# US 2021/0343510 A1 · Quartz component with protective coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0343510 A1
- Document ID: US20210343510A1
- Status: Published application
- Kind: A1
- Application number: 17/305,883
- Filed: 2021-07-16
- Published: 2021-11-04
- Earliest claimed: 2018-03-02
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Lin Xu; Robin Koshy; John E. Daugherty; Satish Srinivasan; David Wetzel
- Web page: https://patentgrep.com/patent/US20210343510A1

## CPC

- H01J 37/32495: {Means for protecting the vessel against plasma}
- C23C 16/40: Oxides
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/4404: {Coatings or surface treatment on the inside of the reaction chamber or on parts thereof}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/45555: {applied in non-semiconductor technology}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/56: After-treatment
- H01J 37/32119: {Windows}
- H01J 37/32238: {Windows}
- H01J 37/3244: {Gas supply means}
- H01J 37/32715: {Workpiece holder}
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A quartz structure includes a protective layer comprising yttrium oxide. The quartz structure may be fabricated by: (a) receiving a quartz structure; and (b) coating the quartz structure with a protective layer comprising yttrium oxide to form a part to be used in the plasma reactor. The part has a size and shape adapted for forming a window or injector in a plasma reactor. The protective layer does not substantially change the size or shape of the quartz structure. The part may be installed in the plasma reactor at a location where, during operation, a plasma will contact or be proximate to the part.

## Claims

### Claim 1

A method comprising:
(a) receiving a quartz structure; and
(b) coating the quartz structure with a protective layer comprising yttrium oxide to form a quartz component for a plasma reactor,
wherein the quartz component has a size and shape adapted for forming a part to be used in the plasma reactor.

### Claim 2 (depends on 1)

The method of claim 1, wherein the protective layer does not substantially change the size or shape of the quartz structure.

### Claim 3 (depends on 1)

The method of claim 1, further comprising installing the quartz component in the plasma reactor at a location where, during operation, a plasma will contact or be proximate to the quartz component.

### Claim 4 (depends on 1)

The method of claim 1, wherein the plasma reactor is an etching tool, an ashing tool, and/or a deposition tool.

### Claim 5 (depends on 1)

The method of claim 1, wherein the quartz component has a size and shape to serve as a window between a plasma source located exterior to the plasma reactor and an interior region of the plasma reactor.

### Claim 6 (depends on 1)

The method of claim 1, wherein coating the quartz structure with a protective layer comprising yttrium oxide comprises depositing the protective layer by an atomic layer deposition (ALD) process.

### Claim 7 (depends on 6)

The method of claim 6, wherein the ALD process is a plasma-enhanced process.

### Claim 8 (depends on 6)

The method of claim 6, wherein the quartz structure, prior to coating the quartz structure with a protective layer comprising yttrium oxide, has a hydroxyl-terminated surface.

### Claim 9 (depends on 6)

The method of claim 6, wherein the ALD process comprises one or more cycles of:
exposing the quartz structure to a yttrium-containing species; and
exposing the quartz structure to an oxygen-containing species.

### Claim 10 (depends on 9)

The method of claim 9, wherein the oxygen-containing species is water.

### Claim 11 (depends on 1)

The method of claim 1, wherein coating the quartz structure with a protective layer comprising yttrium oxide is performed at a temperature between about 150° C. and about 500° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein coating the quartz structure with a protective layer comprising yttrium oxide is performed at a temperature between about 200° C. and about 450° C.

### Claim 13 (depends on 1)

The method of claim 1, further comprising roughening the protective layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein roughening the protective layer comprises:
exposing the protective layer to deionized water.

### Claim 15 (depends on 14)

The method of claim 14, wherein the deionized water has a temperature of between about 50° C. and 100° C.

### Claim 16 (depends on 1)

The method of claim 1, wherein the part to be used in the plasma reactor is a window or an injector.

### Claim 17 (depends on 1)

The method of claim 1, wherein the protective layer has a thickness of between about 10 nm and 10 μm, wherein the thickness is an average thickness over a surface of the quartz structure.

### Claim 18 (depends on 1)

The method of claim 1, wherein the protective layer has a thickness of between about 100 nm and 5 μm, wherein the thickness is an average thickness over a surface of the quartz structure.

### Claim 19 (depends on 1)

The method of claim 1, wherein the quartz structure has a surface roughness, Ra, of between about 0.01 μm and 2 μm, wherein the surface roughness is an average surface roughness over a surface of the quartz structure.

### Claim 20 (depends on 1)

The method of claim 1, wherein the protective layer is at least about 99% by mass yttrium oxide.