# US 2021/0332464 A1 · Non-oriented electrical steel sheet and method of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332464 A1
- Document ID: US20210332464A1
- Status: Published application
- Kind: A1
- Application number: 17/055,601
- Filed: 2019-05-20
- Published: 2021-10-28
- Earliest claimed: 2018-05-21
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Masanori UESAKA; Yoshiaki ZAIZEN; Tomoyuki OKUBO; Hiroaki NAKAJIMA; Yoshihiko ODA
- Web page: https://patentgrep.com/patent/US20210332464A1

## CPC

- C22C 38/105: {containing Co and Ni}
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1261: {following hot rolling}
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C21D 9/68: Furnace coilers; Hot coilers (cold coilers B21C47/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- H01F 1/16: in the form of sheets (H01F1/147 takes precedence)
- H01F 1/14775: {in the form of sheets}
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a non-oriented electrical steel sheet that contains substantially no Al and contains large amounts of Si and Mn and has low iron loss, comprising a chemical composition containing C: 0.0050% or less, Si: 2.0% or more and 6.0% or less, Mn: 1.0% or more and 3.0% or less, P: 0.20% or less, S: 0.0050% or less, N: 0.0050% or less, Al: 0.0050% or less, and one or more selected from B: 0.0001% or more and 0.0050% or less, Nb: 0.0001% or more and 0.0050% or less, and V: 0.0005% or more and 0.0500% or less, with a balance consisting of Fe and inevitable impurities, wherein a number density of Si—Mn nitrides with an average diameter of 50 nm or more and 500 nm or less is 1 or less per μm3.

## Claims

### Claim 1

A non-oriented electrical steel sheet, comprising
a chemical composition containing, in mass %,
C: 0.0050% or less,
Si: 2.0% or more and 6.0% or less,
Mn: 1.0% or more and 3.0% or less,
P: 0.20% or less,
S: 0.0050% or less,
N: 0.0050% or less,
Al: 0.0050% or less, and
one or more selected from the group consisting of B: 0.0001% or more and 0.0050% or less, Nb: 0.0001% or more and 0.0050% or less, and V: 0.0005% or more and 0.0500% or less,
with a balance consisting of Fe and inevitable impurities,
wherein a number density of Si—Mn nitrides with an average diameter of 50 nm or more and 500 nm or less is 1 or less per μm3.

### Claim 2 (depends on 1)

The non-oriented electrical steel sheet according to claim 1, wherein the chemical composition further contains, in mass %, one or two selected from the group consisting of Sn: 0.01% or more and 0.50% or less and Sb: 0.01% or more and 0.50% or less.

### Claim 3 (depends on 1)

The non-oriented electrical steel sheet according to claim 1, wherein the chemical composition further contains, in mass %, one or more selected from the group consisting of Ca: 0.0001% or more and 0.0300% or less, Mg: 0.0001% or more and 0.0300% or less, and REM: 0.0001% or more and 0.0300% or less.

### Claim 4 (depends on 1)

The non-oriented electrical steel sheet according to claim 1, wherein the chemical composition further contains, in mass %, one or two selected from the group consisting of Ni: 0.01% or more and 5.00% or less and Co: 0.01% or more and 5.00% or less.

### Claim 5 (depends on 1)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 1 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less.

### Claim 6 (depends on 1)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 1 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
subjecting the hot-rolled sheet to hot-rolled sheet annealing;
thereafter cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less, and
the hot-rolled sheet after the hot-rolled sheet annealing is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more.

### Claim 7 (depends on 2)

The non-oriented electrical steel sheet according to claim 2, wherein the chemical composition further contains, in mass %, one or more selected from the group consisting of Ca: 0.0001% or more and 0.0300% or less, Mg: 0.0001% or more and 0.0300% or less, and REM: 0.0001% or more and 0.0300% or less.

### Claim 8 (depends on 2)

The non-oriented electrical steel sheet according to claim 2, wherein the chemical composition further contains, in mass %, one or two selected from the group consisting of Ni: 0.01% or more and 5.00% or less and Co: 0.01% or more and 5.00% or less.

### Claim 9 (depends on 2)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 2 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less.

### Claim 10 (depends on 2)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 2 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
subjecting the hot-rolled sheet to hot-rolled sheet annealing;
thereafter cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less, and
the hot-rolled sheet after the hot-rolled sheet annealing is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more.

### Claim 11 (depends on 3)

The non-oriented electrical steel sheet according to claim 3, wherein the chemical composition further contains, in mass %, one or two selected from the group consisting of Ni: 0.01% or more and 5.00% or less and Co: 0.01% or more and 5.00% or less.

### Claim 12 (depends on 3)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 3 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less.

### Claim 13 (depends on 3)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 3 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
subjecting the hot-rolled sheet to hot-rolled sheet annealing;
thereafter cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less, and
the hot-rolled sheet after the hot-rolled sheet annealing is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more.

### Claim 14 (depends on 4)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 4 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less.

### Claim 15 (depends on 4)

A method of producing a non-oriented electrical steel sheet, the method comprising:
hot rolling a slab having the chemical composition according to claim 4 to obtain a hot-rolled sheet;
coiling the hot-rolled sheet;
subjecting the hot-rolled sheet to hot-rolled sheet annealing;
thereafter cold rolling the hot-rolled sheet once or twice with intermediate annealing being performed therebetween, to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to final annealing,
wherein the hot-rolled sheet after the hot rolling is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more, and thereafter the coiling is performed at 650° C. or less, and
the hot-rolled sheet after the hot-rolled sheet annealing is cooled at an average cooling rate from 800° C. to 650° C. of 30° C./s or more.