# US 2021/0332262 A1 · Gloves with hydrophilic coating and method of manufacturing therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332262 A1
- Document ID: US20210332262A1
- Status: Published application
- Kind: A1
- Application number: 17/229,785
- Filed: 2021-04-13
- Published: 2021-10-28
- Earliest claimed: 2020-04-22
- Assignees: Top Glove International Sdn. Bhd.
- Applicants: Top Glove International Sdn. Bhd.
- Inventors: CHONG BAN WONG; SIEW SZEN LING; MENG LAI LOW; SITI HAJAR MAT ZANI
- Web page: https://patentgrep.com/patent/US20210332262A1

## CPC

- C09D 5/024: {characterised by the additives}
- C09D 183/04: Polysiloxanes
- A41D 19/0082: {Details}
- B29C 41/14: Dipping a core {(B29C41/10 takes precedence)}
- B29C 41/22: Making multilayered or multicoloured articles
- C08J 5/02: Direct processing of dispersions, e.g. latex, to articles
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08J 7/056: Forming hydrophilic coatings
- C08K 5/101: of monocarboxylic acids
- C08K 5/3432: Six-membered rings
- C08K 5/41: Compounds containing sulfur bound to oxygen
- C09D 7/40: Additives
- C09D 7/63: organic
- C09D 7/65: macromolecular (C09D7/41-C09D7/48 take precedence)
- C09D 191/06: Waxes
- B29K 2007/00: Use of natural rubber as moulding material
- B29K 2021/00: Use of unspecified rubbers as moulding material
- B29K 2105/0064: {Latex, emulsion or dispersion}
- B29K 2995/0092: hydrophilic
- B29L 2031/4864: {Gloves}
- C08J 2307/02: Latex
- C08J 2321/02: Latex
- C08J 2483/04: Polysiloxanes
- C08K 5/098: Metal salts of carboxylic acids
- C08K 5/19: Quaternary ammonium compounds
- C08K 5/42: Sulfonic acids; Derivatives thereof
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A hydrophilic coating includes silicone emulsion, wax dispersion, stearate based chemical, surfactant and water. Further, the present invention discloses a method of preparing a glove with hydrophilic coating using either chlorinated or polymer coated method, wherein the glove is any one from the group consisting of acrylonitrile butadiene rubber, natural rubber, polyisoprene rubber, polychloroprene rubber, styrene butadiene rubber, butadiene copolymers rubber, polyurethanes rubber, rubber of vinyl containing substances, thermoplastic elastomer, vinyl acetate ethylene rubber and mixtures thereof.

## Claims

### Claim 1

A hydrophilic coating includes silicone emulsion, wax dispersion, stearate based chemical, surfactant and water, wherein the silicone emulsion is used at weight concentration ranging between 0.01% to 1.0% in the hydrophilic coating, wherein the wax dispersion is used at weight concentration ranging between 0.01% to 1.0% in the hydrophilic coating, wherein the stearate based chemical is used at weight concentration ranging between 0.01% to 1.0% in the hydrophilic coating, wherein the surfactant is used at weight concentration ranging between 0.4% to 2.0% in the hydrophilic coating and wherein remaining of the hydrophilic coating is filled by the water to a weight concentration of 100%.

### Claim 2 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the silicone emulsion is used at weight concentration ranging between 0.05% to 0.5% in the hydrophilic coating.

### Claim 3 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the wax dispersion is used at weight concentration ranging between 0.05% to 0.5% in the hydrophilic coating.

### Claim 4 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the stearate based chemical is used at weight concentration ranging between 0.1% to 0.5% in the hydrophilic coating.

### Claim 5 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the surfactant is used at weight concentration ranging between 0.5% to 1.0% in the hydrophilic coating.

### Claim 6 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the silicone emulsion is any one selected from the group consisting of polydimethylsiloxane silicone emulsion, amino type silicone, organo functional silicone emulsion, resin type silicone emulsion, film forming silicone and mixtures thereof.

### Claim 7 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the wax dispersion is any one selected from the group consisting of high density polyethylene wax, low density polyethylene wax, polypropylene wax, paraffin wax, carnauba wax, polytetrafluoroethylene wax and mixtures thereof.

### Claim 8 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the stearate based chemical is any one selected from the group consisting of potassium stearate, calcium stearate, magnesium stearate, zinc stearate and mixtures thereof.

### Claim 9 (depends on 1)

The hydrophilic coating as claimed in claim 1 wherein the surfactant is any one selected from the group consisting of any anionic surfactant, any cationic surfactant and mixtures thereof, wherein the anionic surfactant is sodium lauryl ether sulphate and wherein the cationic surfactant is cetylpyridinium chloride.

