# US 2021/0343520 A1 · Ultrathin atomic layer deposition film accuracy thickness control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343520 A1
- Document ID: US20210343520A1
- Status: Published application
- Kind: A1
- Application number: 17/305,938
- Filed: 2021-07-16
- Published: 2021-11-04
- Earliest claimed: 2015-03-20
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Jun Qian; Hu Kang; Adrien LaVoie; Seiji Matsuyama; Purushottam Kumar
- Web page: https://patentgrep.com/patent/US20210343520A1

## CPC

- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- C23C 16/02: Pretreatment of the material to be coated (C23C16/04 takes precedence)
- C23C 16/401: {containing silicon}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45542: {Plasma being used non-continuously during the ALD reactions}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H01J 37/32743: {for introducing the material into processing chamber}
- H01J 37/32899: {Multiple chambers, e.g. cluster tools}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H01J 37/32834: {Exhausting}
- H01J 2237/1825: Evacuating means
- H01J 2237/201: for mounting multiple objects
- H01J 2237/20278: Motorised movement
- H01J 2237/332: Coating
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Methods for depositing ultrathin films by atomic layer deposition with reduced wafer-to-wafer variation are provided. Methods involve exposing the substrate to soak gases including one or more gases used during a plasma exposure operation of an atomic layer deposition cycle prior to the first atomic layer deposition cycle to heat the substrate to the deposition temperature.

## Claims

### Claim 1

A method for depositing a silicon oxide film by atomic layer deposition on a semiconductor substrate, the method comprising:
(a) inserting a substrate into a chamber;
(b) after inserting the substrate into the chamber and prior to performing a first cycle of atomic layer deposition at a deposition temperature, raising the substrate's temperature to about the deposition temperature by exposing the substrate to a soak gas for a duration of about 500 seconds or less; and
(c) performing the atomic layer deposition,
wherein a cycle of the atomic layer deposition comprises
exposing the substrate to a silicon-containing precursor in a non-plasma environment for a duration sufficient to substantially adsorb the silicon-containing precursor to the surface of the substrate and
exposing the substrate to an oxidant in a plasma environment to form at least a portion of the silicon oxide film,
wherein soaking the substrate comprises exposing the substrate to a soak gas comprising only one or more gases used when exposing the substrate to the oxidant in the plasma environment during the atomic layer deposition cycle to form the at least a portion of the silicon oxide film, and
wherein the thickness of the silicon oxide film deposited by the atomic layer deposition is less than about 5 nm.

### Claim 2 (depends on 1)

The method of claim 1, wherein the soak gas in (b) contains only a gas or gases used when exposing the substrate to the oxidant in the plasma environment to form the at least a portion of the silicon oxide film.

### Claim 3 (depends on 1)

The method of claim 1, wherein the soak gas in (b) comprises two or more gases, and no other gases, used when exposing the substrate to the oxidant in the plasma environment to form the at least a portion of the silicon oxide film, and wherein the two or more gases are present in the soak gas in substantially the same proportion as they are in the oxidant.

### Claim 4 (depends on 1)

The method of claim 1, wherein the soak gas in (b) is selected from the group consisting of argon, nitrogen, oxygen, nitrous oxide, and combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the soak gas in (b) comprises no helium.

### Claim 6 (depends on 1)

The method of claim 1, wherein the flow rate of the soak gas in (b) is within about 10% of a maximum flow rate achievable by the chamber.

### Claim 7 (depends on 6)

The method of claim 6, wherein the flow rate of the soak gas in (b) is at least about 15 slm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the flow rate of the soak gas in (b) is at least about 25% to about 200% of the flow rate of the one or more gases used when exposing the substrate to the oxidant in the plasma environment during the atomic layer deposition cycle.

### Claim 9 (depends on 1)

The method of claim 1, wherein wafer-to-wafer variation of the average silicon oxide film thickness over the surface of the substrate is less than about ±2 Å.

### Claim 10 (depends on 1)

The method of claim 1, wherein (c) comprises performing two or more atomic layer deposition cycles to deposit the silicon oxide film on the substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein between two and about fifty atomic layer deposition cycles are performed.

### Claim 12 (depends on 1)

The method of claim 1, wherein the silicon-containing precursor is selected from the group consisting of silane, disilane, trisilane, tetrasilane, halogen-substituted versions of any of the foregoing silanes, amine-substituted versions of any of the foregoing silanes, and trisilylamine.

### Claim 13 (depends on 1)

The method of claim 1, wherein the oxidant is selected from the group consisting of oxygen, nitrous oxide, and combinations thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the atomic layer deposition is performed at a temperature of between about 30° C. and about 70° C.

### Claim 15 (depends on 1)

The method of claim 1, wherein the cycle of the atomic layer deposition further comprises purging the chamber between each exposing operation.

