# US 2021/0340670 A1 · In situ protective coating of chamber components for semiconductor processing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0340670 A1
- Document ID: US20210340670A1
- Status: Published application
- Kind: A1
- Application number: 17/309,032
- Filed: 2019-10-08
- Published: 2021-11-04
- Earliest claimed: 2018-10-19
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Akhil Singhal; David Charles Smith; Karl Frederick Leeser
- Web page: https://patentgrep.com/patent/US20210340670A1

## CPC

- C23C 16/4404: {Coatings or surface treatment on the inside of the reaction chamber or on parts thereof}
- C23C 16/345: {Silicon nitride}
- C23C 16/402: {Silicon dioxide}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C23C 16/56: After-treatment
- H10P 72/0462: {characterised by the construction of the processing chambers, e.g. modular processing chambers}
- C23C 16/45544: {characterized by the apparatus}
- H01J 37/32477: {characterised by the means for protecting vessels or internal parts, e.g. coatings}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

An in situ protective coating is deposited on surfaces of chamber components of a reaction chamber at high temperatures. The in situ protective coating may be deposited at a temperature greater than about 200° C. to provide a high quality coating that is resistant to certain types of halogen chemistries, such as fluorine-based species, chlorine-based species, bromine-based species, or iodine-based species. Subsequent coatings or layers may be deposited on the in situ protective coating having different etch selectivities than the underlying in situ protective coating. The in situ protective coating may be deposited throughout the reaction chamber to deposit on surfaces of the chamber components, including on chamber walls.

## Claims

### Claim 1

A method comprising:
introducing a first reactant in a gas phase into a reaction chamber to adsorb onto surfaces of a plurality of chamber components, wherein the plurality of chamber components are part of the reaction chamber; and
introducing a second reactant in a gas phase into the reaction chamber, wherein the first reactant and the second reactant react to deposit a protective coating on the surfaces of the plurality of chamber components at a temperature greater than about 200° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first reactant reacts with the second reactant in a plasma-enhanced atomic layer deposition (PEALD) process.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
controlling a radio-frequency (RF) signal supplied to the reaction chamber to cause a substantial portion of a plasma glow discharge of the second reactant to form in one or more areas outside an area between an upper electrode and a lower electrode.

### Claim 4 (depends on 3)

The method of claim 3, wherein a phase difference between a first phase of the RF signal supplied to the upper electrode and a second phase of the RF signal supplied to the lower electrode is between about 180 degrees out-of-phase and 0 degrees out-of-phase.

### Claim 5 (depends on 4)

The method of claim 4, wherein the phase difference is about 0 degrees out-of-phase.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first reactant reacts with the second reactant in a thermal ALD process.

### Claim 7 (depends on 1)

The method of claim 1, wherein the protective coating includes an oxide, a nitride, a carbide, or combinations thereof.

### Claim 8 (depends on 7)

The method of claim 7, wherein the protective coating includes silicon oxide (SiO2), aluminum oxide (Al2O3), zirconium oxide (ZrO2), hafnium oxide (HfO2), tin oxide (SnO2), or silicon nitride (Si3N4).

### Claim 9 (depends on 1)

The method of claim 1, wherein one or more materials of the plurality of chamber components include aluminum (Al).

### Claim 10 (depends on 1)

The method of claim 1, wherein the plurality of chamber components include at least chamber walls of the reaction chamber.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
depositing a film material on a wafer in the reaction chamber and on the protective coating; and
etching the film material on the wafer and on the protective coating, wherein the film material is etched at a substantially greater rate than the protective coating.

### Claim 12 (depends on 11)

The method of claim 11, wherein an etchant used for etching the film material includes a fluorine-based species, a chlorine-based species, a bromine-based species, an iodine-based species, or combinations thereof.

### Claim 13 (depends on 11)

The method of claim 11, further comprising:
re-depositing the protective coating on the surfaces of the plurality of chamber components in the reaction chamber after etching the film material.

### Claim 14 (depends on 1)

The method of claim 1, wherein the first reactant reacts with the second reactant to deposit the protective coating on the surfaces of the plurality of chamber components at a temperature between about 250° C. and about 650° C.

### Claim 15

A method comprising:
depositing a protective coating on surfaces of a plurality of chamber components in a reaction chamber, wherein the plurality of chamber components are part of the reaction chamber, wherein the protective coating is deposited at a temperature greater than about 200° C. by plasma-enhanced chemical vapor deposition (PECVD), plasma-enhanced atomic layer deposition (PEALD), or thermal atomic layer deposition (thermal ALD).

### Claim 16 (depends on 15)

The method of claim 15, further comprising:
depositing, on the surfaces of the plurality of chamber components in the reaction chamber, a film material on the protective coating, wherein the film material is etched at a substantially greater rate than the protective coating during exposure to a fluorine-based species, chlorine-based species, bromine-based species, or iodine-based species.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
re-depositing the protective coating on the surfaces of the plurality of chamber components in the reaction chamber after exposure to the fluorine-based species, chlorine-based species, bromine-based species, or iodine-based species.

### Claim 18 (depends on 16)

The method of claim 16, wherein the protective coating is deposited by PECVD or PEALD, wherein the method further comprises:
controlling a radio-frequency (RF) signal supplied to the reaction chamber to cause a substantial portion of a plasma glow discharge to form in one or more areas outside an area between an upper electrode and a lower electrode.

### Claim 19 (depends on 18)

The method of claim 18, wherein a phase difference between a first phase of the RF signal supplied to the upper electrode and a second phase of the RF signal supplied to the lower electrode is about 0 degrees out-of-phase.

### Claim 20 (depends on 15)

The method of claim 15, wherein the protective coating includes silicon oxide (SiO2), aluminum oxide (Al2O3), zirconium oxide (ZrO2), hafnium oxide (HfO2), tin oxide (SnO2), or silicon nitride (Si3N4), and wherein one or more materials of the plurality of chamber components include aluminum (Al).