# US 2021/0331968 A1 · Process for providing a corrosion resistant coated glass substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0331968 A1
- Document ID: US20210331968A1
- Status: Published application
- Kind: A1
- Application number: 17/372,738
- Filed: 2021-07-12
- Published: 2021-10-28
- Earliest claimed: 2016-04-26
- Assignees: Pilkington Group Limited
- Applicants: Pilkington Group Limited
- Inventors: SIMON JAMES HURST; KARIKATH SUKUMAR VARMA; ANNA LOUISE COLLEY; KIERAN JAMES CHEETHAM; PETER MICHAEL HARRIS; SIMON PAUL OLIVER
- Web page: https://patentgrep.com/patent/US20210331968A1

## CPC

- C03C 17/25: by deposition from the liquid phase
- A47K 3/30: Screens or {collapsible} cabinets {for showers or baths (A47K3/283 takes precedence)}
- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- C03C 17/30: with silicon-containing compounds
- C03C 2217/213: SiO2
- C03C 2217/78: Coatings specially designed to be durable, e.g. scratch-resistant
- C03C 2218/116: by spin-coating, centrifugation
- C03C 2218/32: After-treatment
- C03C 2218/365: Coating different sides of a glass substrate
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- A47K: SANITARY EQUIPMENT; ACCESSORIES THEREFOR, e.g. TOILET ACCESSORIES

## Abstract

A corrosion-resistant coated glass substrate suitable for use in a humid environment and a process for producing same, the process comprising providing a soda lime silica glass substrate, providing a liquid coating composition comprising a polysilazane at a concentration of between 0.5% and 80% by weight, contacting one or both surfaces of the glass substrate directly with the coating composition, and curing the coating composition thereby forming a corrosion-resistant coated glass substrate having a silica layer on one or both sides of the glass substrate with a thickness of from 12 nm to 300 nm.

## Claims

### Claim 1

A process for producing a corrosion-resistant coated glass substrate suitable for use in a humid environment, the process comprising:
i) providing a soda lime silica glass substrate;
ii) providing a liquid coating composition comprising a polysilazane at a concentration of between 0.5% and 80% by weight;
iii) contacting one or both surfaces of the glass substrate directly with the coating composition; and
iv) curing the coating composition thereby forming a corrosion-resistant coated glass substrate having a silica layer on one or both sides of the glass substrate with a thickness of from 12 nm to 300 nm.

### Claim 2 (depends on 1)

A process according to claim 1 wherein the silica layer or each silica layer comprises 95% or more silica in the form of SiO2, more preferably the silica layer or each silica layer comprises 97% or more silica in the form of SiO2.

### Claim 3 (depends on 1)

A process according to claim 1 wherein the silica layer or each silica layer comprises 98% or more silica in the form of SiO2.

### Claim 4 (depends on 1)

A process according to claim 1 wherein the silica layer or each silica layer comprises a continuous film.

### Claim 5 (depends on 1)

A process according to claim 1 wherein the silica layer or each silica layer comprises a non-porous film.

### Claim 6 (depends on 1)

A process according to claim 1, wherein the corrosion-resistant coated glass substrate exhibits a haze increase of 24% or below after 50 days at 98% relative humidity and 60° C.

### Claim 7 (depends on 1)

A process according to claim 1, wherein the silica layer, or each silica layer has a thickness of: 15 nm or higher; preferably 20 nm or higher; more preferably 25 nm or higher; and most preferably 75 nm or higher.

### Claim 8 (depends on 1)

A process according to claim 1, wherein the silica layer or each silica layer has a thickness: 280 nm or lower; more preferably 260 nm or lower.

### Claim 9

A process according to claim, wherein the silica layer or each silica layer has a thickness in the range: 15 nm to 300; preferably 20 nm to 300 nm; more preferably 20 nm to 280 nm; and most preferably 20 nm to 250 nm.

### Claim 10 (depends on 1)

A process according to claim 1 wherein the silica layer or each silica layer has a refractive index in the range 1.42 to 1.55.

### Claim 11 (depends on 1)

A process according to claim 1, wherein the silica layer or each silica layer comprises nitrogen in an amount of 5% or less, more preferably the silica layer or each silica layer comprises nitrogen in an amount of 3% or less.

### Claim 12 (depends on 1)

A process according to claim 1, wherein the silica layer or each silica layer comprises nitrogen in an amount of 2% or less.

### Claim 13 (depends on 1)

A process according to claim 1, wherein the silica layer is deposited directly on each surface of the glass substrate.