### Claim 10 (depends on 1)

A method to prepare a glove with hydrophilic coating as claimed in claim 1 wherein the method comprises the steps of:
i. cleaning and/or washing formers to produce cleaned formers;
ii. dipping the cleaned formers obtained in step (i) into a coagulant solution to coat a coagulant layer on the former;
iii. drying the coagulant layer coated on the former obtained in step (ii) at a temperature between 80° C. to 200° C. for a time period ranging from 1 minute to 10 minutes;
iv. dipping the former obtained in step (iii) into first latex formulation to produce a first latex layer;
v. drying the first latex layer coated on the former obtained in step (iv) at a temperature between 80° C. to 150° C. for a time period ranging from 20 seconds to 5 minutes;
vi. dipping the former obtained in step (v) into second latex formulation to produce a second latex layer;
vii. drying the second latex layer coated on the former obtained in step (vi) at a temperature between 80° C. to 200° C. for a time period ranging from 20 seconds to 5 minutes;
viii. treating the second latex layer coated on the former obtained in step (vii) with hot water at a temperature between 40° C. to 80° C. for a time period ranging from 20 seconds to 5 minutes to leach out chemical residues to form pre-leached latex film;
ix. beading the pre-leached latex film coated on the former obtained in step (viii) to produce beaded latex film;
x. curing the beaded latex film coated on the former obtained in step (ix) at a temperature between 90° C. to 150° C. for a time period ranging from 5 minutes to 45 minutes and thereafter cooled to produce cooled latex film, wherein the step of cooling is carried out by way of dipping the cured latex film coated on the former into cold water having a temperature ranging between 20° C. to 40° C. for a time period ranging between 20 seconds to 5 minutes;
xi. treating the cooled latex film coated on the former obtained in step (x) with chlorine water to obtain treated latex film;
xii. treating the treated latex film coated on the former obtained in step (xi) with hot water at a temperature between 40° C. to 80° C. for a time period ranging from 20 seconds to 5 minutes to leach out chemical residues to obtain post-leached latex film;
xiii. spraying hydrophilic solution onto the post-leached latex film coated on the former obtained in step (xii) or dipping the post-leached latex film coated on the former obtained in step (xii) into hydrophilic solution to obtain latex film with hydrophilic coating;
xiv. drying the latex film with hydrophilic coating coated on the former obtained in step (xiii) at a temperature between 80° C. to 200° C. for a time period ranging from 20 seconds to 5 minutes to produce glove with hydrophilic coating; and
xv. stripping the glove with hydrophilic coating coated on the former obtained in step (xiv) from the former; and
wherein the first and the second latex formulations are selected from the group consisting of acrylonitrile butadiene rubber, natural rubber, polyisoprene rubber, polychloroprene rubber, styrene butadiene rubber, butadiene copolymers rubber, polyurethanes rubber, rubber of vinyl containing substances, thermoplastic rubber, vinyl acetate ethylene rubber and mixtures thereof and wherein the first and the second latex formulations are identical latex formulation.

### Claim 11 (depends on 1)

A method to prepare a glove with hydrophilic coating as claimed in claim 1 wherein the method comprises the steps of:
i. cleaning and/or washing formers to produce cleaned formers;
ii. dipping the cleaned formers obtained in step (i) into a coagulant solution to coat a coagulant layer on the former;
iii. drying the coagulant layer coated on the former obtained in step (ii) at a temperature between 80° C. to 200° C. for a time period ranging from 1 minute to 10 minutes;
iv. dipping the former obtained in step (iii) into first latex formulation to produce a first latex layer;
v. drying the first latex layer coated on the former obtained in step (iv) at a temperature between 80° C. to 150° C. for a time period ranging from 20 seconds to 5 minutes;
vi. dipping the former obtained in step (v) into second latex formulation to produce a second latex layer;
vii. drying the second latex layer coated on the former obtained in step (vi) at a temperature between 80° C. to 200° C. for a time period ranging from 20 seconds to 5 minutes;
viii. treating the second latex layer coated on the former obtained in step (vii) with hot water at a temperature between 40° C. to 80° C. for a time period ranging from 20 seconds to 5 minutes to leach out chemical residues to form pre-leached latex film;
ix. treating the pre-leached latex film coated on the former obtained in step (viii) with polymer solution to produce polymer coated latex film, wherein the polymer coating is carried out by way of dipping the pre-leached latex film coated on the former into the polymer solution having a concentration ranging between 1.5% to 5.0%;
x. beading the polymer coated latex film coated on the former obtained in step (ix) to produce beaded latex film;
xi. curing the beaded latex film coated on the former obtained in step (x) at a temperature between 90° C. to 150° C. for a time period ranging from 5 minutes to 45 minutes to cured latex film;
xii. treating the cured latex film coated on the former obtained in step (xi) with hot water at a temperature between 40° C. to 80° C. for a time period ranging from 20 seconds to 5 minutes to leach out chemical residues to obtain post-leached latex film;
xiii. spraying hydrophilic solution onto the post-leached latex film coated on the former obtained in step (xii) or dipping the post-leached latex film coated on the former obtained in step (xii) into hydrophilic solution to obtain latex film with hydrophilic coating;
xiv. drying the latex film with hydrophilic coating coated on the former obtained in step (xiii) at a temperature between 80° C. to 200° C. for a time period ranging from 20 seconds to 5 minutes to produce glove with hydrophilic coating; and
xv. stripping the glove with hydrophilic coating coated on the former obtained in step (xiv) from the former; and
wherein the first and the second latex formulations are selected from the group consisting of acrylonitrile butadiene rubber, natural rubber, polyisoprene rubber, polychloroprene rubber, styrene butadiene rubber, butadiene copolymers rubber, polyurethanes rubber, rubber of vinyl containing substances, thermoplastic rubber, vinyl acetate ethylene rubber and mixtures thereof and wherein the first and the second latex formulations are identical latex formulation.

