# US 2021/0332473 A1 · Methods of fabricating thin films comprising lithium-containing materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332473 A1
- Document ID: US20210332473A1
- Status: Published application
- Kind: A1
- Application number: 17/268,344
- Filed: 2019-08-13
- Published: 2021-10-28
- Earliest claimed: 2018-08-14
- Assignees: Massachusetts Institute of Technology; ETH Zurich
- Applicants: Massachusetts Institute of Technology; ETH Zurich
- Inventors: Reto Max Pfenninger; Michal Struzik; Inigo Garbayo; Andreas Nenning; Jennifer Rupp
- Web page: https://patentgrep.com/patent/US20210332473A1

## CPC

- C23C 14/3485: {using pulsed power to the target}
- H01M 6/40: Printed batteries {, e.g. thin film batteries}
- C23C 14/088: {of the type ABO3 with A representing alkali, alkaline earth metal or Pb and B representing a refractory or rare earth metal}
- C23C 14/24: Vacuum evaporation
- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- C23C 14/542: {Controlling the film thickness or evaporation rate}
- H01M 4/0423: {Physical vapour deposition}
- H01M 4/0426: {Sputtering}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 2300/0068: inorganic
- H01M 2300/0071: Oxides
- H01M 2300/0094: in the form of layered products, e.g. coatings
- Y02E 60/10: Energy storage using batteries
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Thin films of lithium-containing materials and methods for fabricating them are generally described. In some embodiments, the formation of a first vapor is induced from a first target and the formation of a second vapor is induced from a second target, resulting in the formation of a thin film. In some embodiments, at least a portion of the formation of the first vapor and the formation of the second vapor occurs under vacuum conditions. In some embodiments, the thin film has a relatively high ionic conductivity, mixed ionic/electronic conductivity, or other properties beneficial for applications such as active electrode materials or solid-state electrolytes.

## Claims

### Claim 1

A method, comprising:
inducing formation of a first vapor from a first target comprising a lithium-containing material and formation of a second vapor from a second target comprising lithium and nitrogen such that the first vapor and the second vapor are deposited on a surface, resulting in the formation of a thin film comprising a lithium-containing material on the surface,
wherein at least a portion of the formation of the first vapor and at least a portion of the formation of the second vapor occur under vacuum conditions.

### Claim 2 (depends on 1)

The method of claim 1, wherein the formation of the first vapor comprises inducing a plasma state of at least a portion of the first target.

### Claim 3 (depends on 1)

The method of claim 1, wherein the formation of the first vapor comprises sputtering, evaporation, and/or pulsed laser irradiation of at least a portion of the first target.

### Claim 4 (depends on 1)

The method of claim 1, wherein the formation of the second vapor comprises inducing a plasma state of at least a portion of the second target.

### Claim 5 (depends on 1)

The method of claim 1, wherein the formation of the second vapor comprises sputtering, evaporation, and/or pulsed laser irradiation of at least a portion of the second target.

### Claim 6 (depends on 1)

The method of claim 1, wherein the formation of the first vapor and the formation of the second vapor are induced simultaneously.

### Claim 7 (depends on 1)

The method of claim 1, wherein the formation of the first vapor and the formation of the second vapor are induced sequentially.

### Claim 8 (depends on 1)

The method of claim 1, wherein the surface and/or the thin film are held at a temperature of between 580° C. and 800° C. for at least a portion of time during the formation of the thin film.

### Claim 9 (depends on 1)

The method of claim 1, wherein the surface and/or the thin film are held at a temperature of between 15° C. and 35° C. for at least a portion of time during the formation of the thin film.

### Claim 10 (depends on 1)

The method of claim 1, wherein the surface and/or the thin film are held at a temperature of between 200° C. and 900° C. for at least a portion of time during the formation of the thin film.

### Claim 11 (depends on 1)

The method of claim 1, wherein the surface and/or the thin film are held at a first temperature for at least a portion of time during the formation of the thin film and then held at a second temperature following the formation of the thin film, wherein the second temperature is at least 100° C. higher than the first temperature.

### Claim 12 (depends on 1)

The method of claim 1, wherein the surface and/or the thin film are held at a temperature of between 580° C. and 800° C. following the formation of the thin film.

### Claim 13 (depends on 1)

The method of claim 1, wherein the surface and/or the thin film are held at a temperature of between 200° C. and 900° C. following the formation of the thin film.

### Claim 14 (depends on 1)

The method of claim 1, wherein the thin film comprises nitrogen at a lattice site.

### Claim 15 (depends on 1)

The method of claim 1, wherein the thin film comprises interstitial nitrogen.

### Claim 16 (depends on 1)

The method of claim 1, wherein the lithium-containing material of the first target and/or the lithium-containing material of the thin film comprises a lithium-containing oxide.

### Claim 17 (depends on 1)

The method of claim 1, wherein the lithium-containing material of the first target and/or the lithium-containing material of the thin film comprises a lithium metal oxide.

### Claim 18 (depends on 1)

The method of claim 1, wherein lithium-containing material of the first target and/or the lithium-containing material of the thin film comprises one or more transition metals.

### Claim 19 (depends on 1)

The method of claim 1, wherein the lithium-containing material of the first target and/or the lithium-containing material of the thin film comprises a garnet.

### Claim 20 (depends on 1)

The method of claim 1, wherein the lithium-containing material of the first target and/or the lithium-containing material of the thin film comprises a perovskite.

### Claim at position 21

21-61. (canceled)