# US 2021/0331272 A1 · Method of forming a single, angled and hourglass shaped weld

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0331272 A1
- Document ID: US20210331272A1
- Status: Published application
- Kind: A1
- Application number: 16/860,702
- Filed: 2020-04-28
- Published: 2021-10-28
- Earliest claimed: 2020-04-28
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Huaxin Li; Liang Wang; Stephen R. McKenny; Daniel J. Wilson
- Web page: https://patentgrep.com/patent/US20210331272A1

## CPC

- B23K 26/035: Aligning the laser beam (automatically B23K26/042)
- B23K 26/062: by direct control of the laser beam
- B23K 26/0622: by shaping pulses
- B23K 26/0665: {by beam condensation on the workpiece, e.g. for focusing}
- B23K 26/08: Devices involving relative movement between laser beam and workpiece
- B23K 26/123: {in an atmosphere of particular gases}
- B23K 26/242: Fillet welding, i.e. involving a weld of substantially triangular cross section joining two parts
- B23K 26/282: of tube sections
- B23K 26/32: taking account of the properties of the material involved
- B23K 26/323: involving parts made of dissimilar metallic material
- B23K 26/60: Preliminary treatment
- B23K 33/006: {for cylindrical workpieces}
- B23K 2101/006: {Vehicles}
- B23K 2101/008: {Gears}
- B23K 2103/04: Steel {or steel} alloys
- B23K 2103/05: {Stainless steel}
- B23K 2103/18: Dissimilar materials
- H05B 6/10: Induction heating apparatus, other than furnaces, for specific applications
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL

## Abstract

Angled, single laser weld and a method of forming an angled, single laser weld including arranging a first and second faying surfaces of a first and second component adjacently to form an interface between the components; irradiating at least one of the first and second components at the interface with a laser, wherein the first faying surface defines a plane formed at an angle alpha in the range of +1-5 degrees to 60 degrees from an axis A perpendicular to the first front surface and the second faying surface matches the first faying surface; and forming a junction at the interface with an hourglass shaped weld.

## Claims

### Claim 1

A method of welding components, comprising:
arranging a first faying surface of a first component and a second faying surface of a second component adjacently to define an interface between the first component and the second component, wherein the first component includes a first front surface and a first back surface opposing the first front surface, and the second component includes a second front surface and a second back surface opposing the second front surface;
irradiating at least one of a) the first front surface of the first component and b) the second front surface of the second component at the interface with a laser, wherein the first faying surface defines a plane formed at an angle alpha in the range of +/−5 degrees to 60 degrees from an axis A perpendicular to the first front surface and the second faying surface matches the first faying surface;
melting the first faying surface and second faying surface and forming a melt pool at the interface; and
forming a junction at the interface with an hourglass shaped weld.

### Claim 2 (depends on 1)

The method of claim 1, wherein the laser defines a center axis and the center axis of the laser deviates from the plane defined by the first faying surface at an angle beta in the range of +/−0.1 degrees to 5 degrees.

### Claim 3 (depends on 1)

The method of claim 1, further comprising adjusting a carbon equivalent of the hourglass shaped weld by adjusting an incident angle of laser as defined by a center axis of the laser.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first component exhibits a first ideal diameter and the second component exhibits a second ideal diameter, wherein the first ideal diameter is smaller than the second ideal diameter.

### Claim 5 (depends on 4)

The method of claim 4, wherein a center axis defined by the laser is tilted at an angle in the range of 5 to 35 degrees from the axis perpendicular to the first component.

### Claim 6 (depends on 1)

The method of claim 1, further comprising focusing the laser at a focal point between the first front surface and the first back surface at a distance in the range of 35 percent to 65 percent of a thickness of the first component, wherein the thickness is measured perpendicular to the first front surface.

### Claim 7 (depends on 1)

The method of claim 1, further comprising operating the laser at a spot size in the range of 200 to 600 micrometers.

### Claim 8 (depends on 1)

The method of claim 1, wherein the laser further comprises a center axis and further comprising offsetting the center axis from the interface and towards the first component at a distance in the range of 0.05 mm to 0.8 mm.

### Claim 9 (depends on 1)

The method of claim 1, further comprising operating the laser at a power in the range of 2 kW to 6 kW.

### Claim 10 (depends on 1)

The method of claim 1, further comprising operating the laser at a weld speed in the range of 1.00 meters per minute to 3.00 meters per minute.

### Claim 11 (depends on 1)

The method of claim 1, further comprising preheating the interface at the first back surface and the second back surface to a temperature in the range of 100° C. to 180° C.

### Claim 12 (depends on 11)

The method of claim 11, further comprising preheating by at least one of the following: induction heating and heating with a defocused laser.

### Claim 13 (depends on 1)

The method of claim 1, further comprising defining a notch in at least one of the a) first back surface and the first faying surface and b) the second back surface and the second faying surface and a portion of the melt pool flows into the notch.

### Claim 14 (depends on 1)

The method of claim 1, further comprising applying an inert gas at the interface of the first back surface and the second back surface.

### Claim 15 (depends on 1)

The method of claim 1, further comprising forming only one hourglass shaped weld at the junction.

### Claim 16 (depends on 1)

The method of claim 1, forming the hourglass shaped weld to exhibit a weld surface length to weld midpoint length ratio in the range of 1:1 to 2.0:1.

### Claim 17 (depends on 1)

The method of claim 1, forming the hourglass shaped weld to exhibit a weld root length to weld midpoint length ratio in the range of 1:1 to 2.0:1.

### Claim 18 (depends on 1)

The method of claim 1, wherein the first component is a circular gear and defines a center axis and the angle alpha of the plane deviates +/−10 degrees to 30 degrees from the center axis.

### Claim 19

A welded part, comprising:
a first component and a second component fused together at a junction; and
an hourglass shaped weld formed at the junction, wherein the hourglass shaped weld defines a plane that is at an angle gamma in the range of +/−5 degrees to 60 degrees from an axis perpendicular to a first front surface of the first component and wherein the hourglass shaped weld exhibits a surface length to midpoint length ratio in the range of 1 to 2.0:1 and the hourglass shaped weld exhibits a root length to midpoint length ratio in the range of 1 to 2.0:1.

### Claim 20 (depends on 19)

The welded part of claim 19, wherein the first component includes a gear and the second component includes a flange.