# US 2021/0332237 A1 · Polycarbonate resin composition, method for producing the same, masterbatch pellet, and molded body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332237 A1
- Document ID: US20210332237A1
- Status: Published application
- Kind: A1
- Application number: 17/414,195
- Filed: 2019-12-25
- Published: 2021-10-28
- Earliest claimed: 2018-12-27
- Assignees: Ube Material Industries, Ltd.; National University Corporation Yamagata University
- Applicants: Ube Material Industries, Ltd.; National University Corporation Yamagata University
- Inventors: Tetsuo Takayama; Yuzo Kato; Toru Inagaki
- Web page: https://patentgrep.com/patent/US20210332237A1

## CPC

- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08K 5/098: Metal salts of carboxylic acids
- C08K 7/00: Use of ingredients characterised by shape
- C08L 23/12: Polypropene
- C08J 3/226: {using a polymer as a carrier}
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08J 2423/12: Polypropene
- C08J 2453/02: of vinyl aromatic monomers and conjugated dienes
- C08K 2003/3063: {Magnesium sulfate}
- C08L 2205/03: containing three or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The polycarbonate resin composition according to the present invention includes: 50 to 90% by mass of polycarbonate resin (A); 2.0 to 20% by mass of olefin polymer (B); 5 to 40% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2); 0.1 to 8% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid; and 1 to 20% by mass of elastomer (E).

## Claims

### Claim 1

A polycarbonate resin composition, comprising: 50 to 90% by mass of polycarbonate resin (A): 2.0 to 20% by mass of olefin polymer (B); 5 to 40% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2); 0.1 to 8% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid:
and 1 to 20% by mass of elastomer (E).

### Claim 2 (depends on 1)

The polycarbonate resin composition according to claim 1, haying a sea-island structure consisting of a sea phase including the polycarbonate resin and an island phase having the elastomer on an outer circumference.

### Claim 3 (depends on 1)

A method for producing the polycarbonate resin composition according to claim 1, comprising:
a first step of melt-kneading 2 to 50% by mass of olefin polymer (B), 40 to 70% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), 0.1 to 5% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid, and 1 to 50% by mass of elastomer (E) to obtain masterbatch pellets; and
a second step of melt-kneading 10 to 60% by mass of the masterbatch pellets and 40 to 90% by mass of polycarbonate resin (A) to produce a polycarbonate resin composition.

### Claim 4 (depends on 1)

A method for producing the polycarbonate resin composition according to claim 1, comprising:
a first step of melt-kneading 28 to 50% by mass of olefin polymer (B), 40 to 70% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), and 0.1 to 5% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid to obtain masterbatch pellets, and
a second step of melt-kneading 10 to 59% by mass of the masterbatch pellets, 40 to 89% by mass of polycarbonate resin (A), and 1 to 20% by mass of elastomer (E) to produce a polycarbonate resin composition.

### Claim 5 (depends on 1)

A method for producing the polycarbonate resin composition according to claim 1, the method comprising melt-kneading 50 to 90% by mass of polycarbonate resin (A), 2.0 to 20% by mass of olefin polymer (B), 5 to 40% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), 0.1 to 8% by mass of at least one (D) selected from a fatty acid metal salt and a fatly acid, and 1 to 20% by mass of elastomer (E).

### Claim 6 (depends on 1)

A method for producing the polycarbonate resin composition according to claim 1, the method comprising:
melt-kneading 2.0 to 20% by mass of olefin polymer (B), 5 to 40% by mass of basic magnesium sulfite (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), 0.1 to 8% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid, and 1 to 20% by mass of elastomer (E); and then
adding and melt-kneading 50 to 90% by mass of polycarbonate resin (A).

### Claim 7

Masterbatch pellets for producing a polycarbonate resin composition by kneading with a diluent including polycarbonate resin (A), the masterbatch pellets comprising
2 to 50% by mass of olefin polymer (B), 40 to 70% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfite (C-1) and fan-shaped basic magnesium sulfate (C-2), 0.1 to 5% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid, and I to 50% by mass of elastomer (E).

### Claim 8 (depends on 1)

A molded body, being a molded product of the polycarbonate resin composition according to claim 1.

### Claim 9 (depends on 2)

A method for producing the polycarbonate resin composition according to claim 2, comprising:
a first step of melt-kneading 2 to 50% by mass of olefin polymer (B), 40 to 70% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfite (C-2), 0.1 to 5% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid, and 1 to 50% by mass of elastomer (E) to obtain masterbatch pellets; and
a second step of melt-kneading 10 to 60% by mass of the masterbatch pellets and 40 to 90% by mass of polycarbonate resin (A) to produce a polycarbonate resin composition.

### Claim 10 (depends on 2)

A method for producing the polycarbonate resin composition according to claim 2, comprising:
a first step of melt-kneading 28 to 50% by mass of olefin polymer (B), 40 to 70% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), and 0.1 to 5% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid to obtain masterbatch pellets; and
a second step of melt-kneading 10 to 59% by mass of the masterbatch pellets, 40 to 89% by mass of polycarbonate resin (A), and 1 to 20% by mass of elastomer (E) to produce a polycarbonate resin composition.

### Claim 11 (depends on 2)

A method for producing the polycarbonate resin composition according to claim 2, the method comprising melt-kneading 50 to 90% by mass of polycarbonate resin (A), 2.0 to 20% by mass of olefin polymer (B), 5 to 40% by mass of basic magnesium sulfate (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), 0.1 to 8% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid, and 1 to 20% by mass of elastomer (E).

### Claim 12 (depends on 2)

A method for producing the polycarbonate resin composition according to claim 2, the method comprising:
melt-kneading 2.0 to 20% by mass of olefin polymer (B), 5 to 40% by mass of basic magnesium sulfite (C) selected from fibrous basic magnesium sulfate (C-1) and fan-shaped basic magnesium sulfate (C-2), 0.1 to 8% by mass of at least one (D) selected from a fatty acid metal salt and a fatty acid, and 1 to 20% by mass of elastomer (E); and then
adding and melt-kneading 50 to 90% by mass of polycarbonate resin (A).