# US 2021/0332232 A1 · Sintered powder (sp) containing a partially crystalline terephthalate polyester, an amorphous terephthalate polyester and a phosphinic acid salt

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332232 A1
- Document ID: US20210332232A1
- Status: Published application
- Kind: A1
- Application number: 17/272,331
- Filed: 2019-08-21
- Published: 2021-10-28
- Earliest claimed: 2018-08-30
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Claus GABRIEL; Angelika ZEPP; Thomas MEIER; Natalie Beatrice Janine HERLE
- Web page: https://patentgrep.com/patent/US20210332232A1

## CPC

- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- B29C 64/153: using layers of powder being selectively joined, e.g. by selective laser sintering or melting
- B29C 64/314: Preparation
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/10: Pre-treatment
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B29K 2067/006: {PBT, i.e. polybutylene terephthalate}
- C08L 2203/30: used for thermoforming
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention relates to a sinter powder (SP) comprising at least one semicrystalline terephthalate polyester (A), at least one amorphous terephthalate polyester (B) and at least one phosphinic salt (C). The present invention further relates to a method of producing a shaped body by sintering the sinter powder (SP) or by an FFF (fused filament fabrication) method, to a shaped body obtainable by the method of the invention, and to the use of a phosphinic salt in a sinter powder (SP) for broadening the sintering window (WSP) of the sinter powder (SP).

## Claims

### Claim 1

A sinter powder (SP) comprising the following components:
(A) at least one semicrystalline terephthalate polyester,
(B) at least one amorphous terephthalate polyester,
(C) at least one phosphinic salt of the general formula (I)
in which R1 and R2 are independently hydrogen or C1-C8-alkyl;
M is (C1-C4-alkyl)4N, (C1-C4-alkyl)3NH, (C2-C4-alkylOH)4N, (C2-C4alkylOH)3NH, (C2-C4-alkylOH)2N(CH3)2, (C2-C4-alkylOH)2NHCH3, (C6H5)4N, (C6H5)NH, (C6H4CH3)4N, (C6H4CH3)3NH, NH4, an alkali metal ion, an alkaline earth metal ion, an aluminum ion, a zinc ion, an iron ion or a boron ion;
m is 1, 2 or 3 and indicates the number of positive charges of M; and
n is 1, 2 or 3 and indicates the number of phosphinic anions, wherein
the amorphous terephthalate polyester (B) comprises not more than 2.5% by weight of crystalline terephthalate polyester, based on the total weight of the amorphous terephthalate polyester (B).

### Claim 2 (depends on 1)

The sinter powder (SP) according to claim 1, which comprises in the range from 50% to 90% by weight of component (A), in the range from 5% to 25% by weight of component (B) and in the range from 5% to 25% by weight of component (C), based in each case on the sum total of the percentages by weight of (A), (B) and (C).

### Claim 3 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the at least one semicrystalline terephthalate polyester (component A) is selected from the group consisting of polyethylene terephthalate (PET) and polybutylene terephthalate (PBT).

### Claim 4 (depends on 1)

The sinter powder (SP) according to claim 1, wherein component (C) is a phosphinic salt of the formula (I′)

### Claim 5 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the at least one amorphous terephthalate polyester (component B) is an amorphous polyethylene terephthalate ester.

### Claim 6 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the sinter powder has a median particle size (D50) in the range from 10 to 250 μm.

### Claim 7 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the sinter powder (SP) has
a D10 in the range from 10 to 60
a D50 in the range from 25 to 90 μm and
a D90 in the range from 50 to 150 μm.

### Claim 8 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the sinter powder (SP) has a melting temperature (TM) in the range from 150 to 260° C.

### Claim 9 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the sinter powder (SP) has a crystallization temperature (TC) in the range from 110 to 210° C.

### Claim 10 (depends on 1)

The sinter powder (SP) according to claim 1, wherein the sinter powder (SP) has a sintering window (WSP), where the sintering window (WSP) is the difference between the onset temperature of melting (TMonset) and the onset temperature of crystallization (TConset) and where the sintering window (WSP) is in the range from 10 to 40 K.

### Claim 11

A process for producing a sinter powder (SP), comprising the steps of
a) mixing the following components:
(A) at least one semicrystalline terephthalate polyester,
(B) at least one amorphous terephthalate polyester,
(C) at least one phosphinic salt of the general formula (I)
in which R1 and R2 are independently hydrogen or C1-C8-alkyl;
M is (C1-C4-alkyl)4N, (C1-C4-alkyl)3NH, (C2-C4-alkylOH)4N, (C2-C4alkylOH)3NH, (C2-C4-alkylOH)2N(CH3)2, (C2-C4-alkylOH)2NHCH3, (C6H5)4N, (C6H5)NH, (C6H4CH3)4N, (C6H4CH3)3NH, NH4, an alkali metal ion, an alkaline earth metal ion, an aluminum ion, a zinc ion, an iron ion or a boron ion;
m is 1, 2 or 3 and indicates the number of positive charges of M; and
n is 1, 2 or 3 and indicates the number of phosphinic anions; and
b) grinding the mixture obtained in step a) to obtain the sinter powder (SP).

### Claim 12 (depends on 1)

A method of producing a shaped body, comprising the steps of:
i) providing a layer of a sinter powder (SP) according to claim 1,
ii) exposing the layer of the sinter powder (SP) provided in step i).

### Claim 13 (depends on 1)

The use of a sinter powder (SP) according to claim 1 in a sintering method or in a fused filament fabrication method.

### Claim 14 (depends on 12)

A shaped body obtainable by a method according to claim 12.

### Claim 15

The use of a phosphinic salt of the general formula (I)
in which R1 and R2 are independently hydrogen or C1-C8-alkyl;
M is (C1-C4-alkyl)4N, (C1-C4-alkyl)3NH, (C2-C4-alkylOH)4N, (C2-C4alkylOH)3NH, (C2-C4-alkylOH)2N(CH3)2, (C2-C4-alkylOH)2NHCH3, (C6H5)4N, (C6H5)NH, (C6H4CH3)4N, (C6H4CH3)3NH, NH4, an alkali metal ion, an alkaline earth metal ion, an aluminum ion, a zinc ion, an iron ion or a boron ion;
m is 1, 2 or 3 and indicates the number of positive charges of M; and
n is 1, 2 or 3 and indicates the number of phosphinic anions,
for broadening the sintering window (WSP) of a sinter powder (SP).