# US 2021/0332169 A1 · Polyolefin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0332169 A1
- Document ID: US20210332169A1
- Status: Published application
- Kind: A1
- Application number: 17/268,146
- Filed: 2019-12-20
- Published: 2021-10-28
- Earliest claimed: 2018-12-21
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Jeongkyu Lee; Sung Min Lee; Hyojoon Lee; Chang Hwan Jang; Sung Ho Park; Seul Ki Im; Jinyoung Lee; Sung Joon Oh; Seyoung Kim; Jisoo Song
- Web page: https://patentgrep.com/patent/US20210332169A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/65904: {in combination with another component of C08F4/64}
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65927: {two cyclopentadienyl rings being mutually bridged}
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08L 2201/10: Transparent films; Clear coatings; Transparent materials
- C08L 2314/06: Metallocene or single site catalysts
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention relates to polyolefin. More specifically, the present invention relates to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency, and such polyolefin has a density of 0.915 g/cm3 to 0.930 g/cm3 measured according to ASTM D1505; and satisfies the following requirements (provided that S1+S2+S3=1), when measuring the relative content of peak area according to melting temperature (Tm) using SSA (Successive Self-nucleation and Annealing) analysis: the content(S1) of peak area at Tm less than 100° C. is 0.33 to 0.35; the content(S2) of peak area at Tm of 100° C. or more and 120° C. or less is 0.52 to 0.56; and the content(S3) of peak area at Tm greater than 120° C. is 0.10 to 0.14.

## Claims

### Claim 1

A polyolefin having a density of 0.915 g/cm3 to 0.930 g/cm3 measured according to ASTM D1505; and
satisfying the following requirements 1) to 3), when
measuring a relative content of peak area according to melting temperature (Tm) using SSA (Successive Self-nucleation and Annealing) analysis:
1) a content(S1) of peak area at Tm less than 100° C. is 0.33 to 0.35;
2) a content(S2) of peak area at Tm of 100° C. or more and 120° C. or less is 0.52 to 0.56; and
3) the a content(S3) of peak area at Tm greater than 120° C. is 0.10 to 0.14,
provided that S1+S2+S3=1.

### Claim 2 (depends on 1)

The polyolefin according to claim 1, wherein the SSA is conducted by heating the polyolefin to a first heating temperature of 120 to 124° C. using differential scanning calorimetry, maintaining for 15 to 30 minutes, and then, cooling to 28 to 32° C., and while decreasing heating temperature by stages with (n+1)th heating temperature being 3 to 7° C. lower than nth heating temperature, repeating heating-annealing-quenching until a final heating temperature becomes 50 to 54° C. , and finally, increasing the temperature from 30° C. to 160° C. .

### Claim 3 (depends on 1)

The polyolefin according to claim 1, which has a melt index (MI216) measured under load of 2.16 kg at a temperature of 190° C. according to ASTM D1238 of 0.5 to 1.5 g/10 min.

### Claim 4 (depends on 1)

The polyolefin according to claim 1, which has a haze measured by a polyolefin film(BUR 2.3, film thickness 55 to 65 μm) prepared from the polyolefin using a film applicator, according to ISO 13468, of 12% or less.

### Claim 5 (depends on 1)

The polyolefin according to claim 1, which has a dart drop impact strength measured by a polyolefin film(BUR 2.3, film thickness 55 to 65 μm) prepared from the polyolefin using a film applicator, according to ASTM D 1709 [Method A], of 850 g or more.

### Claim 6 (depends on 1)

The polyolefin according to claim 1, wherein the polyolefin is copolymer of ethylene and alpha olefin.

### Claim 7 (depends on 7)

The polyolefin according to claim 7, wherein the alpha olefin includes one or more selected from the group consisting of propylene, 1-butene, 1-pentene, 4-methyl-1-pentene, 1-hexene, 1-heptene, 1-octene, 1-decene, 1-undecene, 1-dodecene, 1-tetradecene, 1-hexadecene, 1-eicosene, norbornene, norbornadiene, ethylidene norbordene, phenyl norbordene, vinyl norbordene, dicyclopentadiene, 1,4-butadiene, 1,5-pentadiene, 1,6-hexadiene, styrene, alpha-methyl styrene, divinylbenzene, and 3-chloromethyl styrene.

