# US 2021/0333677 A1 · Electrochromic polyamic acid material, preparation method thereof, and display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0333677 A1
- Document ID: US20210333677A1
- Status: Published application
- Kind: A1
- Application number: 16/496,963
- Filed: 2019-06-14
- Published: 2021-10-28
- Earliest claimed: 2019-05-21
- Assignees: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Applicants: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Inventors: Yamin WANG
- Web page: https://patentgrep.com/patent/US20210333677A1

## CPC

- C09K 11/06: containing organic luminescent materials
- C08G 73/101: {containing chain terminating or branching agents}
- C08G 73/1032: {characterised by the solvent(s) used}
- C08G 73/1042: {Copolyimides derived from at least two different tetracarboxylic compounds or two different diamino compounds}
- C08G 73/105: {with oxygen only in the diamino moiety}
- C08G 73/1078: {wholly aromatic in the diamino moiety}
- C08G 73/1085: {Polyimides with diamino moieties or tetracarboxylic segments containing heterocyclic moieties}
- G02F 1/15165: {Polymers}
- G02F 1/157: Structural association of cells with optical devices, e.g. reflectors or illuminating devices
- G02F 1/163: Operation of electrochromic cells, e.g. electrodeposition cells; Circuit arrangements therefor
- H10K 59/50: OLEDs integrated with light modulating elements, e.g. with electrochromic elements, photochromic elements or liquid crystal elements
- H10K 85/111: {comprising aromatic, heteroaromatic, or aryl chains, e.g. polyaniline, polyphenylene or polyphenylene vinylene}
- H10K 85/151: {Copolymers}
- C09K 2211/1425: Non-condensed systems
- C09K 2211/1433: bridged by heteroatoms, e.g. N, P, Si or B
- C09K 2211/1466: containing nitrogen as the only heteroatom
- G02F 1/1516: comprising organic material
- G02F 2202/022: polymeric
- G02F 2202/046: fluorescent
- H10K 50/15: Hole transporting layers
- H10K 50/17: Carrier injection layers
- H10K 2101/50: Oxidation-reduction potentials, e.g. excited state redox potentials
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present invention provides an electrochromic polyamic acid material, a preparation method thereof and a display device, wherein the molecular structure of the electrochromic polyamic acid material includes oligoaniline and carbazolyl triphenylamine. The oligoaniline serves as an electrochemically sensitive group, and the carbazolyl triphenylamine serves as a fluorescence emitting group. The electrochromic polyamic acid material is an electrically controlled fluorescent polymer. Fluorescence intensity of the electrochromic polyamic acid material undergoes reversible fluorescence conversion with a change of an applied voltage, due to a redox reaction of the oligoaniline at different voltages, resulting in an interchange between a benzene ring and an anthracene ring in a molecular structure, and an electron/energy transfer path with the fluorescence emitting group are generated or eliminated, thereby realizing the electrically controlled fluorescent properties of the electrochromic polyamic acid material.

## Claims

### Claim 1

An electrochromic polyamic acid material, comprising a molecular structure represented by formula below:
wherein the molecular structure of the electrochromic polyamic acid material comprises oligoaniline and carbazolyltriphenylamine.

### Claim 2 (depends on 1)

The electrochromic polyamic acid material according to claim 1, wherein
the oligoaniline is an electrochemically sensitive group; and
the carbazolyltriphenylamine serves as a fluorescence emitting group.

### Claim 3

A method of preparing an electrochromic polyamic acid material, comprising following steps;
providing a first compound comprising oligoaniline, a second compound comprising carbazolyltriphenylamine, 1,2,4,5-cyclohexanetetracarboxylic dianhydride, and a first solvent;
mixing the first compound and the 1,2,4,5-cyclohexanetetracarboxylic dianhydride in a reaction vessel, and purging the reaction vessel with argon gas;
adding the second compound and the first solvent to the reaction vessel to form a first mixed solution;
magnetically stirring the first mixed solution at room temperature to carry out copolymerization reaction to obtain a second mixed solution;
stirring the second mixed solution and pouring a second solvent into the reaction vessel to form a gray precipitate; and
washing the gray precipitate with water or the second solvent, followed by drying under vacuum to obtain the electrochromic polyamic acid material.

### Claim 4 (depends on 3)

The method of preparing the electrochromic polyamic acid material according to claim 3, wherein
the first compound is an electroactive diamine monomer;
the second compound is 4,40-diamino-400-N-carbazolyltriphenylamine;
the first compound, the second compound, and the 1,2,4,5-cyclohexanetetracarboxylic dianhydride have a molar ratio of 1:1:1 to 1.2:1:1.3.

### Claim 5 (depends on 3)

The method of preparing the electrochromic polyamic acid material according to claim 3, wherein
the first solvent comprises N,N′-dimethylacetamide, dimethyl sulfoxide, N,N′-dimethylformamide, and N-methyl-2-pyrrolidone, and has a volume of 8 to 12 mL; and
the second solvent comprises methanol, and has a volume of 100 to 500 mL.

### Claim 6 (depends on 3)

The method of preparing the electrochromic polyamic acid material according to claim 3, wherein
in the step of magnetically stirring the first mixed solution at the room temperature to carry out the copolymerization reaction to obtain the second mixed solution, the copolymerization reaction is carried out for 24 to 96 hours.

### Claim 7 (depends on 3)

The method of preparing the electrochromic polyamic acid material according to claim 3, wherein
in the step of drying under vacuum to obtain the electrochromic polyamic acid material, a vacuum temperature is 300 to 475° C.

### Claim 8

A display device, comprising an electrochromic polyamic acid material comprising a molecular structure represented by formula below:
wherein the molecular structure of the electrochromic polyamic acid material comprises oligoaniline and carbazolyltriphenylamine, and the oligoaniline is an electrochemically sensitive group, and the carbazolyltriphenylamine serves as a fluorescence emitting group.

### Claim 9 (depends on 8)

The display device according to claim 8, further comprising:
a first electrode;
a hole injection layer disposed on the first electrode and made of material comprising the electrochromic polyamic acid material;
a hole transport layer disposed on the hole injection layer;
a light emitting layer disposed on the hole transport layer;
an electron transport layer disposed on the light emitting layer;
an electron injection layer disposed on the electron transport layer; and
a second electrode disposed on the electron transport layer.

### Claim 10 (depends on 9)

The display device according to claim 9, wherein
the first electrode is an anode made of indium tin oxide, and the second electrode is a cathode made of one of lithium fluoride and aluminum.