# US 2021/0332503 A1 · Infrared reflecting fiber and fabricating method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332503 A1
- Document ID: US20210332503A1
- Status: Published application
- Kind: A1
- Application number: 16/941,584
- Filed: 2020-07-29
- Published: 2021-10-28
- Earliest claimed: 2020-04-28
- Assignees: Taiwan Textile Research Institute
- Applicants: Taiwan Textile Research Institute
- Inventors: Sheng-Shan CHANG; Jo-Cheng CHIANG; Chao-Huei LIU
- Web page: https://patentgrep.com/patent/US20210332503A1

## CPC

- D01F 1/106: {Radiation shielding agents, e.g. absorbing, reflecting agents}
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C09C 1/3623: {Grinding}
- C09C 1/363: {Drying, calcination}
- C09C 1/3669: {Treatment with low-molecular organic compounds}
- C09C 1/62: Metallic pigments or fillers {(C09C1/0015 takes precedence)}
- D01F 6/62: from polyesters
- D01F 6/92: of polyesters
- C01P 2002/54: one element only
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/62: L* (lightness axis)
- C01P 2006/63: a* (red-green axis)
- C01P 2006/64: b* (yellow-blue axis)
- C08L 2203/12: used for fibers
- D01F 8/14: with at least one polyester as constituent
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

An infrared reflecting fiber includes 76.0 parts by weight to 88.5 parts by weight of a carrier, 1.8 parts by weight to 4.0 parts by weight of an infrared reflecting composition, 2.5 parts by weight to 7.5 parts by weight of a titanium dioxide containing composition, and 6.0 parts by weight to 16.0 parts by weight of a color adjusting composition. The carrier includes polyethylene terephthalate (PET). When a content of 5.0 wt % to 7.5 wt % of the infrared reflecting composition and a balance of the carrier are mixed together to form a first fiber, a maximum infrared reflectivity of the first fiber is between 61% and 70%.

## Claims

### Claim 1

An infrared reflecting fiber, comprising:
76.0 parts by weight to 88.5 parts by weight of a carrier, wherein the carrier comprises polyethylene terephthalate (PET);
1.8 parts by weight to 4.0 parts by weight of an infrared reflecting composition, wherein when a content of 5.0 wt % to 7.5 wt % of the infrared reflecting composition and a balance of the carrier are mixed together to form a first fiber, a maximum infrared reflectivity of the first fiber is between 61% and 70%;
2.5 parts by weight to 7.5 parts by weight of a titanium dioxide containing composition; and
6.0 parts by weight to 16.0 parts by weight of a color adjusting composition.

### Claim 2 (depends on 1)

The infrared reflecting fiber of claim 1, wherein the infrared reflecting composition comprises 74 parts by weight to 78 parts by weight of a substrate powder, 18 parts by weight to 22 parts by weight of an infrared reflecting colorant, and 2 parts by weight to 6 parts by weight of an additive.

### Claim 3 (depends on 2)

The infrared reflecting fiber of claim 2, wherein the substrate powder comprises polybutylene terephthalate (PBT).

### Claim 4 (depends on 2)

The infrared reflecting fiber of claim 2, wherein the infrared reflecting colorant comprises a titanium-nickel-antimony metal composite material.

### Claim 5 (depends on 4)

The infrared reflecting fiber of claim 4, wherein when a content of 1.0 wt % to 1.5 wt % of the infrared reflecting colorant and a balance of the carrier are mixed together to form a second fiber, a maximum infrared reflectivity of the second fiber is between 64% and 70%.

### Claim 6 (depends on 2)

The infrared reflecting fiber of claim 2, wherein the infrared reflecting colorant comprises a chromium-iron metal composite material.

### Claim 7 (depends on 6)

The infrared reflecting fiber of claim 6, wherein when a content of 1.0 wt % to 1.5 wt % of the infrared reflecting colorant and a balance of the carrier are mixed together to form a third fiber, a maximum infrared reflectivity of the third fiber is between 61% and 63%.

### Claim 8 (depends on 2)

The infrared reflecting fiber of claim 2, wherein the additive comprises a paraffin-based dispersant and a heat stabilizer.

