# US 2021/0332392 A1 · Compositions and methods of use thereof for scandium separation from rare earth containing material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332392 A1
- Document ID: US20210332392A1
- Status: Published application
- Kind: A1
- Application number: 17/240,794
- Filed: 2021-04-26
- Published: 2021-10-28
- Earliest claimed: 2020-04-24
- Assignees: Lawrence Livermore National Security, LLC
- Applicants: Lawrence Livermore National Security, LLC
- Inventors: Dan Mcfarland Park; Ziye Dong; Yongqin Jiao
- Web page: https://patentgrep.com/patent/US20210332392A1

## CPC

- C12P 3/00: Preparation of elements or inorganic compounds except carbon dioxide {(recovery of carbon dioxides as by-products C12F3/02)}
- C22B 3/18: with the aid of microorganisms or enzymes, e.g. bacteria or algae
- C22B 59/00: Obtaining rare earth metals
- C22B 61/00: Obtaining metals not elsewhere provided for in this subclass (iron C21)
- Y02P 10/20: Recycling
- C12P: FERMENTATION OR ENZYME-USING PROCESSES TO SYNTHESISE A DESIRED CHEMICAL COMPOUND OR COMPOSITION OR TO SEPARATE OPTICAL ISOMERS FROM A RACEMIC MIXTURE {(brewing of beer C12C; producing vinegar C12J; producing specific peptides or proteins C07K; producing enzymes C12N9/00; DNA or RNA concerning genetic engineering, vectors, e.g. plasmids, or their isolation, preparation or purification C12N15/00; measuring or testing processes involving enzymes or microorganisms C12Q; measuring or testing processes involving nucleic acid amplification reactions C12Q1/6844; fermentation processes to form a food composition, A21 or A23; compounds in general, see the relevant compound class, e.g. C01, C07)}
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

This disclosure provides microbes for the preferential separation of Scandium (Sc) from rare earth element (REE) containing materials, as well as methods of use thereof.

## Claims

### Claim 1

A method for preferentially separating scandium (Sc) from a rare earth element (REE) containing material comprising the steps of:
(a) contacting microbes with the REE containing material at a pH between about 3 to about 4 to form Sc-microbe complexes; and
(b) separating the Sc from the microbes by contacting the Sc-microbe complexes with a solution comprising an organic chelator,
wherein the microbes are Arthrobacter nicotianae (A. nicotianae) microbes.

### Claim 2 (depends on 1)

The method of claim 1, wherein the organic chelator is citrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the solution comprising the organic chelator has a pH of about 5 to about 6.

### Claim 4 (depends on 1)

The method of claim 1, wherein in the contacting step (a) Sc is selectively absorbed by the microbes to form the Sc-microbe complexes and the microbes absorb substantially no other REEs, non-REE components, or any other elements in the REE containing material other than Sc.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pH of the REE containing material is incrementally adjusted from a pH of about 3 to about 4 in the contacting step (a).

### Claim 6 (depends on 1)

The method of claim 1, wherein the pH of the REE containing material is incrementally adjusted from 3 to 3.4, 3.4 to 3.6, and 3.6 to 3.8 in the contacting step (a).

### Claim 7 (depends on 1)

The method of claim 1, wherein the solution is incrementally adjusted from pH 5 to 6 in the separating step (b).

### Claim 8 (depends on 4)

The method of claim 4, wherein the other REEs are selected from the group consisting of lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), and yttrium (Y).

### Claim 9 (depends on 4)

The method of claim 4, wherein the non-REE component is a metal selected from the group consisting of iron (Fe), calcium (Ca), aluminum (Al), magnesium (Mg), zinc (Zn), nickel (Ni), sodium (Na), lithium (Li), potassium (K), cobalt (Co), manganese (Mn), and copper (Cu).

### Claim 10 (depends on 4)

The method of claim 4, wherein the non-REE component is a radionucleotide selected from the group consisting of uranyl (U) and thorium (in).

### Claim 11 (depends on 1)

The method of claim 1, wherein Sc is preferentially separated from Fe in the REE containing material.

### Claim 12 (depends on 1)

The method of claim 1, further comprising repeating steps (a) and (b) with a second, third, fourth, fifth, six, seventh, eighth, ninth, tenth or more REE containing material.

### Claim 13 (depends on 1)

The method of claim 1, wherein step (b) is repeated until at least about 100%, at least about 90%, at least about 80%, at least about 70%, at least about 60%, at least about 50%, at least about 40%, at least about 30%, at least about 20%, or at least about 10% of the Sc is separated from the Sc-microbe complexes.

### Claim 14 (depends on 1)

The method of claim 1, wherein the Sc is separated relative to any other REE, any non-REE component, and/or to any other element in a purity of at least about 10%, at least about 15%, at least about 20%, at least about 30%, at least about 40%, at least about 50%, at least about 55%, at least about 60%, at least about 65%, at least about 70%, at least about 80%, at least about 85%, at least about 90%, at least about 95%, or at least about 100%, relative to any other REE, any non-REE component, or any other element.

### Claim 15 (depends on 1)

The method of claim 1, wherein the microbes are embedded into a solid support.

### Claim 16 (depends on 1)

The method of claim 1, wherein the microbes are embedded into silicon dioxide (SiO2), polyethylene glycol diacrylate, agarose, and/or acrylamide.

### Claim 17 (depends on 15)

The method of claim 15, wherein a cell density of the microbes in the SiO2 is about 1 g/ml.

### Claim 18 (depends on 15)

The method of claim 15, wherein a cell density of the microbes in the SiO2 is about 2 g/ml.

### Claim 19 (depends on 1)

The method of claim 1, further comprising adding the microbes to a column prior to step (a).

### Claim 20 (depends on 1)

The method of claim 1, wherein Fe and/or Al are present in the REE containing material in a concentration three orders of magnitude higher than that of a concentration of Sc.

### Claim 21 (depends on 1)

The method of claim 1, wherein the solution comprises citrate.

### Claim 22 (depends on 1)

The method of claim 1, wherein the solution comprises citrate at a concentration of about 25 mM.

### Claim 23 (depends on 1)

The method of claim 1, wherein the microbes selectively bind to the Sc due to a stronger ionic interaction of Sc relative to other REEs or non-REE components.