### Claim 16

A method for depositing a film by atomic layer deposition on a semiconductor substrate, the method comprising:
(a) inserting a substrate into a chamber; and
(b) after inserting the substrate into the chamber and prior to performing a first cycle of atomic layer deposition at a deposition temperature, raising the substrate's temperature to about the deposition temperature by exposing the substrate to a soak gas for a duration of about 500 seconds or less; and
(c) performing the atomic layer deposition,
wherein a cycle of the atomic layer deposition comprises
exposing the substrate to a precursor in a non-plasma environment for a duration sufficient to substantially adsorb the precursor to the surface of the substrate,
exposing the substrate to a second reactant in a plasma environment to form at least a portion of the film, and
wherein soaking the substrate comprises exposing the substrate to a soak gas comprising only one or more gases used when exposing the substrate to the second reactant in the plasma environment during the atomic layer deposition cycle to form the at least a portion of the film, and
wherein the thickness of the film deposited by the atomic layer deposition is less than about 5 nm.

### Claim 17 (depends on 16)

The method of claim 16, wherein the soak gas in (b) contains only a gas or gases used when exposing the substrate to the second reactant in the plasma environment to form the at least a portion of the film.

### Claim 18 (depends on 16)

The method of claim 16, wherein the soak gas in (b) comprises two or more gases, and no other gases, used when exposing the substrate to the second reactant in the plasma environment to form the at least a portion of the film, and wherein the two or more gases are present in the soak gas in substantially the same proportion as they are in the second reactant.

### Claim 19 (depends on 16)

The method of claim 16, wherein the soak gas in (b) is selected from the group consisting of argon, nitrogen, oxygen, nitrous oxide, and combinations thereof.

### Claim 20 (depends on 16)

The method of claim 16, wherein the soak gas in (b) comprises no helium.

### Claim 21 (depends on 16)

The method of claim 16, wherein the flow rate of the soak gas in (b) is within 10% of a maximum flow rate achievable by the chamber.

### Claim 22 (depends on 21)

The method of claim 21, wherein the flow rate of the soak gas in (b) is at least about 15 slm.

### Claim 23 (depends on 16)

The method of claim 16, wherein the flow rate of the soak gas in (b) is at least about 25% to about 200% of the flow rate of the one or more gases used when exposing the substrate to the oxidant in the plasma environment during the atomic layer deposition cycle.

### Claim 24 (depends on 16)

The method of claim 16, wherein wafer-to-wafer variation of the average film thickness over the surface of the substrate is less than about ±2 Å.

### Claim 25 (depends on 16)

The method of claim 16, wherein (c) comprises performing two or more atomic layer deposition cycles to deposit the film on the substrate.

### Claim 26 (depends on 25)

The method of claim 25, wherein between two and about fifty atomic layer deposition cycles are performed.

### Claim 27 (depends on 16)

The method of claim 16, wherein the film deposited by the atomic layer deposition is selected from the group consisting of silicon oxide, silicon nitride, silicon carbide, metal oxide, doped silicon oxide, doped silicon nitride, doped silicon carbide, and doped metal oxide.

### Claim 28 (depends on 16)

The method of claim 16, wherein the film deposited by the atomic layer deposition is an oxide and the atomic layer deposition is performed at a temperature of about 50° C.

### Claim 29 (depends on 16)

The method of claim 16, wherein the film deposited by the atomic layer deposition is a nitride or carbide and the atomic layer deposition is performed at a temperature of between about 200° C. and about 300° C.

### Claim 30 (depends on 16)

The method of claim 16, wherein the precursor comprises a chemical selected from the group consisting of silicon, metals, electron-donating atoms, and electron-donating groups.

### Claim 31 (depends on 16)

The method of claim 16, wherein the second reactant is a reductant or oxidant.

### Claim 32 (depends on 16)

The method of claim 16, wherein the cycle of the atomic layer deposition further comprises purging the chamber between each exposing operation.

### Claim 33

An apparatus for processing semiconductor substrates, the apparatus comprising:
(a) one or more stations, each reaction station comprising a pedestal for holding a substrate;
(b) at least one outlet for coupling to a vacuum;
(c) one or more process gas inlets for coupling to precursor and reactant sources;
(d) a robot for inserting substrates into the one or more reaction chambers; and
(e) a controller for controlling operations in the apparatus, comprising machine-readable instructions for:
(i) inserting a substrate into one of the one or more stations,
(ii) introducing a soak gas for a duration of about 500 seconds or less;
(iii) introducing a silicon-containing precursor for a duration sufficient to substantially adsorb the silicon-containing precursor onto the surface of the substrate;
(iv) introducing a second reactant into the one or more reaction chambers and igniting a plasma; and
(v) repeating (iii) and (iv) to form a film on the substrate, the film having a thickness less than about 5 nm,
wherein the soak gas in (ii) comprises only one or more gases used in (iv).

### Claim 34 (depends on 33)

The apparatus of claim 33, wherein the controller further comprises machine-readable instructions for performing (ii) at least once after each new substrate is inserted into one of the one or more stations by the robot.

### Claim 35 (depends on 33)

The apparatus of claim 33, wherein the apparatus comprises two or more stations.