# US 2021/0341004 A1 · Welded member for plated steel plate excellent in weld zone porosity resistance and fatigue properties and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0341004 A1
- Document ID: US20210341004A1
- Status: Published application
- Kind: A1
- Application number: 16/471,781
- Filed: 2018-06-18
- Published: 2021-11-04
- Earliest claimed: 2016-12-23
- Assignees: Posco
- Applicants: Posco
- Inventors: Gyu-Yeol BAE; Tae-Young LEE
- Web page: https://patentgrep.com/patent/US20210341004A1

## CPC

- F16B 5/08: by means of welds or the like (welding B23K)
- B23K 9/02: Seam welding; Backing means; Inserts
- B23K 9/09: Arrangements or circuits for arc welding with pulsed current or voltage
- B23K 9/0953: {using computing means}
- B23K 9/23: taking account of the properties of the materials to be welded
- B23K 2101/34: Coated articles {; Surface treated articles}
- F16B: DEVICES FOR FASTENING OR SECURING CONSTRUCTIONAL ELEMENTS OR MACHINE PARTS TOGETHER, e.g. NAILS, BOLTS, CIRCLIPS, CLAMPS, CLIPS OR WEDGES; JOINTS OR JOINTING (couplings for transmitting rotation F16D)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

Disclosed is a welded member for plated steel plate having excellent weld zone porosity resistance and fatigue properties and a method of manufacturing the same. The welded member for plated steel plate having excellent weld zone porosity resistance and fatigue properties according to an embodiment of the present invention comprises a weld metal portion formed by arc welding and overlapping a first member and a laminated second member so as to partially overlap the first member, wherein the toe angle (θ) of the weld metal portion is 45° or less, and the first member and the second member are plated steel plates.

## Claims

### Claim 1

A welded member for plated steel plate having excellent weld zone porosity resistance and fatigue properties comprising,
a weld metal portion formed by arc welding and overlapping a first member and a laminated second member so as to partially overlap the first member,
wherein the toe angle (θ) of the weld metal portion is 45° or less, and the first member and the second member are plated steel plates.

### Claim 2 (depends on 1)

The welded member for plated steel plate according to claim 1, wherein the plated steel plate is a Zn—Mg—Al alloy plated or galvanized hot-rolled steel plate.

### Claim 3 (depends on 2)

The welded member for plated steel plate according to claim 2, wherein the hot-rolled steel plate has a tensile strength of 590 MPa or more and a thickness of 6 mm or less.

### Claim 4 (depends on 3)

The welded member for plated steel plate according to claim 3, wherein the hot-rolled steel plate is a 590FB steel.

### Claim 5 (depends on 1)

The welded member for plated steel plate according to claim 1, wherein the pore area ratio of the weld metal portion is less than 0.5%.

### Claim 6 (depends on 1)

The welded member for plated steel plate according to claim 1, wherein the fatigue strength of the weld metal portion is 250 MPa or more, and the fatigue life is 2,000,000 cycles or more with a cyclic fatigue load of 10 kN (minimum/maximum load ratio, R=0.1).

### Claim 7

A method of manufacturing a welded member for plated steel plate having excellent weld zone porosity resistance and fatigue properties comprising:
forming a weld metal portion through arc welding and overlapping a first member and a laminated second member so as to partially overlap the first member, wherein the first member and the second member are plated steel plates,
supplying a welding current to a solid wire to generate an arc,
wherein the welding current is a pulse current repeated with a first peak and a second peak having a current value smaller than the first peak as one pulse period, and
a welding molten metal stirring wave frequency defined by the following formula (1) is 20 To 30 Hz.
1/(TH+TL) Formula (1)
Here, TH is a period of the first peak, and TL is a period of the second peak.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the solid wire is fed into a shielding gas which is Ar gas containing 10 to 30% of CO2 gas.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the welding current is in the range of 200 to 300 A.

### Claim 10 (depends on 7)

The method according to claim 7, wherein the diameter of solid wire: 1.0 to 1.2 mm, torch angle: 30 to 45°, push angle: 0 to 25°, and welding speed: 0.6 to 1.0 m/min.

### Claim 11 (depends on 7)

The method according to claim 7, wherein the first member and the second member are Zn—Mg—Al alloy plated or galvanized hot-rolled steel plates.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the hot-rolled steel sheet has a tensile strength of 590 MPa or more and a thickness of 6 mm or less.