# US 2021/0333703 A1 · Extreme Ultraviolet Mask Blank Defect Reduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0333703 A1
- Document ID: US20210333703A1
- Status: Published application
- Kind: A1
- Application number: 17/234,996
- Filed: 2021-04-20
- Published: 2021-10-28
- Earliest claimed: 2020-04-23
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc
- Inventors: Wen Xiao; Vibhu Jindal; Weimin Li; Sanjay Bhat; Azeddine Zerrade
- Web page: https://patentgrep.com/patent/US20210333703A1

## CPC

- G03F 1/24: Reflection masks; Preparation thereof
- G03F 1/72: Repair or correction of mask defects
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Extreme ultraviolet (EUV) mask blanks and methods for their manufacture, and production systems therefor are disclosed. The method for forming an EUV mask blank comprises smoothing out surface defects on a surface of a substrate.

## Claims

### Claim 1

A method of manufacturing an extreme ultraviolet (EUV) mask blank, the method comprising:
scanning a surface of a glass substrate comprising pits and scratches with a laser, the glass substrate having a softening point temperature;
melting the surface to form a molten mass to fill the pits and scratches; and
cooling the molten mass and forming a cooled, smooth surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the cooled, smooth surface has an average roughness of less than 0.1 nm.

### Claim 3 (depends on 1)

The method of claim 1, further comprising depositing a metal smoothing layer on the glass substrate.

### Claim 4 (depends on 3)

The method of claim 3, wherein the metal smoothing layer has a thickness in a range of from 2 nm to 50 nm.

### Claim 5 (depends on 3)

The method of claim 3, wherein melting the surface comprises melting the metal smoothing layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the metal smoothing layer comprises a metal having a melting point that is of from 200 to 400° C. lower than the softening point temperature of the glass substrate.

### Claim 7 (depends on 6)

The method of claim 6, comprises a metal selected from the group consisting of zinc, aluminum, brass, magnesium, silver, copper and alloys thereof.

### Claim 8 (depends on 5)

The method of claim 5, wherein the cooled, smooth surface has an average roughness of less than 0.1 nm.

### Claim 9 (depends on 5)

The method of claim 5, wherein the glass substrate further comprises bumps and particles, and the metal smoothing layer covers the pits and bumps so that the cooled, smooth surface has an average roughness of less than 0.1 nm.

### Claim 10

A method of manufacturing an extreme ultraviolet (EUV) mask blank, the method comprising:
depositing a metal smoothing layer on a surface of a glass substrate comprising pits and scratches, the glass substrate having a softening point temperature;
melting the metal smoothing layer to form a molten mass; and
filling the pits and scratches with the molten mass; and
cooling the glass substrate to form a cooled, smooth surface.

### Claim 11 (depends on 10)

The method of claim 10, wherein the melting the metal smoothing layer is performed in rapid thermal processing chamber.

### Claim 12 (depends on 11)

The method of claim 11, wherein the metal smoothing layer comprises a metal having a melting point that is of from 200 to 400° C. lower than the softening point temperature of the glass substrate.

### Claim 13 (depends on 12)

The method of claim 12, wherein the metal smoothing layer comprises a metal selected from the group consisting of zinc, aluminum, brass, magnesium, silver, copper and alloys thereof.

### Claim 14 (depends on 12)

The method of claim 12, wherein the cooled, smooth surface has an average roughness of less than 0.1 nm.

### Claim 15 (depends on 12)

The method of claim 12, wherein the glass substrate further comprises bumps and particles, and the metal smoothing layer covers the pits and bumps so that the cooled, smooth surface has an average roughness of less than 0.1 nm.

### Claim 16 (depends on 12)

The method of claim 12, wherein the metal smoothing layer is heated to a temperature in a range of from 400° C. to 1100° C. at a heating ramp rate exceeding 100° C./second.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal smoothing layer is heated to a temperature in a range of from 400° C. to 1100° C. from 5 seconds to 10 minutes.

### Claim 18

An extreme ultraviolet mask blank comprising:
a glass substrate comprising a softening point temperature and pits, scratches, bumps and particles on a surface of the glass substrate;
a metal smoothing layer covering the pits, scratches, bumps and particles, wherein the metal smoothing layer comprises a metal having a melting point that is of from 200 to 400° C. lower than the softening point temperature of the glass substrate; and
a multilayer stack reflective of EUV radiation on the metal smoothing layer.

### Claim 19 (depends on 18)

The extreme ultraviolet mask blank of claim 18, wherein the metal smoothing layer comprises a metal selected from the group consisting of zinc, aluminum, brass, magnesium, silver, copper and alloys thereof.

### Claim 20 (depends on 19)

The extreme ultraviolet mask blank of claim 19, wherein the multilayer stack comprises alternating layers of silicon and molybdenum.