# US 2021/0332261 A1 · Increased deposition efficiency via dual reactor system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332261 A1
- Document ID: US20210332261A1
- Status: Published application
- Kind: A1
- Application number: 17/239,516
- Filed: 2021-04-23
- Published: 2021-10-28
- Earliest claimed: 2020-04-23
- Applicants: HZO, Inc.
- Inventors: Robert Eugene Askin, III; Sean Clancy
- Web page: https://patentgrep.com/patent/US20210332261A1

## CPC

- C08G 61/025: {Polyxylylenes}
- C09D 165/02: Polyphenylenes
- B05D 1/08: Flame spraying
- C08G 2261/3424: non-conjugated, e.g. paracyclophanes or xylenes
- C09D 165/04: Polyxylylenes
- C23C 14/12: Organic material
- C23C 16/4488: {by in situ generation of reactive gas by chemical or electrochemical reaction}
- C23C 16/45512: {Premixing before introduction in the reaction chamber}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for depositing Parylene onto a substrate includes operating a first pyrolysis chamber at a first set of parameters to cause cracking of dimers into monomers at the first set of parameters and operating a second pyrolysis chamber at a second set of parameters to cause cracking of dimers into monomers at the second set of parameters. The method includes mixing the monomers at the first set of parameters with monomers at the second set of parameters together and polymerizing the mixture as a protective coating.

## Claims

### Claim 1

A method for depositing Parylene onto a substrate, comprising:
operating a first pyrolysis chamber at a first set of parameters to cause cracking of dimers into monomers at the first set of parameters;
operating a second pyrolysis chamber at a second set of parameters to cause cracking of dimers into monomers at the second set of parameters;
mixing the monomers at the first set of parameters with monomers at the second set of parameters together; and
polymerizing the mixture as a protective coating.

### Claim 2 (depends on 1)

The method of claim 1, further comprising mixing the monomers at the first set of parameters with monomers at the second set of parameters before entering a deposition chamber.

### Claim 3 (depends on 1)

The method of claim 1, further comprising mixing the monomers at the first set of parameters with monomers at the second set of parameters after entering a deposition chamber.

### Claim 4 (depends on 1)

The method of claim 1, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene.

### Claim 5 (depends on 1)

The method of claim 1, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene, wherein the first Parylene and the second Parylene are different Parylenes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene, wherein the first Parylene and the second Parylene are a same Parylene.

### Claim 7 (depends on 1)

The method of claim 1, wherein the parameters may be any one of temperature, pressure, residence time, concentration of dimer, amount of dimer, type of dimer, flow rate, or type of material, or a combination thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first set of parameters includes a longer residence time than the second set of parameters.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first set of parameters includes a higher pressure than the second set of parameters.

### Claim 10

A method for depositing Parylene onto a substrate, comprising:
operating a first pyrolysis chamber at a first set of parameters to cause cracking of dimers into monomers at the first set of parameters;
operating a second pyrolysis chamber at a second set of parameters to cause cracking of dimers into monomers at the second set of parameters;
mixing the monomers at the first set of parameters with monomers at the second set of parameters together before entering a deposition chamber; and
polymerizing the mixture as a protective coating in the deposition chamber.

### Claim 11 (depends on 10)

The method of claim 10, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene.

### Claim 12 (depends on 10)

The method of claim 10, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene, wherein the first Parylene and the second Parylene are different Parylenes.

### Claim 13 (depends on 10)

The method of claim 10, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene, wherein the first Parylene and the second Parylene are a same Parylene.

### Claim 14 (depends on 10)

The method of claim 10, wherein the parameters may be any one of temperature, pressure, residence time, concentration of dimer, amount of dimer, type of dimer, flow rate, or type of material, or a combination thereof.

### Claim 15

A method for depositing Parylene onto a substrate, comprising:
operating a first pyrolysis chamber at a first set of parameters to cause cracking of dimers into monomers at the first set of parameters;
operating a second pyrolysis chamber at a second set of parameters to cause cracking of dimers into monomers at the second set of parameters;
mixing the monomers at the first set of parameters with monomers at the second set of parameters together after entering a deposition chamber; and
polymerizing the mixture as a protective coating in the deposition chamber.

### Claim 16 (depends on 15)

The method of claim 15, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene.

### Claim 17 (depends on 15)

The method of claim 15, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene, wherein the first Parylene and the second Parylene are different Parylenes.

### Claim 18 (depends on 15)

The method of claim 15, wherein the monomers at the first set of parameters are a precursor to a first Parylene and wherein the monomers at the second set of parameters are a precursor to a second Parylene, wherein the first Parylene and the second Parylene are a same Parylene.

### Claim 19 (depends on 15)

The method of claim 15, wherein the parameters may be any one of temperature, pressure, residence time, concentration of dimer, amount of dimer, type of dimer, flow rate, or type of material, or a combination thereof.

### Claim 20 (depends on 15)

The method of claim 15, wherein the first set of parameters includes a longer residence time than the second set of parameters.