# US 2021/0332210 A1 · Method for preparing polymer mould-free stereostructure foamed product from supercritical fluid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332210 A1
- Document ID: US20210332210A1
- Status: Published application
- Kind: A1
- Application number: 16/609,739
- Filed: 2018-10-23
- Published: 2021-10-28
- Earliest claimed: 2018-09-06
- Assignees: Guangdong Speed New Material Technology Co., Ltd
- Applicants: Guangdong Speed New Material Technology Co., Ltd
- Inventors: Yunping FENG
- Web page: https://patentgrep.com/patent/US20210332210A1

## CPC

- C08J 9/122: {Hydrogen, oxygen, CO2, nitrogen or noble gases}
- B29B 11/12: Compression moulding
- B29C 44/022: {Foaming unrestricted by cavity walls, e.g. without using moulds or using only internal cores}
- B29C 44/3453: {Feeding the blowing agent to solid plastic material}
- B29C 44/348: {by regulating the temperature and/or the pressure, e.g. suppression of foaming until the pressure is rapidly decreased}
- B29C 44/60: Measuring, controlling or regulating
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2203/08: Supercritical fluid
- C08J 2323/02: not modified by chemical after treatment
- C08J 2323/08: Copolymers of ethene (C08J2323/16 takes precedence)
- C08J 2367/04: Polyesters derived from hydroxy carboxylic acids, e.g. lactones (C08J2367/06 takes precedence)
- C08J 2375/04: Polyurethanes
- C08J 2375/08: from polyethers
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid, containing a supercritical fluid delivery system, a stereoscopic foaming system and a preheating system, and has the following steps: performing pressure molding on a polymer material to obtain a foaming preform, then preheating the foaming preform in the preheating system, delivering the foaming preform to the stereoscopic foaming system after a temperature rises to a preheating temperature, introducing the supercritical fluid, and decompressing after the supercritical fluid is swelled and diffused to the polymer. The polymer is swelled using high-temperature medium-pressure supercritical fluid by utilizing a one-step method in a stereoscopic foaming tank and then subjected to free mould-free stereoscopic pressure-relief foam molding, so as to obtain a polymer microcellular foamed product with controllable product shape, size precision, pore fineness and product density.

## Claims

### Claim at position 1

1: A method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid, comprising a supercritical fluid delivery system, a stereoscopic foaming system and a preheating system, wherein the supercritical fluid delivery system is a supercritical CO2 or supercritical N2 delivery system, or a N2/CO2 mixed gas; the stereoscopic foaming system comprises a stereoscopic foaming tank, a temperature control device, a pressure control device and a pressure release device, and the supercritical fluid delivery system is connected with the stereoscopic foaming system; the preheating system comprises a preheating tank, a heating cycle device and a temperature control device;
swelling and impregnating the polymer using high-temperature medium-pressure supercritical fluid by utilizing a one-step method in a stereoscopic foaming tank and then directly subjected to free mould-free stereoscopic pressure-relief foam molding specifically comprises the following steps: performing pressure molding on a polymer material to obtain a foaming preform, then preheating the foaming preform in the preheating system, delivering the foaming preform to the stereoscopic foaming system after a temperature rises to a preheating temperature, closing and sealing the stereoscopic foaming tank, opening an intake valve, introducing the supercritical fluid to be regulated to be at a target temperature and pressure, swelling and diffusing the supercritical fluid toward the polymer for 30-120 min, and opening the pressure release device for pressure relief and foaming, so as to obtain a polymer microcellular foamed product with controllable product shape, size precision, pore fineness and product density.

### Claim at position 2 (depends on 1)

2: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 1, wherein the polymer is selected from but not limited to any one or a combination of polyethylene, polylactic acid, polypropylene, polystyrene, polymethyl methacrylate, polycarbonate, an acrylonitrile-butadiene-styrene copolymer, polyethylene terephthalate, polyamide, polyimide, polyphenylene sulfide, polyether sulfone, polyether ether ketone, rubber, silicone rubber, EPDM, an ethylene-vinyl acetate copolymer, thermoplastic polyurethane and a thermoplastic elastomer.

### Claim at position 3 (depends on 2)

3: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 2, wherein the polymer selects an amorphous polymer, the target temperature is 1.0-50° C. below the melting temperature of the polymer, and the pressure is 5-15 MPa.

### Claim at position 4 (depends on 2)

4: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 2, wherein the polymer selects a crystalline polymer, the target temperature is 1.0-50° C. below the melting temperature of the polymer, and the pressure is 5-15 MPa.

### Claim at position 5

5-8. (canceled)

### Claim at position 6 (depends on 3)

9: The method for preparing a polymer mould-ree stereostructure foamed product from supercritical fluid according to claim 3, wherein the pressure relief rate of the of the pressure release device of the stereoscopic foaming tank is 1-1000 MPa/s.

### Claim at position 7 (depends on 4)

10: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 4, wherein the pressure relief rate of the of the pressure release device of the stereoscopic foaming tank is 1-1000 MPa/s.

### Claim at position 8 (depends on 3)

11: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 3, wherein the supercritical CO2 delivery system comprises a CO2 liquid storage tank and a CO2 booster station, and the supercritical N2 delivery system comprises a N2 liquid storage tank and a N2 booster station.

### Claim at position 9 (depends on 4)

12: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 4, wherein the supercritical CO2 delivery system comprises a CO2 liquid storage tank and a CO2 booster station, and the supercritical N2 delivery system comprises a N2 liquid storage tank and a N2 booster station.

### Claim at position 10 (depends on 1)

13: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 1, wherein the supercritical CO2 delivery system is a N2/CO2 mixed gas in which the volume percentage of N2 is 50-99%.

### Claim at position 11 (depends on 3)

14: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 3, wherein the volume expansion ratio of the polymer microcellular foamed product has a volume expansion ratio of 2-60 folds, an average pore diameter of 0.1-100 μm and a pore density of 1.0×106-1.0×1015 pores/cm3.

### Claim at position 12 (depends on 4)

15: The method for preparing a polymer mould-free stereostructure foamed product from supercritical fluid according to claim 4, wherein the volume expansion ratio of the polymer microcellular foamed product has a volume expansion ratio of 2-60 folds, an average pore diameter of 0.1-100 μm and a pore density of 1.0×106-1.0×1015 pores/cm3.