# US 2021/0343523 A1 · Method for forming semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343523 A1
- Document ID: US20210343523A1
- Status: Published application
- Kind: A1
- Application number: 17/375,211
- Filed: 2021-07-14
- Published: 2021-11-04
- Earliest claimed: 2019-06-26
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corp.
- Inventors: Zhen-Zhen WANG; Jian-Jun ZHANG
- Web page: https://patentgrep.com/patent/US20210343523A1

## CPC

- H10P 14/6923: {the material being boron or phosphorus doped silicon oxides, e.g. BPSG, BSG or PSG}
- H10D 64/01: Manufacture or treatment
- H10D 64/516: {the thicknesses being non-uniform}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/093: {by modifying materials of the dielectric parts}
- H10W 20/098: {by filling between adjacent conductive parts}
- H10W 20/47: comprising two or more dielectric layers having different properties, e.g. different dielectric constants
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a semiconductor structure is provided, which comprises the following steps. A gate is formed by a method comprising the following steps. A gate dielectric layer is formed on a substrate. A gate electrode is formed on the gate dielectric layer. A nitride spacer is formed on a sidewall of the gate electrode. A phosphorus containing dielectric layer is formed on the gate. The phosphorus containing dielectric layer has a varied phosphorus dopant density distribution profile. The phosphorus containing dielectric layer comprises a phosphorus dopant density region on an upper surface of the gate and having a triangle-like shape.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
forming a gate by a method comprising:
forming a gate dielectric layer on a substrate;
forming a gate electrode on the gate dielectric layer;
forming a nitride spacer on a sidewall of the gate electrode; and
forming a phosphorus containing dielectric layer on the gate, wherein the phosphorus containing dielectric layer has a varied phosphorus dopant density distribution profile, the phosphorus containing dielectric layer comprises:
a first phosphorus dopant density region on the gate and having a top point; and
a second phosphorus dopant density region on the first phosphorus dopant density region and having another top point, wherein a straight line defined between the top point of the first phosphorus dopant density region and the another top point of the second phosphorus dopant density region is deviated from a vertical direction.

### Claim 2 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the phosphorus containing dielectric layer has a flame-like distribution profile portion.

### Claim 3 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein a phosphorus dopant density of the first phosphorus dopant density region is larger than a phosphorus dopant density of the second phosphorus dopant density region.

### Claim 4 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the phosphorus containing dielectric layer comprises phosphosilicate glass (PSG) or borophosphosilicate glass (BPSG), and the nitride spacer comprises silicon nitride (SiN).

### Claim 5 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the phosphorus containing dielectric layer is formed by a method comprising a high density plasma chemical vapor deposition (HDPCVD).

### Claim 6 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the nitride spacer has a width gradually increased from a top to a bottom of the nitride spacer.

### Claim 7

A method for forming a semiconductor structure, comprising:
forming a gate by a method comprising:
forming a gate dielectric layer on a substrate;
forming a gate electrode on the gate dielectric layer;
forming a nitride spacer on a sidewall of the gate electrode; and
forming a phosphorus containing dielectric layer on the gate, wherein the phosphorus containing dielectric layer has a varied phosphorus dopant density distribution profile, the phosphorus containing dielectric layer comprises a phosphorus dopant density region on an upper surface of the gate and having a triangle-like shape.

### Claim 8 (depends on 7)

The method for forming the semiconductor structure according to claim 7, wherein the phosphorus containing dielectric layer has a flame-like distribution profile portion or a bud-like distribution profile portion.

### Claim 9 (depends on 7)

The method for forming the semiconductor structure according to claim 7, wherein the phosphorus containing dielectric layer comprises phosphosilicate glass (PSG) or borophosphosilicate glass (BPSG), and the nitride spacer comprises silicon nitride (SiN).

### Claim 10 (depends on 7)

The method for forming the semiconductor structure according to claim 7, wherein the phosphorus containing dielectric layer is formed by a method comprising a high density plasma chemical vapor deposition (HDPCVD).

### Claim 11 (depends on 7)

The method for forming the semiconductor structure according to claim 7, wherein the nitride spacer has a width gradually increased from a top to a bottom of the nitride spacer.

### Claim 12

A method for forming a semiconductor structure, comprising:
forming a gate by a method comprising:
forming a gate dielectric layer on a substrate;
forming a gate electrode on the gate dielectric layer;
forming a nitride spacer on a sidewall of the gate electrode;
forming a phosphorus containing dielectric layer on the gate, wherein the phosphorus containing dielectric layer has a varied phosphorus dopant density distribution profile;
forming a contact opening in the phosphorus containing dielectric layer by performing an etching step having etch selectivity to the phosphorus containing dielectric layer; and
forming a contact element in the contact opening.

### Claim 13 (depends on 12)

The method for forming the semiconductor structure according to claim 12, further comprising forming a source/drain in the substrate, wherein the contact opening exposes the source/drain and the nitride spacer.

### Claim 14 (depends on 12)

The method for forming the semiconductor structure according to claim 12, wherein the phosphorus containing dielectric layer has a flame-like distribution profile portion or a bud-like distribution profile portion.

### Claim 15 (depends on 12)

The method for forming the semiconductor structure according to claim 12, wherein the phosphorus containing dielectric layer comprises phosphosilicate glass (PSG) or borophosphosilicate glass (BPSG), and the nitride spacer comprises silicon nitride (SiN).

### Claim 16 (depends on 12)

The method for forming the semiconductor structure according to claim 12, wherein the nitride spacer has a width gradually increased from a top to a bottom of the nitride spacer.

### Claim 17 (depends on 12)

The method for forming the semiconductor structure according to claim 12, wherein the phosphorus containing dielectric layer is formed by a method comprising a high density plasma chemical vapor deposition (HDPCVD).

### Claim 18 (depends on 17)

The method for forming the semiconductor structure according to claim 17, wherein the high density plasma chemical vapor deposition has process parameters comprising:
a depositing rate of 5500 Å/min-6500 Å/min; and
a sputtering rate of 700 Å/min-1000 Å/min.

### Claim 19 (depends on 12)

The method for forming the semiconductor structure according to claim 12, wherein the phosphorus containing dielectric layer comprises a phosphorus dopant density region on an upper surface of the gate and having a width gradually decreased from a bottom portion to a top portion of the phosphorus dopant density region.