# US 2021/0340667 A1 · Pulsed directed energy deposition based fabrication of hybrid titanium/aluminum material for enhanced corrosion resistance and strength

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0340667 A1
- Document ID: US20210340667A1
- Status: Published application
- Kind: A1
- Application number: 17/375,508
- Filed: 2021-07-14
- Published: 2021-11-04
- Earliest claimed: 2020-02-04
- Assignees: Hamilton Sundstrand Corporation
- Applicants: Hamilton Sundstrand Corporation
- Inventors: Tahany Ibrahim El-Wardany; Ranadip Acharya; Colette Opsahl Fennessy; Matthew Pess
- Web page: https://patentgrep.com/patent/US20210340667A1

## CPC

- C23C 14/16: on metallic substrates or on substrates of boron or silicon
- C23C 28/02: only coatings {only including layers} of metallic material
- B23K 15/0086: {welding for purposes other than joining, e.g. build-up welding}
- C23C 14/025: {Metallic sublayers}
- C23C 14/28: by wave energy or particle radiation (C23C14/32 - C23C14/48 take precedence)
- C23C 24/08: by application of heat or pressure and heat (C23C24/04 takes precedence)
- C23C 24/082: {without intermediate formation of a liquid in the layer}
- C23C 24/087: {Coating with metal alloys or metal elements only}
- C23C 24/10: with intermediate formation of a liquid phase in the layer
- C23C 24/106: {Coating with metal alloys or metal elements only}
- C23C 28/021: {including at least one metal alloy layer}
- C23C 28/026: {including at least one amorphous metallic material layer}
- C23C 28/028: {Including graded layers in composition or in physical properties, e.g. density, porosity, grain size}
- Y10T 428/12736: Al-base component
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of providing a protective titanium layer to an outer surface of an aluminum component includes providing an aluminum component and forming a first layer of titanium-based bulk metallic glass on the component, wherein formation of the bulk metallic glass layer comprises depositing a titanium alloy powder using pulsed directed energy deposition.

## Claims

### Claim 1

A method of providing a protective titanium layer to an outer surface of an aluminum component, the method comprising:
providing an aluminum component; and
forming a first layer of titanium-based bulk metallic glass on the component, wherein formation of the bulk metallic glass layer comprises depositing a titanium alloy powder using pulsed directed energy deposition.

### Claim 2 (depends on 1)

The method of claim 1 and further comprising applying vibrational energy to the component during deposition of a second layer of the titanium alloy powder to introduce crystalline phases into the second layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein vibrational energy is applied by an ultrasonic transducer.

### Claim 4 (depends on 2)

The method of claim 2, wherein vibrational energy is applied intermittently to form both crystalline phases and amorphous phases in the second layer.

### Claim 5 (depends on 2)

The method of claim 2, wherein crystalline phases are introduced in an amount to provide a tensile ductility of at least ten percent.

### Claim 6 (depends on 2)

The method of claim 2, and further comprising depositing a magnesium-containing powder using directed energy deposition to form an insulating layer between the component and the first layer of titanium-based bulk metallic glass.

### Claim 7 (depends on 2)

The method of claim 2, wherein forming the first layer of titanium-based bulk metallic glass further comprises simultaneously depositing a magnesium-containing powder using pulsed directed energy deposition.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first layer of titanium-based bulk metallic glass comprises a plurality of sub-layers and wherein depositing the magnesium-containing powder comprises depositing an amount of magnesium-containing powder that decreases with successive sub-layers.

### Claim 9 (depends on 2)

The method of claim 2 and further comprising forming a third layer of titanium-based bulk metallic glass on the component, wherein the second layer is formed between the first layer and the third layer.

### Claim 10 (depends on 2)

The method of claim 2, and further comprising:
modeling a target microstructure for each of a plurality of titanium alloy layers; and
devising a deposition process based on the microstructure model, wherein devising the deposition process comprises determining a schedule for applying vibrational energy.

### Claim 11 (depends on 2)

The method of claim 2, wherein the titanium alloy powder has a melting point not exceeding 250 K greater than a melting point of the aluminum component.

### Claim 12 (depends on 2)

The method of claim 2, wherein the component is an airfoil and the titanium-based bulk metallic glass layer is formed on a leading edge of the airfoil.

### Claim 13

A method of providing a protective titanium layer to an aluminum component, the method comprising:
forming a first titanium-based layer on the component, wherein the first titanium-based layer is a bulk metallic glass characterized by an amorphous microstructure, and wherein forming the first titanium-based layer comprises:
depositing titanium alloy powder on an outer surface of the aluminum component; and
pulsing energy directly to titanium alloy powder to melt the titanium alloy powder.

### Claim 14 (depends on 13)

The method of claim 13 and further comprising forming a second titanium-based layer on the component, wherein forming the second titanium-based layer comprises:
depositing titanium alloy powder;
pulsing energy directly to titanium alloy powder to melt the titanium alloy powder; and
applying vibrational energy to the component to introduce crystalline phases into the second titanium-based layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein crystalline phases are introduced in an amount to provide a tensile ductility of at least ten percent.

### Claim 16 (depends on 14)

The method of claim 14, wherein vibrational energy is applied intermittently to form both crystalline phases and amorphous phases in the second titanium-based layer.

### Claim 17 (depends on 14)

The method of claim 14, and further comprising depositing a magnesium-containing powder using directed energy deposition to form an insulating layer between the component and the first titanium-based layer.

### Claim 18 (depends on 14)

The method of claim 14, wherein forming the first titanium-based layer further comprises simultaneously depositing a magnesium-containing powder using pulsed directed energy deposition.

### Claim 19 (depends on 14)

The method of claim 14, wherein forming the first titanium-based layer comprises solidifying the melted titanium alloy powder by cooling at a rate of 105-106 K/s.