# US 2021/0332187 A1 · Modified polyamide, method of preparing the same, and single component fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332187 A1
- Document ID: US20210332187A1
- Status: Published application
- Kind: A1
- Application number: 17/158,060
- Filed: 2021-01-26
- Published: 2021-10-28
- Earliest claimed: 2020-04-27
- Assignees: Taiwan Textile Research Institute
- Applicants: Taiwan Textile Research Institute
- Inventors: Po-Hsun HUANG; Wei-Hsiang LIN; Ta KO; Wei-Peng LIN
- Web page: https://patentgrep.com/patent/US20210332187A1

## CPC

- C08G 69/40: Polyamides containing oxygen in the form of ether groups (C08G69/12, C08G69/32 take precedence)
- C08G 69/36: derived from amino acids, polyamines and polycarboxylic acids
- D01F 6/80: from copolyamides
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

A modified polyamide is provided, which has a structure of formula (1), in which a+c is 3-8, b is 8-40, m is 3-11, n is 2-16, x is 100-220, and y is 1-6. A method of preparing a modified polyamide is also provided, which includes copolymerizing C4-C12 lactam, C4-C18 linear aliphatic dicarboxylic acid, polyetherdiamine, and diethylenetriamine (DETA), in which the lactam is 80 to 95 parts by weight, and the linear aliphatic dicarboxylic acid is 1 to 4 parts by weight, and the polyetherdiamine is 4 to 16 parts by weight, and the diethylenetriamine is 0.2 to 0.6 parts by weight.

## Claims

### Claim 1

A modified polyamide having a structure of formula (I), wherein a+c is 3-8, b is 8-40, m is 3-11, n is 2-16, x is 100-220, and y is 1-6.

### Claim 2 (depends on 1)

A single component fiber composed of the modified polyamide of claim 1.

### Claim 3

A method of preparing a modified polyamide, comprising:
copolymerizing C4-C12 lactam, C4-C18 linear aliphatic dicarboxylic acid, polyetherdiamine, and diethylenetriamine (DETA), wherein the lactam is 80 to 95 parts by weight, and the linear aliphatic dicarboxylic acid is 1 to 4 parts by weight, and the polyetherdiamine is 4 to 16 parts by weight, and the diethylenetriamine is 0.2 to 0.6 parts by weight.

### Claim 4 (depends on 3)

The method of claim 3, wherein the diethylenetriamine is 0.2 wt % to 0.6 wt % base on a total weight of the lactam, the linear aliphatic dicarboxylic acid, the polyetherdiamine, and the diethylenetriamine.

### Claim 5 (depends on 3)

The method of claim 3, wherein the polyetherdiamine is 4 wt % to 16 wt % based on a total weight of the lactam, the linear aliphatic dicarboxylic acid, the polyetherdiamine, and the diethylenetriamine.

### Claim 6 (depends on 3)

The method of claim 3, wherein the polyetherdiamine has a structure of formula (II):
wherein a+c is 3-8, and b is 8-40.

### Claim 7 (depends on 3)

The method of claim 3, wherein an average molecular weight of the polyetherdiamine is in a range of from 600 to 2,200.

### Claim 8 (depends on 3)

The method of claim 3, wherein copolymerizing the lactam, the linear aliphatic dicarboxylic acid, the polyetherdiamine, and the diethylenetriamine is performed at a temperature of 200° C. to 270° C. and an absolute pressure of 0.1 bar to 3 bar.

### Claim 9

A single component fiber comprising a modified polyamide formed by copolymerizing C4-C12 lactam, C4-C18 linear aliphatic dicarboxylic acid, polyetherdiamine, and diethylenetriamine.

### Claim 10 (depends on 9)

The single component fiber of claim 9, wherein the polyetherdiamine has a structure of formula (II):
wherein a+c is 3-8, and b is 8-40.