treatment step range from 750 torr to 850 torr.

### Claim 8 (depends on 5)

The method for manufacturing the semiconductor structure of claim 5, wherein in the first heat treatment step, a temperature rise rate of the base is 5° C./s to 20° C./s, the first temperature ranges from 300° C. to 600° C., and the first period of time ranges from 10 s to 60 s.

### Claim 9 (depends on 8)

The method for manufacturing the semiconductor structure of claim 8, wherein in the first heat treatment step, the temperature rise rate of the base is 10° C./s to 15° C./s, the first temperature ranges from 400° C. to 500° C., and the first period of time ranges from 20 s to 40 s.

### Claim 10 (depends on 5)

The method for manufacturing the semiconductor structure of claim 5, wherein in the second heat treatment step, a temperature rise rate of the base is 5° C./s to 20° C./s, the second temperature ranges from 700° C. to 800° C., and the second period of time ranges from 30 s to 50 s.

### Claim 11 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein a material of the metal compound layer comprises CoSi2, NiSix, TaSix or TiSix.

### Claim 12 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein the reducing gas comprises NH3, H2 or SF6.

### Claim 13 (depends on 1)

The method for manufacturing the semiconductor structure of claim 1, wherein the base further comprises a substrate, a dielectric layer located on a surface of the substrate; and a groove in the dielectric layer for exposing the substrate.

### Claim 14 (depends on 13)

The method for manufacturing the semiconductor structure of claim 13, further comprising:
removing an unreacted portion of the metal layer;
forming a first conductive layer at a bottom and side walls of the groove and a top surface of the dielectric layer; and
forming a second conductive layer which completely covers the first conductive layer on a side of the first conductive layer away from the substrate.

### Claim 15 (depends on 14)

The method for manufacturing the semiconductor structure of claim 14, wherein a material of the first conductive layer comprises TiN or TaN, and a material of the second conductive layer comprises Ti, W, Ta, Al or Ni.