# US 2021/0331247 A1 · Method of producing additively manufactured object and additively manufactured object

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0331247 A1
- Document ID: US20210331247A1
- Status: Published application
- Kind: A1
- Application number: 17/235,214
- Filed: 2021-04-20
- Published: 2021-10-28
- Earliest claimed: 2020-04-28
- Assignees: Mitsubishi Heavy Industries, Ltd.
- Applicants: Mitsubishi Heavy Industries, Ltd.
- Inventors: Takahiro TACHIBANA; Noriyuki HIRAMATSU; Tomoko TAMURA
- Web page: https://patentgrep.com/patent/US20210331247A1

## CPC

- B22F 10/64: by thermal means (control of energy beam parameters for post heating B22F10/364)
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/007: {containing Co}
- C21D 6/04: Hardening by cooling below 0 degrees Celsius
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- C22C 38/06: containing aluminium
- C22C 38/105: {containing Co and Ni}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- B22F 2301/052: Aluminium
- B22F 2301/15: Nickel or cobalt
- B22F 2301/205: Titanium, zirconium or hafnium
- B22F 2301/35: Iron
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2998/10: Processes characterised by the sequence of their steps
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of producing an additively manufactured object comprises: a step of cooling a shaped body of an alloy formed by additive manufacturing to 0° C. or lower; and a step of aging the shaped body under a temperature condition of 400° C. or higher and 600° C. or lower after the step of cooling the shaped body. The alloy contains: Fe as a main component; 17.0 mass % or more and 19.0 mass % or less of Ni; 7.0 mass % or more and 12.5 mass % or less of Co; 4.6 mass % or more and 5.2 mass % or less of Mo; 0.13 mass % or more and 1.6 mass % or less of Ti; and 0.05 mass % or more and 0.15 mass % or less of Al.

## Claims

### Claim 1

A method of producing an additively manufactured object, comprising:
a step of cooling a shaped body of an alloy formed by additive manufacturing to 0° C. or lower; and
a step of aging the shaped body under a temperature condition of 400° C. or higher and 600° C. or lower after the step of cooling the shaped body,
wherein the alloy contains:
Fe as a main component;
17.0 mass % or more and 19.0 mass % or less of Ni;
7.0 mass % or more and 12.5 mass % or less of Co;
4.6 mass % or more and 5.2 mass % or less of Mo;
0.13 mass % or more and 1.6 mass % or less of Ti; and
0.05 mass % or more and 0.15 mass % or less of Al.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein the step of cooling the shaped body is performed after formation of the shaped body without solution treatment of the shaped body.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein the step of cooling the shaped body includes cooling the shaped body to −130° C. or lower, or −160° C. or lower.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein the alloy contains:
Fe as a main component;
18.0 mass % or more and 19.0 mass % or less of Ni;
8.5 mass % or more and 12.5 mass % or less of Co;
4.6 mass % or more and 5.2 mass % or less of Mo;
0.5 mass % or more and 1.6 mass % or less of Ti; and
0.05 mass % or more and 0.15 mass % or less of Al.

### Claim 5

An additively manufactured object, made of an alloy,
wherein the alloy contains:
Fe as a main component;
17.0 mass % or more and 19.0 mass % or less of Ni;
7.0 mass % or more and 12.5 mass % or less of Co;
4.6 mass % or more and 5.2 mass % or less of Mo;
0.13 mass % or more and 1.6 mass % or less of Ti; and
0.05 mass % or more and 0.15 mass % or less of Al, and
wherein the additively manufactured object has a Vickers hardness of 535 Hv or more.

### Claim 6 (depends on 5)

The additively manufactured object according to claim 5,
wherein a content of retained austenite is less than 2 vol %.

### Claim 7 (depends on 5)

The additively manufactured object according to claim 5,
wherein the additively manufactured object is an aggregate of beads of the alloy.

### Claim 8 (depends on 7)

The additively manufactured object according to claim 7,
wherein each of the beads has a cross-sectional area of 0.25 mm2 or more and 20 mm2 or less.

### Claim 9 (depends on 7)

The additively manufactured object according to claim 7,
wherein each of the beads has a width of 1 mm or more and 15 mm or less.

### Claim 10 (depends on 5)

The additively manufactured object according to claim 5, which has a 0.2% proof stress of 1860 MPa or more.

### Claim 11 (depends on 5)

The additively manufactured object according to claim 5, which has a tensile strength of 1900 MPa or more.