### Claim 14 (depends on 13)

A process as claimed in claim 13, wherein the silica layer deposited directly on each surface of the glass substrate comprises a thickness of 20 nm to 200 nm.

### Claim 15 (depends on 1)

A process according to claim 1, wherein the glass substrate is toughened glass.

### Claim 16 (depends on 1)

A process according to claim 1, wherein the silica layer or each silica layer is/are the only coating on the glass substrate.

### Claim 17 (depends on 1)

A process according to claim 1, wherein the silica layer or each silica layer is/are undoped.

### Claim 18 (depends on 1)

A process according to claim 1, wherein the silica layer on one or each surface of the glass substrate comprises 97% or more silica in the form of SiO2; and wherein the silica layer on one or each surface of the glass substrate has a thickness of 75 nm or higher and a thickness of less than 144 nm.

### Claim 19 (depends on 1)

A process according to claim 1 wherein the coating composition is cured using a predetermined curing temperature and/or ultraviolet radiation.

### Claim 20 (depends on 1)

A process according to claim 1, wherein the liquid coating composition comprises a solvent, preferably an aprotic solvent, more preferably dialkyl ether.

### Claim 21 (depends on 1)

A process according to claim 1, wherein the polysilazane is a compound of formula [R1R2Si—NR]n, wherein one of R1, R2, and R3 are each independently selected from H or C1 to C4 alkyl, and n is an integer.

### Claim 22 (depends on 21)

A process as claimed in claim 21, wherein the polysilazane comprises perhydropolysilazane.

### Claim 23 (depends on 1)

A process according to claim 1, wherein the or both surfaces of the glass substrate is/are contacted directly with the coating composition by a method selected from: dip coating, spin coating, roller coating, spray coating, air atomisation spraying, ultrasonic spraying, and/or slot-die coating.

### Claim 24 (depends on 23)

A process as claimed in claim 23, further comprising cleaning one or both surfaces of the glass substrate before depositing the coating composition.

### Claim 25 (depends on 24)

A process as claimed in claim 24, wherein cleaning the glass substrate surfaces comprises treatment with one or more of: abrasion with ceria; washing with alkaline aqueous solution; washing with deionised water rinse; and/or plasma treatment.

### Claim 26 (depends on 19)

A process according to claim 19, wherein the predetermined curing temperature is a temperature of 130° C. or higher, preferably a temperature in the range 130° C. to 650° C. or 150° C. to 550° C., and more preferably a temperature in the range 250° C. to 520° C.

### Claim 27 (depends on 19)

A process according to claim 19, wherein the ultraviolet radiation used to cure the coating composition applied directly to one or both surfaces of the glass substrate comprises UV C radiation.

### Claim 28 (depends on 1)

A process according to claim 1, wherein the polysilazane is at a concentration in the range 0.5% to 20% by weight in the coating composition, preferably in the range 0.5% to 10% by weight, more preferably in the range 1% to 5% by weight.

### Claim 29

A process for producing a corrosion-resistant coated glass substrate suitable for use in a humid environment, the process comprising:
i) providing a soda lime silica glass substrate;
ii) providing a liquid coating composition comprising a polysilazane at a concentration of between 0.5% and 80% by weight;
iii) contacting one or both surfaces of the glass substrate directly with the coating composition; and
iv) curing the coating composition thereby forming a corrosion-resistant coated glass substrate having a silica layer on one or both sides of the glass substrate, wherein
v) the silica layer on one or each surface of the glass substrate comprises 97% or more silica in the form of SiO2; and wherein
vi) the silica layer on one or each surface of the glass substrate comprises a fully-densified, continuous, non-porous film.

### Claim 30

A process for producing a corrosion-resistant coated glass substrate suitable for use in a humid environment, the process comprising:
i) providing a soda lime silica glass substrate;
ii) providing a liquid coating composition comprising a polysilazane at a concentration of between 0.5% and 80% by weight;
iii) contacting one or both surfaces of the glass substrate directly with the coating composition; and
iv) curing the coating composition thereby forming a corrosion-resistant coated glass substrate having a silica layer on one or both sides of the glass substrate, wherein
v) the silica layer on one or each surface of the glass substrate comprises 97% or more silica in the form of SiO2; and wherein
vi) the silica layer on one or each surface of the glass substrate comprises a fully-densified, continuous, non-porous film, and
vii) the silica layer on one or each surface of the glass substrate has a thickness of 75 nm or higher and a thickness of less than 144 nm.