### Claim 9 (depends on 2)

The infrared reflecting fiber of claim 2, wherein a particle diameter of the infrared reflecting colorant is between 150 nm and 250 nm.

### Claim 10 (depends on 1)

The infrared reflecting fiber of claim 1, wherein a titanium dioxide in the titanium dioxide containing composition is rutile.

### Claim 11 (depends on 1)

The infrared reflecting fiber of claim 1, wherein the color adjusting composition comprises 74 parts by weight to 78 parts by weight of a substrate powder, 18 parts by weight to 22 parts by weight of a color adjusting colorant, and 2 parts by weight to 6 parts by weight of an additive.

### Claim 12 (depends on 11)

The infrared reflecting fiber of claim 11, wherein a particle diameter of the color adjusting colorant is between 150 nm and 250 nm.

### Claim 13

A method of fabricating an infrared reflecting fiber, comprising:
mixing 1.8 parts by weight to 4.0 parts by weight of an infrared reflecting composition, 2.5 parts by weight to 7.5 parts by weight of a titanium dioxide containing composition, 6.0 parts by weight to 16.0 parts by weight of a color adjusting composition, and 76.0 parts by weight to 88.5 parts by weight of a carrier, wherein when a content of 5.0 wt % to 7.5 wt % of the infrared reflecting composition and a balance of the carrier are mixed together to form a first fiber, a maximum infrared reflectivity of the first fiber is between 61% and 70%.

### Claim 14 (depends on 13)

The method of fabricating the infrared reflecting fiber of claim 13, wherein a method of fabricating the infrared reflecting composition comprises:
performing a liquid grinding step to an infrared reflecting colorant;
performing a drying step to form a refined infrared reflecting colorant after the liquid grinding step; and
evenly mixing 74 parts by weight to 78 parts by weight of a substrate powder, 18 parts by weight to 22 parts by weight of the refined infrared reflecting colorant, and 2 parts by weight to 6 parts by weight of an additive to obtain the infrared reflecting composition.

### Claim 15 (depends on 14)

The method of fabricating the infrared reflecting fiber of claim 14, wherein a particle diameter of the refined infrared reflecting colorant is between 150 nm and 250 nm.

### Claim 16 (depends on 14)

The method of fabricating the infrared reflecting fiber of claim 14, wherein the liquid grinding step comprises:
mixing 65 parts by weight to 80 parts by weight of a water, 20 parts by weight to 30 parts by weight of the infrared reflecting colorant, and 1 part by weight to 2 parts by weight of a liquid dispersant; and
grinding with a planetary ball mill at a speed of 100 rpm to 300 rpm for 4.5 hours to 5.5 hours.

### Claim 17 (depends on 13)

The method of fabricating the infrared reflecting fiber of claim 13, wherein a method of fabricating the titanium dioxide containing composition comprises:
performing a liquid grinding step to a titanium dioxide;
performing a drying step to form a refined titanium dioxide after the liquid grinding step; and
evenly mixing 74 parts by weight to 78 parts by weight of a substrate powder, 18 parts by weight to 22 parts by weight of the refined titanium dioxide, and 2 parts by weight to 6 parts by weight of an additive to obtain the titanium dioxide containing composition.

### Claim 18 (depends on 17)

The method of fabricating the infrared reflecting fiber of claim 17, wherein a particle diameter of the refined titanium dioxide is between 150 nm and 250 nm.

### Claim 19 (depends on 17)

The method of fabricating the infrared reflecting fiber of claim 17, wherein the liquid grinding step comprises:
mixing 65 parts by weight to 80 parts by weight of a water, 20 parts by weight to 30 parts by weight of the titanium dioxide, and 1 part by weight to 2 parts by weight of a liquid dispersant; and
grinding with a planetary ball mill at a speed of 100 rpm to 300 rpm for 4.5 hours to 5.5 hours.

### Claim 20 (depends on 13)

The method of fabricating the infrared reflecting fiber of claim 13, wherein a method of fabricating the color adjusting composition comprises:
evenly mixing 74 parts by weight to 78 parts by weight of a substrate powder, 18 parts by weight to 22 parts by weight of a color adjusting colorant, and 2 parts by weight to 6 parts by weight of an additive to obtain the color adjusting composition.