# US 2021/0332222 A1 · Application of lignin in preparing radial tire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332222 A1
- Document ID: US20210332222A1
- Status: Published application
- Kind: A1
- Application number: 17/305,327
- Filed: 2021-07-05
- Published: 2021-10-28
- Earliest claimed: 2020-07-08
- Assignees: Nanjing Tech University
- Applicants: Nanjing Tech University
- Inventors: Chenjie ZHU; Hanjie YING; Ming LI; Pingkai OUYANG; Jiannong SHEN; Xinjian XU; Wei ZHUANG; Tao SHEN
- Web page: https://patentgrep.com/patent/US20210332222A1

## CPC

- B60C 1/0016: {Compositions of the tread}
- C08L 7/00: Compositions of natural rubber
- B60C 1/00: Tyres characterised by the chemical composition or the physical arrangement or mixture of the composition
- B60C 1/0041: {Compositions of the carcass layers}
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The invention belongs to the field of rubber tire processing, and particularly discloses an application of a lignin in preparing a radial tire, wherein the lignin is capable of completely or partially replacing resorcinol, and meanwhile, the lignin is also capable of completely or partially replacing an anti-aging agent. Compared with the prior art, the resorcinol is replaced or partially replaced by a biomass-derived lignin or a modified lignin in the invention, so that requirements of cost reduction, environmental protection and no toxicity are satisfied. Especially, the lignin modified by demethylation according to the invention is capable of effectively enhancing various properties of rubber.

## Claims

### Claim 1

A method for preparing a radial tire with a lignin comprising a step of mixing the lignin in the radial tire.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the lignin completely or partially replaces a resorcinol in preparing the radial tire.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the lignin completely or partially replaces an anti-aging agent in preparing the radial tire.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the lignin completely or partially replaces an anti-aging agent in preparing the radial tire.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in parts by weight, an amount of the lignin is 2 parts to 25 parts per 100 parts of rubber; wherein a particle size d50 of the lignin is 1 μm to 10 μm.

### Claim 6 (depends on 2)

The method according to claim 2, wherein in parts by weight, an amount of the resorcinol is 0 part to 0.5 part per 100 parts of rubber.

### Claim 7 (depends on 3)

The method according to claim 3, wherein in parts by weight, an amount of the anti-aging agent is 0 part to 1 part per 100 parts of rubber.

### Claim 8 (depends on 4)

The method according to claim 4, wherein in parts by weight, an amount of the anti-aging agent is 0 part to 1 part per 100 parts of rubber.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the lignin is one or more selected from the group consisting of an alkali lignin, a soda lignin, an organic solvent lignin and an enzymolysis lignin.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the lignin is a modified lignin prepared by modifying any one of an alkali lignin, a soda lignin, an organic solvent lignin and an enzymolysis lignin; wherein the modifying is any one or a combination of several of acylation, esterification, etherification, phenolization, alkylation, demethylation, amination, vulcanization and unsaturated functionalization.

### Claim 11 (depends on 6)

The method according to claim 6, wherein the radial tire further comprises the following ingredients: a filler, a zinc oxide, an adhesion accelerator, a vulcanizing agent, an adhesive and a vulcanizing accelerator.

### Claim 12 (depends on 11)

The method according to claim 11, wherein based on 100 parts of rubber, weight parts of the ingredients are as follows:
45 parts to 65 parts of the filler;
6 part to 10 parts of the zinc oxide;
0.2 part to 1 part of the adhesion accelerator;
3 parts to 6 parts of the vulcanizing agent;
4 parts to 8 parts of the adhesive; and
1 part to 3 parts of the vulcanizing accelerator.