# US 2021/0331235 A1 · Powder bed materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0331235 A1
- Document ID: US20210331235A1
- Status: Published application
- Kind: A1
- Application number: 16/605,423
- Filed: 2018-06-08
- Published: 2021-10-28
- Earliest claimed: 2018-06-08
- Assignees: Hewlett-Packard Development Company, L.P.
- Applicants: Hewlett-Packard Development Company, L.P.
- Inventors: John Samuel Dilip Jangam; Thomas Anthony; Krzysztof Nauka; Kristopher J. Erickson
- Web page: https://patentgrep.com/patent/US20210331235A1

## CPC

- B22F 10/14: by jetting of binder onto a bed of metal powder
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/142: Thermal or thermo-mechanical treatment
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- B22F 3/10: Sintering only
- B22F 9/18: with reduction of metal compounds
- B22F 2009/043: {by ball milling}
- B22F 2207/11: Gradients other than composition gradients, e.g. size gradients
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B29C 64/165: using a combination of solid and fluid materials, e.g. a powder selectively bound by a liquid binder, catalyst, inhibitor or energy absorber
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A powder bed material can include from 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm. From 10 wt % to 100 wt % of the metal particles can be surface-activated metal particles having in intact inner volume and an outer volume with structural defects. The structural defects can exhibit an average surface grain density of 50,000 to 5,000,000 per mm2.

## Claims

### Claim 1

A powder bed material, comprising 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm, wherein 10 wt % to 100 wt % of the metal particles are surface-activated metal particles having in intact inner volume and an outer volume with structural defects, and wherein the structural defects exhibit an average surface grain density of 50,000 to 5,000,000 per mm2.

### Claim 2 (depends on 1)

The powder bed material of claim 1, wherein the metal particles are elemental metals or alloys of aluminum, titanium, copper, cobalt, chromium, nickel, vanadium, tungsten, tungsten carbide, tantalum, molybdenum, magnesium, gold, silver, iron, stainless-steel, steel, or an admixture thereof.

### Claim 3 (depends on 1)

The powder bed material of claim 1, wherein structural defects are introduced by ball milling with a 50 μm to 500 μm milling beads harder than the metal particles suspended in an aliphatic oil at a milling speed of 400 RPM to 1000 RPM for 10 minutes to 24 hours.

### Claim 4 (depends on 1)

The powder bed material of claim 1, wherein the structural defects are introduced by flash heating the metal particles with from 1 to 10 pulses of light energy at from 15 J/cm2 to 50 J/cm2.

### Claim 5 (depends on 1)

The powder bed material of claim 1, wherein the structural defects are introduced by flash heating and exhibit an average surface grain density of 60,000 mm2 to 120,000 per mm2.

### Claim 6 (depends on 1)

The powder bed material of claim 1, wherein the structural defects are introduced by ball milling and exhibit an average surface grain density of 80,000 mm2 to 2,000,000 per mm2.

### Claim 7

A material set, comprising:
a powder bed material, comprising 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm, wherein 10 wt % to 100 wt % of the metal particles are surface-activated metal particles having in intact inner volume and an outer volume with structural defects, and wherein the structural defects exhibit an average surface grain density of 50,000 to 5,000,000 per mm2; and
a binder fluid to adhere a first portion of the powder bed material relative to a second portion of the powder bed material not in contact with the fluid.

### Claim 8 (depends on 7)

The material set of claim 7, wherein the binder fluid includes water and a polymer binder or a polymerizable binder.

### Claim 9 (depends on 7)

The material set of claim 7, wherein the binder fluid is stable at room temperature, and includes water, dispersed metal oxide nanoparticles, and a reducing agent to reduce the dispersed metal oxide nanoparticles when heat is applied to the binder fluid.

### Claim 10 (depends on 7)

The material set of claim 7, wherein structural defects are introduced by ball milling with a 50 μm to 500 μm milling beads harder than the metal particles suspended in an aliphatic oil at a milling speed of 400 RPM to 1000 RPM for 10 minutes to 24 hours.

### Claim 11 (depends on 7)

The material set of claim 7, wherein the structural defects are introduced by flash heating the metal particles with from 1 to 10 pulses of light energy at from 15 J/cm2 to 50 J/cm2.

### Claim 12 (depends on 7)

The material set of claim 7, wherein the average surface grain density is from 80,000 mm2 to 2,000,000 per mm2.

### Claim 13

A method of three-dimensional printing, comprising:
spreading a powder bed material to form a powder layer having a thickness of from 20 μm to 400 μm, wherein the powder bed material includes 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm, wherein 10 wt % to 100 wt % of the metal particles are surface-activated metal particles having in intact inner volume and an outer volume with structural defects, and wherein the structural defects exhibit an average surface grain density of 50,000 to 5,000,000 per mm2;
selectively binding a first portion of the powder bed material to form a green layer within the powder layer; and
building up additional green layers by sequentially repeating the spreading and the selectively binding of the powder bed material until a green three-dimensional object is formed.

### Claim 14 (depends on 13)

The method of claim 13, further comprising heat fusing the green three-dimensional object to sinter or anneal the metal particles together.

### Claim 15 (depends on 14)

The method of claim 14, wherein the heat fusing starts at a temperature from 0.6 to 0.8 of the melting temperature of the metal particles.