# US 2021/0333589 A1 · Liquid crystal display panel and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0333589 A1
- Document ID: US20210333589A1
- Status: Published application
- Kind: A1
- Application number: 16/627,817
- Filed: 2019-12-19
- Published: 2021-10-28
- Earliest claimed: 2019-11-27
- Assignees: Tcl China Star Optoelectronics Technology Co., Ltd.
- Applicants: TCL China Star Optoelectronics Technology Co., Ltd.
- Inventors: Dong LIAO
- Web page: https://patentgrep.com/patent/US20210333589A1

## CPC

- G02F 1/1339: Gaskets; Spacers; Sealing of cells
- G02F 1/13398: {Spacer materials; Spacer properties}
- G02F 1/1303: {Apparatus specially adapted to the manufacture of LCDs}
- G02F 2202/022: polymeric
- G02F 2202/28: Adhesive materials or arrangements
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

The present invention provides a liquid crystal display panel and a manufacturing method thereof. By mixing a spacer particle composite in a sealant, wherein temperature-responsive polymer vesicles comprise temperature-responsive polymer bodies and free radical inhibitors encapsulated by the temperature-responsive polymer bodies, and the temperature-responsive polymer vesicles release the free radical inhibitors at a default temperature, thereby preventing orientation dark lines or uneven peripheral brightnesses when the liquid crystal display panel displays.

## Claims

### Claim 1

A liquid crystal display panel, comprising:
a first substrate, a second substrate disposed opposite to the first substrate, a sealant disposed between the first substrate and the second substrate, and liquid crystal molecules disposed in a cavity surrounded by the first substrate, the second substrate, and the sealant;
wherein temperature-responsive polymer vesicles are disposed within the sealant, the temperature-responsive polymer vesicles comprise temperature-responsive polymer bodies and free radical inhibitors encapsulated by the temperature-responsive polymer bodies, and the temperature-responsive polymer vesicles release the free radical inhibitors under a default temperature condition.

### Claim 2 (depends on 1)

The liquid crystal display panel as claimed in claim 1, further comprising a plurality of spacer particles dispersed in the sealant, wherein each of the temperature-responsive polymer vesicles is disposed on a surface of one of the spacer particles.

### Claim 3 (depends on 2)

The liquid crystal display panel as claimed in claim 2, wherein a size of each of the spacer particles is 2 μm to 6 μm.

### Claim 4 (depends on 2)

The liquid crystal display panel as claimed in claim 2, wherein a mass ratio of the spacer particles to the sealant is (0.5˜1.5):100.

### Claim 5 (depends on 1)

The liquid crystal display panel as claimed in claim 1, wherein the default temperature condition is a temperature higher than or equal to 55 degrees Celsius.

### Claim 6 (depends on 1)

The liquid crystal display panel as claimed in claim 1, wherein the temperature-responsive polymer vesicles comprise first temperature-responsive polymer vesicles and second temperature-responsive polymer vesicles, each of the first temperature-responsive polymer vesicles releases the free radical inhibitors at a temperature higher than a first threshold temperature, each of the second temperature-responsive polymer vesicles releases the free radical inhibitors at a temperature higher than a second threshold temperature, and the second threshold temperature is higher than the first threshold temperature.

### Claim 7 (depends on 6)

The liquid crystal display panel as claimed in claim 6, wherein the first threshold temperature is 55 degrees Celsius, and the second threshold temperature is 120 degrees Celsius.

### Claim 8 (depends on 1)

The liquid crystal display panel as claimed in claim 1, wherein a size of each of the temperature-responsive polymer vesicles is 10 nm to 500 nm.

### Claim 9 (depends on 1)

The liquid crystal display panel as claimed in claim 1, wherein a material of the sealant comprises a matrix resin, a photoinitiator, and a crosslinking agent.

### Claim 10 (depends on 1)

The liquid crystal display panel as claimed in claim 1, wherein a material of the temperature-responsive polymer bodies is polyoxyethylene-b-poly N-isopropylacrylamide, and the free radical inhibitors are made of a material selected from at least one of 2,6-di-tert-butyl-4-methylphenol and tetramethylpiperidine nitrogen oxide.

### Claim 11

A manufacturing method of a liquid crystal display panel, comprising following steps of:
coating a mixture of an adhesive and a spacer particle composite on a first substrate to form a frame-shaped sealant, wherein the spacer particle composite comprises spacer particles and temperature-responsive polymer vesicles, each of the temperature-responsive polymer vesicles is disposed on a surface of one of the spacer particles, the temperature-responsive polymer vesicles comprise temperature-responsive polymer bodies and free radical inhibitors encapsulated by the temperature-responsive polymer bodies, the temperature-responsive polymer vesicles release the free radical inhibitors under a default temperature condition, and the adhesive comprises a matrix resin, a photoinitiator, and a crosslinking agent;
disposing a second substrate on the frame-shaped sealant to make the first substrate and the second substrate are disposed opposite with each other;
irradiating the frame-shaped sealant with ultraviolet; and
heating the frame-shaped sealant after an irradiation of the ultraviolet to 80 degrees Celsius to 130 degrees Celsius.

### Claim 12 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein a mass ratio of the spacer particles to the adhesive is (0.5˜1.5):100.

### Claim 13 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein an accumulated light of the ultraviolet is 1000 mJ to 6000 mJ.

### Claim 14 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein heating the frame-shaped sealant after the irradiation of the ultraviolet to 120 degrees Celsius for a time of 50 minutes to 60 minutes.

### Claim 15 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein the default temperature condition is a temperature higher than or equal to 55 degrees Celsius.

### Claim 16 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein a size of each of the temperature-responsive polymer vesicles is 10 nm to 500 nm.

### Claim 17 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein a size of each of the spacer particles is 2 μm to 6 μm.

### Claim 18 (depends on 11)

The manufacturing method of the liquid crystal display panel as claimed in claim 11, wherein a material of the temperature-responsive polymer bodies is polyoxyethylene-b-poly N-isopropylacrylamide, and the free radical inhibitors are made of a material selected from at least one of 2,6-di-tert-butyl-4-methylphenol and tetramethylpiperidine nitrogen oxide.