# US 2021/0340978 A1 · Power end frame with residual compressive stress and methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0340978 A1
- Document ID: US20210340978A1
- Status: Published application
- Kind: A1
- Application number: 16/862,763
- Filed: 2020-04-30
- Published: 2021-11-04
- Earliest claimed: 2020-04-30
- Assignees: Caterpillar Inc.
- Applicants: Caterpillar Inc.
- Inventors: Curtis John Graham; Christopher Anthony Kinney
- Web page: https://patentgrep.com/patent/US20210340978A1

## CPC

- F04B 53/22: Arrangements for enabling ready assembly or disassembly
- B23K 9/02: Seam welding; Backing means; Inserts
- B23K 26/356: by shock processing
- B23K 26/70: Auxiliary operations or equipment
- B23K 31/003: {relating to controlling of welding distortion}
- B23P 6/04: Repairing fractures or cracked metal parts or products, e.g. castings
- E21B 43/2607: {Surface equipment specially adapted for fracturing operations}
- F04B 1/04: having cylinders in star- or fan-arrangement
- F04B 1/22: having two or more sets of cylinders or pistons
- F04B 53/16: Casings; Cylinders; Cylinder liners or heads; Fluid connections
- F04B: POSITIVE-DISPLACEMENT MACHINES FOR LIQUIDS; PUMPS (machines for liquids, or pumps, of rotary-piston or oscillating-piston type F04C; non-positive-displacement pumps F04D; pumping of fluid by direct contact of another fluid or by using inertia of fluid to be pumped F04F)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A power end frame includes a housing and a face plate secured to the housing. During use, components of the power end frame, including the housing and the face plate, are subjected to large tensile stresses. This disclosure describes a method of imparting compressive stresses in the power end frame to resist these large tensile stresses.

## Claims

### Claim 1

A method comprising:
providing a power end frame for a pump, the power end frame comprising a face plate and a housing;
forming a weld proximate a junction of the face plate and a portion of the housing; and
laser shock peening at least one of the weld or a surface proximate the weld to form a treated surface at the at least one of the weld or the surface proximate the weld, the treated surface having a residual compressive stress resulting from the laser shock peening.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
processing the weld to form a processed weld surface, wherein the laser shock peening comprises laser shock peening the processed weld surface.

### Claim 3 (depends on 2)

The method of claim 2 wherein the processing the weld comprises applying a post-weld stress relief including at least one of heating the weld or maintaining a temperature of the weld.

### Claim 4 (depends on 2)

The method of claim 2 wherein the processing the weld comprises machining the weld to form the processed weld surface.

### Claim 5 (depends on 1)

The method of claim 1, wherein the residual compressive stress extends into the at least one of the weld or the surface proximate the weld from about 4 mm to about 8 mm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the residual compressive stress is from about 200 MPa to about 300 MPa.

### Claim 7 (depends on 1)

The method of claim 1, wherein the providing the face plate and the at least the portion of the housing comprises providing the power end frame, the method further comprising:
identifying a damaged portion of the power end frame proximate the face plate and the at least the portion of the housing,
wherein the forming the weld comprises forming the weld proximate the damaged portion.

### Claim 8 (depends on 7)

The method of claim 7, further comprising:
machining the damaged portion of the power end frame prior to forming the weld proximate the damaged portion.

### Claim 9 (depends on 8)

The method of claim 8 wherein the machining comprises grinding the damaged portion to remove an existing weld.

### Claim 10

A pump comprising:
a fluid end; and
a power end connected to the fluid end, the power end comprising:
a face plate;
a housing;
a weld formed on at least one of the face plate or the housing; and
a treated surface on at least one of the weld or a surface proximate the weld, the treated surface having a residual compressive stress formed by laser shock peening.

### Claim 11 (depends on 10)

The pump of claim 10 wherein the weld is formed at a junction of the face plate and the housing to secure the face plate to the housing.

### Claim 12 (depends on 10)

The pump of claim 10 wherein the treated surface is a machined surface, machined prior to the laser shock peening forming the residual compressive stress.

### Claim 13 (depends on 10)

The pump of claim 10 wherein the residual compressive stress is from about 200 MPa to about 300 MPa.

### Claim 14 (depends on 10)

The pump of claim 10 wherein the residual compressive stress extends into the treated surface from about 4 mm to about 8 mm.

### Claim 15 (depends on 10)

The pump of claim 10 further comprising:
a first end plate secured to a first end of the housing at a first junction;
a second end plate secured to a second end of the housing at a second junction; and
at least one additional treated surface proximate at least one of the first junction or the second junction.

### Claim 16

A method of repairing a damaged power end of a pump, the method comprising:
providing the damaged power end;
identifying a damaged portion of the damaged power end;
removing material proximate the damaged portion to create one or more machined surfaces;
forming a weld on the one or more machined surfaces; and
laser shock peening at least one of the weld or a surface proximate the weld to form a treated surface at the at least one of the weld or the surface proximate the weld, the treated surface having a residual compressive stress resulting from the laser shock peening.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
processing the weld to form a processed weld surface, wherein the laser shock peening comprises laser shock peening the processed weld surface.

### Claim 18 (depends on 17)

The method of claim 17, wherein the processing the weld comprises at least one of applying a post-weld stress relief or machining the weld to form the processed weld surface.

### Claim 19 (depends on 16)

The method of claim 16, wherein the residual compressive stress extends into the at least one of the weld or the surface proximate the weld from about 4 mm to about 8 mm.

### Claim 20 (depends on 16)

The method of claim 16, wherein the residual compressive stress is from about 200 MPa to about 300 MPa.