# US 2021/0335513 A1 · Solidifying method of hydroxides of radionuclides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0335513 A1
- Document ID: US20210335513A1
- Status: Published application
- Kind: A1
- Application number: 16/859,465
- Filed: 2020-04-27
- Published: 2021-10-28
- Earliest claimed: 2020-04-27
- Assignees: Korea Atomic Energy Research Institute
- Inventors: Hee Chul Eun; Na On Chang; Seon Byeong Kim; Wang Kyu Choi; Sang Yoon Park; Hui Jun Won; Man Soo Choi; Byung Seon Choi; Jei Kwon Moon; Chong Hun Jung; Song Bok Lee; Sang Hun Lee; Bum Kyoung Seo
- Web page: https://patentgrep.com/patent/US20210335513A1

## CPC

- G21F 9/305: {Glass or glass like matrix (C03B5/005 takes precedence; compositional aspects C03C)}
- B09B 3/29: involving a melting or softening step
- C03B 5/005: {of glass-forming waste materials (disposal or transformation of solid waste in general B09B; treatment of radioactive waste G21F9/00)}
- C03B 5/06: in pot furnaces {(C03B5/02 takes precedence)}
- C03C 1/002: {Use of waste materials, e.g. slags}
- C03C 3/066: containing zinc
- C03C 4/0042: {for glass comprising or including particular isotopes}
- C03C 4/087: {for X-rays absorbing glass}
- C03C 14/004: {the non-glass component being in the form of particles or flakes}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C 2214/14: Waste material, e.g. to be disposed of
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- G21F: PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR (radiation protection by pharmaceutical means A61K8/00, A61Q17/04; in cosmonautic vehicles B64G1/54; combined with a reactor G21C11/00; combined with X-ray tubes H01J35/16; combined with X-ray apparatus H05G1/02)
- B09B: DISPOSAL OF SOLID WASTE NOT OTHERWISE PROVIDED FOR
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure provides a solidifying method of a radionuclide. The solidifying method of the radionuclide includes operations of: providing a low melting point glass including Bi2O3, B2O3, ZnO and SiO2; providing a glass mixture mixing a mixture to be treated containing a hydroxide of radionuclide and BaSO4 and the low melting point glass; and heating the glass mixture.

## Claims

### Claim 1

A solidifying method of a radionuclide, comprising operations of:
providing a low melting point glass including Bi2O3, B2O3, ZnO and SiO2;
providing a glass mixture by mixing a mixture to be treated containing a hydroxide of radionuclide and BaSO4, and the low melting point glass; and
heating the glass mixture.

### Claim 2 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the radionuclide comprises at least one selected from a group consisting of radioisotopes of chromium, cobalt, iron and nickel metals.

### Claim 3 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the low melting point glass has a melting point of 440 to 460° C.

### Claim 4 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the mixture to be treated is a waste of HyBRID decontamination process.

### Claim 5 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the mixture to be treated contains BaSO4 in an amount of 90% to 97% by weight, based on a total weight of the mixture to be treated.

### Claim 6 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the mixture to be treated is included in an amount of 15% to 20% by weight in the glass mixture, based on a total weight of the glass mixture.

### Claim 7 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the mixture to be treated and the low melting point glass are provided as powders, respectively.

### Claim 8 (depends on 7)

The solidifying method of the radionuclide of claim 7, wherein the powder of the low melting point glass powder is a powder having a particle size of 0.8 to 1.2 times an average particle size of the powder of the mixture to be treated.

### Claim 9 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the operation of heating the glass mixture is performed at 500 to 550° C.

### Claim 10 (depends on 1)

The solidifying method of the radionuclide of claim 1, wherein the low melting point glass is obtained by including operations of: mixing Bi2O3, B2O3, ZnO and SiO2 powder particles; melting the mixed powder; cooling the molten material; and drying the cooled material.

### Claim 11 (depends on 10)

The solidifying method of the radionuclide of claim 10, wherein the operation of mixing Bi2O3, B2O3, ZnO and SiO2 powder particles is performed by mixing 32 to 38 mol % of Bi2O3, 25 to 30 mol % of B2O3, 29 to 35 mol % of ZnO, and 5 to 7 mol % of SiO2, based on the total number of moles of the powder.

### Claim 12 (depends on 10)

The solidifying method of the radionuclide of claim 10, further comprising an operation of: pulverizing such that the average particle size of the low melting point glass powder is 180 to 220 mesh.