### Claim 12 (depends on 10)

The method to prepare a glove as claimed in claim 10 wherein the step of spraying is carried out by way of spraying the hydrophilic solution onto the post-leached latex film coated on the former at a temperature ranging between 30° C. to 70° C. for a duration ranging between 6 seconds to 25 seconds while the post-leached latex film coated on the former is continuously rotated during and after the spraying step to ensure even coating for a duration ranging between 5 seconds to 60 seconds to yield the latex film with hydrophilic coating.

### Claim 13 (depends on 11)

The method to prepare a glove as claimed in claim 11 wherein the step of spraying is carried out by way of spraying the hydrophilic solution onto the post-leached latex film coated on the former at a temperature ranging between 30° C. to 70° C. for a duration ranging between 6 seconds to 25 seconds while the post-leached latex film coated on the former is continuously rotated during and after the spraying step to ensure even coating for a duration ranging between 5 seconds to 60 seconds to yield the latex film with hydrophilic coating.

### Claim 14 (depends on 12)

The method to prepare a glove as claimed in claim 12 wherein the spraying is carried out at a speed between 1 litre per minute to 5 litres per minute at a pressure between 0.1 bar to 3.0 bar under a temperature ranging between 30° C. to 50° C.

### Claim 15 (depends on 13)

The method to prepare a glove as claimed in claim 13 wherein the spraying is carried out at a speed between 1 litre per minute to 5 litres per minute at a pressure between 0.1 bar to 3.0 bar under a temperature ranging between 30° C. to 50° C.

### Claim 16 (depends on 10)

The method to prepare a glove as claimed in claim 10 wherein the the step of coating is carried out by way of dipping the post-leached latex film coated on the former in a container containing the hydrophilic solution at a temperature ranging between 30° C. to 70° C. for a duration ranging between 6 seconds to 25 seconds to yield the latex film with hydrophilic coating.

### Claim 17 (depends on 11)

The method to prepare a glove as claimed in claim 11 wherein the the step of coating is carried out by way of dipping the post-leached latex film coated on the former in a container containing the hydrophilic solution at a temperature ranging between 30° C. to 70° C. for a duration ranging between 6 seconds to 25 seconds to yield the latex film with hydrophilic coating.

### Claim 18 (depends on 12)

The method to prepare a glove as claimed in claim 12 wherein the hydrophilic solution is used at a weight concentration ranging between 0.1% to 5.0%.

### Claim 19 (depends on 13)

The method to prepare a glove as claimed in claim 13 wherein the hydrophilic solution is used at a weight concentration ranging between 0.1% to 5.0%.

### Claim 20 (depends on 1)

A glove with hydrophilic coating, wherein the hydrophilic coating is as claimed in claim 1 and wherein the glove is any one from the group consisting of acrylonitrile butadiene rubber, natural rubber, polyisoprene rubber, polychloroprene rubber, styrene butadiene rubber, butadiene copolymers rubber, polyurethanes rubber, rubber of vinyl containing substances, thermoplastic elastomer, vinyl acetate ethylene rubber and mixtures thereof.

### Claim 21 (depends on 10)

A glove with hydrophilic coating, wherein the glove is prepared as claimed in claim 10 and wherein the glove is any one from the group consisting of acrylonitrile butadiene rubber, natural rubber, polyisoprene rubber, polychloroprene rubber, styrene butadiene rubber, butadiene copolymers rubber, polyurethanes rubber, rubber of vinyl containing substances, thermoplastic elastomer, vinyl acetate ethylene rubber and mixtures thereof.

### Claim 22 (depends on 11)

A glove with hydrophilic coating, wherein the glove is prepared as claimed in claim 11 and wherein the glove is any one from the group consisting of acrylonitrile butadiene rubber, natural rubber, polyisoprene rubber, polychloroprene rubber, styrene butadiene rubber, butadiene copolymers rubber, polyurethanes rubber, rubber of vinyl containing substances, thermoplastic elastomer, vinyl acetate ethylene rubber and mixtures thereof.