# US 2021/0332479 A1 · Method for filling a gap in a three-dimensional structure on a semiconductor substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332479 A1
- Document ID: US20210332479A1
- Status: Published application
- Kind: A1
- Application number: 17/236,782
- Filed: 2021-04-21
- Published: 2021-10-28
- Earliest claimed: 2020-04-24
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: KiKang KIM; HakYong KWON; HieChul KIM; SungKyu KANG; SeungHwan LEE; SungBae KIM; JongHyun AHN; SeongRyeong KIM; KyuMin KIM; YoungMin KIM
- Web page: https://patentgrep.com/patent/US20210332479A1

## CPC

- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/402: {Silicon dioxide}
- C23C 16/45534: {Use of auxiliary reactants other than used for contributing to the composition of the main film, e.g. catalysts, activators or scavengers}
- C23C 16/505: using radio frequency discharges
- C23C 16/56: After-treatment
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/242: {of Group IV materials}
- H10P 50/283: {by chemical means}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

This application relates to a method of filling a gap in a three-dimensional structure over a semiconductor substrate. The method may include depositing a thin film at least on a three-dimensional structure over a substrate using at least one reaction gas activated with a first radio frequency (RF) power having a first frequency, the three dimensional structure comprising a trench and/or hole. The method may also include etching the deposited thin film using at least one etchant activated with a second RF power having a second frequency lower than the first frequency. The method may further include repeating a cycle of the depositing and the etching at least once until the trench and/or hole are filled with the thin film. According to some embodiments, a thin film having substantially free of voids and/or seams can be formed in the three-dimensional structure.

## Claims

### Claim 1

A method of filling a gap in a three-dimensional structure on a semiconductor substrate, the method comprising:
depositing a thin film on the three-dimensional structure using at least one reaction gas activated with a first radio frequency (RF) power having a first frequency, wherein the three-dimensional structure comprises a trench and/or hole; and
etching the deposited thin film using at least one etchant activated with a second RF power having a second frequency lower than the first frequency.

### Claim 2 (depends on 1)

The method of claim 1, further comprising repeating a cycle of the depositing and the etching at least once until the trench and/or hole are filled with the thin film.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reaction gas comprises oxygen.

### Claim 4 (depends on 3)

The method of claim 3, wherein the reaction gas comprises at least one of O2, O3, H2O, NO2, N2O, or a combination thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first frequency is in a range of about 100 kHz to about 3,000 MHz.

### Claim 6 (depends on 5)

The method of claim 5, wherein the first frequency is in a range of about 27.12 MHz to about 100 MHz.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first RF power is in a range of about 500 watt to about 3,000 watt.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second frequency is in a range of about 100 kHz to about 5,000 kHz.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second RF Power is in a range of about 100 watts to about 500 watts.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first frequency is in a range of about 27.12 MHz to about 100 MHz, and wherein the second frequency is in a range of about 100 kHz to about 5,000 kHz.

### Claim 11 (depends on 1)

The method of claim 1, wherein the etchant comprises fluorine.

### Claim 12 (depends on 11)

The method of claim 11, wherein the etchant comprises at least one of NF3, ClF3, F2, SF6, CF4, or a combination thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein the trench and/or hole has an aspect ratio of at least about 20:1.

### Claim 14 (depends on 13)

The method of claim 13, wherein the repeating is performed about 1-10 times when a width of the trench and/or hole is at least about 200 nm.

### Claim 15 (depends on 13)

The method of claim 13, wherein the repeating is performed about 1-20 times when a width of the trench and/or hole is in a range of about 150 nm to about 200 nm.

### Claim 16 (depends on 13)

The method of claim 13, wherein the repeating is performed about 1-40 times when a width of the trench and/or hole is about 100 nm or less.

### Claim 17

A method of filling a gap in a three-dimensional structure over a semiconductor substrate, the method comprising:
depositing a thin film at least on the three-dimensional structure by a vapor deposition process comprising contacting the three-dimensional structure with a reaction gas, the three-dimensional structure comprising a trench and/or hole; and
etching the deposited thin film using at least one etchant activated with an RF power having a frequency in a range of about 3 kHz to about 13,560 kHz.

### Claim 18 (depends on 17)

The method of claim 17, further comprising repeating a cycle of the depositing and the etching at least once until the trench and/or hole are filled with the thin film.

### Claim 19 (depends on 17)

The method of claim 17, wherein the depositing comprises activating the reaction gas with a frequency in a range of about 100 kHz to about 3,000 MHz.

### Claim 20 (depends on 17)

The method of claim 17, wherein the etchant comprises at least one of NF3, CIF3, F2, SF6, CF4, or a combination thereof.