# US 2021/0331452 A1 · Breathable and waterproof membrane and method for manufacturing the same, and breathable and waterproof fabric

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0331452 A1
- Document ID: US20210331452A1
- Status: Published application
- Kind: A1
- Application number: 17/237,060
- Filed: 2021-04-22
- Published: 2021-10-28
- Earliest claimed: 2020-04-24
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: TE-CHAO LIAO; CHING-YAO YUAN; WEN-JUI CHENG; Chih-Feng Wang
- Web page: https://patentgrep.com/patent/US20210331452A1

## CPC

- B29D 99/005: {Producing membranes}
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 3/266: {characterised by an apertured layer, the apertures going through the whole thickness of the layer, e.g. expanded metal, perforated layer, slit layer regular cells B32B3/12}
- B32B 5/02: characterised by structural features of a {fibrous or filamentary} layer {(layer formed of metallic wires B32B15/02; layer formed of natural mineral fibres B32B19/02; layer formed of wood fibres B32B21/02)}
- B32B 5/024: {Woven fabric}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/08: of synthetic resin
- B32B 27/20: using fillers, pigments, thixotroping agents
- B32B 27/205: {the fillers creating voids or cavities, e.g. by stretching}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/34: comprising polyamides
- B32B 37/156: {at least one layer is calendered and immediately laminated}
- B32B 38/0012: {Mechanical treatment, e.g. roughening, deforming, stretching}
- B32B 37/1284: {Application of adhesive}
- B32B 2038/0028: {Stretching, elongating}
- B32B 2262/0253: Polyolefin fibres
- B32B 2264/10: Inorganic particles
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/558: Impact strength, toughness
- B32B 2307/72: Density
- B32B 2307/724: Permeability to gases, adsorption
- B32B 2307/7265: Non-permeable
- B32B 2307/732: Dimensional properties
- B32B 2437/00: Clothing
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

A breathable and waterproof membrane and a method for manufacturing the same, and a breathable and waterproof fabric are provided. The breathable and waterproof membrane is formed by stretching a polyolefin material. The breathable and waterproof membrane has a density ranging from 0.6 g/cm3 to 0.8 g/cm3. A plurality of micropores are formed on the breathable and waterproof membrane, and the plurality of micropores each has a size smaller than 500 nm. The polyolefin material includes: 60 wt % to 80 wt % of a first polypropylene resin, 15 wt % to 30 wt % of a second polypropylene resin, and 1 wt % to 10 wt % of inorganic particles. The second polypropylene resin is a modified polypropylene resin having a hydrophilic group. The second polypropylene resin is different from the first polypropylene resin.

## Claims

### Claim 1

A breathable and waterproof membrane, having a density ranging from 0.6 g/cm3 to 0.8 g/cm3, wherein a plurality of micropores each having a size smaller than 500 nm are formed on the breathable and waterproof membrane, a polyolefin material is stretched to form the breathable and waterproof membrane, and the polyolefin material includes:
60 wt % to 80 wt % of a first polypropylene resin;
15 wt % to 30 wt % of a second polypropylene resin that is a modified polypropylene resin having a hydrophilic group, the second polypropylene resin being different from the first polypropylene resin; and
1 wt % to 10 wt % of inorganic particles.

### Claim 2 (depends on 1)

The breathable and waterproof membrane according to claim 1, wherein the first polypropylene resin includes a propylene homopolymer as a main material, and the first polypropylene resin selectively includes an ethylene compound, a propylene compound, a butylene compound, an ethylene homopolymer, a butylene homopolymer, an ethylene/propylene copolymer, an ethylene/butylene copolymer, a propylene/butylene copolymer, an ethylene/propylene/butylene copolymer, or any combination thereof.

### Claim 3 (depends on 1)

The breathable and waterproof membrane according to claim 1, wherein a thickness of the breathable and waterproof membrane ranges from 15 μm to 50 μm, the breathable and waterproof membrane has a hydrostatic pressure resistance ranging from 10000 mmH2O to 20000 mmH2O and a moisture permeability ranging from 5000 g/m2/24 hours to 20000 g/m2/24 hours.

### Claim 4 (depends on 1)

The breathable and waterproof membrane according to claim 1, wherein particle sizes of the inorganic particles range from 0.05 μm to 2 μm.

### Claim 5 (depends on 1)

The breathable and waterproof membrane according to claim 1, wherein the hydrophilic group of the second polypropylene resin is at least one selected from the group consisting of: a hydroxyl group, a carboxylic acid group, an amide group, and an amino group.

### Claim 6

A breathable and waterproof membrane, having a density ranging from 0.6 g/cm3 to 0.8 g/cm3, wherein a plurality of micropores each having a size smaller than 500 nm are formed on the breathable and waterproof membrane, the breathable and waterproof membrane includes:
a first surface layer formed from a first material which includes 60 wt % to 80 wt % of a first polypropylene resin and 20 wt % to 40 wt % of a second polypropylene resin;
a middle layer formed from a middle material which includes 60 wt % to 80 wt % of the first polypropylene resin, 15 wt % to 30 wt % of the second polypropylene resin, and 5 wt % to 10 wt % of inorganic particles; and
a second surface layer formed from a second material which includes 60 wt % to 80 wt % of the first polypropylene resin and 20 wt % to 40 wt % of the second polypropylene resin;
wherein the middle layer is formed between the first surface layer and the second surface layer;
wherein the second polypropylene resin is a modified polypropylene resin having a hydrophilic group, and the second polypropylene resin is different from the first polypropylene resin;
wherein, based on a total weight of the first material, the middle material, and the second material being 100 wt %, an amount of the inorganic particles ranges from 1 wt % to 10 wt %.

### Claim 7 (depends on 6)

A breathable and waterproof fabric, comprising the breathable and waterproof membrane according to claim 6 and a fiber cloth, wherein the breathable and waterproof membrane is disposed on the fiber cloth, and a material of the fiber cloth is polyolefin.

### Claim 8 (depends on 7)

The breathable and waterproof fabric according to claim 7, wherein the breathable and waterproof membrane is disposed onto the fiber cloth through coating, lamination, or encapsulation.

### Claim 9

A method for manufacturing a breathable and waterproof membrane, comprising:
providing a polyolefin material which includes 60 wt % to 80 wt % of a first polypropylene resin, 15 wt % to 30 wt % of a second polypropylene resin, and 1 wt % to 10 wt % of inorganic particles; wherein the second polypropylene resin is a modified polypropylene resin having a hydrophilic group, and the second polypropylene resin is different from the first polypropylene resin;
calendering the polyolefin material to form a polyolefin sheet; and
stretching the polyolefin sheet to form the breathable and waterproof membrane which has a density ranging from 0.6 g/cm3 to 0.8 g/cm3, wherein a plurality of micropores each having a size smaller than 500 nm are formed on the breathable and waterproof membrane.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the step of stretching the polyolefin sheet further includes stretching the polyolefin sheet in a machine direction (MD) and in a transverse direction (TD), a stretching magnification in the MD ranges from 2.5 to 5.0, and a stretching magnification in the TD ranges from 6.0 to 10.0.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the polyolefin sheet is stretched in the MD and stretched in the TD sequentially or simultaneously.