### Claim 8 (depends on 1)

The polyolefin according to claim 1, wherein the polyolefin is prepared by polymerizing olefin monomers, in the presence of a hybrid supported metallocene catalyst comprising one or more first metallocene compounds selected from a compound represented by the following Chemical Formula 1; one or more second metallocene compounds selected from a compounds represented by the following Chemical Formula 2; and a carrier supporting the first and second metallocene compounds:
in the Chemical Formula 1,
Q1 and Q2 are identical to or different from each other, and each independently, halogen, a C1-C20 alkyl group, a C2-C20 alkenyl group, a C2-C20 alkoxyalkyl group, a C6-C20 aryl group, a C7-C20 alkylaryl group, or a C7-C20 arylalkyl group;
T1 is carbon, silicon or germanium;
M1 is a Group 4 transition metal;
X1 and X2 are identical to or different from each other, and each independently, halogen, a C1-C20 alkyl group, a C2-C20 alkenyl group, a C6-C20 aryl group, a nitro group, an amido group, a C1-C20 alkylsilyl group, a C1-C20 alkoxy group, or a C1-C20 sulfonate group; and
R1 to R14 are identical to or different from each other, and each independently, hydrogen, halogen, a C1-C20 alkyl group, a C1-C20 haloalkyl group, a C2-C20 alkenyl group, a C1-C20 alkyl silyl group, a C1-C20 silylalkyl group, a C1-C20 alkoxysilyl group, a C1-C20 alkoxy group, a C6-C20 aryl group, a C7-C20 alkylaryl group, or a C7-C20 arylalkyl group, or two or more neighboring groups of R1 to R10 are connected with each other to form a substituted or unsubstituted aliphatic or aromatic ring;
in the Chemical Formula 2,
Q3 and Q4 are identical to or different from each other, and each independently, halogen, a C1-C20 alkyl group, a C2-C20 alkenyl group, a C2-C20 alkoxyalkyl group, a C6-C20 aryl group, a C7-C20 alkylaryl group, or a C7-C20 arylakyl group;
T2 is carbon, silicon or germanium;
M2 is a Group 4 transition metal;
X3 and X4 are identical to or different from each other, and each independently, halogen, a C1-C20 alkyl group, a C2-C20 alkenyl group, a C6-C20 aryl group, a nitro group, an amido group, a C1-C20 alkylsilyl group, a C1-C20 alkoxy group, or a C1-C20 sulfonate group; and
R15 to R28 are identical to or different from each other, and each independently, hydrogen, halogen, a C1-C20 alkyl group, a C1-C20 haloalkyl group, a C2-C20 alkenyl group, a C2-C20 alkoxyalkyl group, a C1-C20 alkylsilyl group, a C1-C20 silylalkyl group, a C1-C20 alkoxysilyl group, a C1-C20 alkoxy group, a C6-C20 aryl group, a C7-C20 alkylaryl group, or a C7-C20 arylalkyl group, provided that R20 and R24 are identical to or different from each other, and each independently, a C1 to C20 alkyl group, or two or more neighboring groups of R15 to R28 are connected with each other to form a substituted or unsubstituted aliphatic or aromatic ring.

### Claim 9 (depends on 8)

The polyolefin according to claim 8, wherein the compound
represented by the Chemical Formula 1 is one of compounds represented by the following Structural Formulas:

### Claim 10 (depends on 8)

The polyolefin according to claim 8, wherein the compound represented by the Chemical Formula 2 is one of compounds represented by the following Structural Formulas:

### Claim 11 (depends on 8)

The polyolefin according to claim 8, wherein a mole ratio of the first and second metallocene compounds is 1.2:1 to 7.5:1.

### Claim 12 (depends on 8)

The polyolefin according to claim 8, wherein in the Chemical Formula 1, R11 to R14 are each independently a C1 to C20 alkyl group, Ri is hydrogen or a C1 to C20 alkyl group, R2 to R10 are each hydrogen, Q1 and Q2 are each independently a C1 to C20 alkyl group or a C6 to C20 aryl group, X1 and X2 are each independently halogen, and M1 is Ti, Zr or Hf.

### Claim 13 (depends on 8)

The polyolefin according to claim 8, wherein in the Chemical Formula 2, R25 and R28 are each independently hydrogen, a C1 to C20 alkyl group, or a C2 to C20 alkoxyalkyl group,
Q3 and Q4 are independently a C1 to C20 alkyl group or a C2 to C20 alkoxyalkyl group, X3 and X4 are each independently halogen, and M2 is Ti, Zr or Hf.