# US 2021/0331040 A1 · Tpu ball structure and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0331040 A1
- Document ID: US20210331040A1
- Status: Published application
- Kind: A1
- Application number: 17/238,171
- Filed: 2021-04-22
- Published: 2021-10-28
- Earliest claimed: 2020-04-24
- Assignees: San Fang Chemical Industry Co., Ltd.
- Applicants: San Fang Chemical Industry Co., Ltd.
- Inventors: CHIH-YI LIN; KUO-KUANG CHENG; CHI-CHIN CHIANG; WEN-HSIN TAI
- Web page: https://patentgrep.com/patent/US20210331040A1

## CPC

- A63B 41/08: Ball covers; Closures therefor
- A63B 41/02: Bladders
- A63B 41/10: Bladder and cover united
- A63B 45/00: Apparatus or methods for manufacturing balls (working of plastics or substances in a plastic state B29)
- B29C 48/08: flexible, e.g. films
- B29C 48/365: using pumps, e.g. piston pumps
- B29C 48/914: {Cooling drums}
- B29C 53/564: {for making non-tubular articles (for winding of reinforced articles having a non-circular cross-section followed by compression B29C70/347)}
- B29C 65/02: by heating, with or without pressure
- B29D 22/04: Spherical articles, e.g. balls (B29D22/02 takes precedence)
- B32B 1/00: Layered products having a non-planar shape
- B32B 5/02: characterised by structural features of a {fibrous or filamentary} layer {(layer formed of metallic wires B32B15/02; layer formed of natural mineral fibres B32B19/02; layer formed of wood fibres B32B21/02)}
- B32B 5/18: characterised by features of a layer {of} foamed material
- B32B 25/10: next to a fibrous or filamentary layer
- B32B 25/12: comprising natural rubber
- B32B 27/065: {of foam}
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 27/40: comprising polyurethanes
- D01D 5/16: using rollers, or like mechanical devices, e.g. snubbing pins
- D01F 6/70: from polyurethanes
- A63B 2209/00: Characteristics of used materials
- B29K 2075/00: Use of {PU, i.e.} polyureas or polyurethanes {or derivatives thereof}, as moulding material
- B32B 2250/03: 3 layers
- B32B 2262/0292: Polyurethane fibres
- B32B 2274/00: Thermoplastic elastomer material
- B32B 2307/51: Elastic
- B32B 2307/732: Dimensional properties
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present disclosure is relates to a TPU ball structure and a manufacturing method thereof. The TPU ball structure includes a ball bladder layer, a yarn layer and a surface layer. The ball bladder layer is made of TPU material. The yarn layer is made of TPU material, and the yarn layer is disposed to cover the ball bladder layer. The surface layer is made of TPU material, and the surface layer is disposed to cover the yarn layer. The above layers of the TPU ball structure are made of TPU material to satisfy a requirement for environmental protection, and are recyclable. There is no need to use adhesive to adhere the above layers of the TPU ball structure. Therefore, the peeling strength between the layers of the TPU ball structure can be increased so that the whole peeling strength of the TPU ball structure can be increased.

## Claims

### Claim 1

A TPU ball structure, comprising:
a ball bladder layer, made of a thermoplastic polyurethane (TPU) material;
a yarn layer, made of a TPU material and disposed to cover the ball bladder layer; and
a surface layer, made of a TPU material and disposed to cover the yarn layer.

### Claim 2 (depends on 1)

The TPU ball structure of claim 1, wherein the TPU yarn is wound to cover the ball bladder layer.

### Claim 3 (depends on 1)

The TPU ball structure of claim 1, wherein the yarn layer is made of TPU winding yarn or TPU hot melt yarn.

### Claim 4 (depends on 1)

The TPU ball structure of claim 1, wherein the surface layer comprises an outer surface layer and a latex layer.

### Claim 5 (depends on 4)

The TPU ball structure of claim 4, wherein the latex layer comprises a foamed latex layer and an unfoamed latex layer, the foamed latex layer is disposed on the unfoamed latex layer, and the outer surface layer is disposed on the foamed latex layer.

### Claim 6 (depends on 5)

The TPU ball structure of claim 5, wherein the thickness composite ratio of the outer surface layer to the foamed latex layer to the unfoamed latex layer is 1:8:1.

### Claim 7 (depends on 5)

The TPU ball structure of claim 5, wherein the thickness of the outer surface layer is 0.1-0.3 mm, the thickness of the foamed latex layer is 0.4-1.6 mm, and the thickness of the unfoamed latex layer is 0.1-0.3 mm.

### Claim 8 (depends on 1)

The TPU ball structure of claim 1, wherein the ball bladder layer comprises a first high-resilience TPU layer, a high-airtightness TPU layer and a second high-resilience TPU layer, the high-airtightness TPU layer is disposed on the second high-resilience TPU layer, and the first high-resilience TPU layer is disposed on the high-airtightness TPU layer.

### Claim 9 (depends on 8)

The TPU ball structure of claim 8, wherein the thickness composite ratio of the first high-resilience TPU layer to the high-airtightness TPU layer to the second high-resilience TPU layer is 1:2:1.

### Claim 10

A manufacturing of a TPU ball structure, comprising:
making a ball bladder layer by using a TPU material;
covering the ball bladder layer by a TPU yarn to form a yarn layer;
making a surface layer by using a TPU material; and
covering the yarn layer by the surface layer and hot-working treatment.

### Claim 11 (depends on 10)

The manufacturing method of claim 10, wherein the step of making the ball bladder layer comprises a step of preparing TPU pellets with the viscosity of 0.5-2 and drying by a drying cylinder so that the moisture content of the TPU pellets is 20-50 ppm, by using a melt-spinning process, the dried TPU pellets are transported to an extruder, melted and transported to a metering pump, and transported to a spinning assembly through the metering pump to eject a TPU filament, the TPU filament is then cooled by cooling air at the temperature of 10-50° C., drawn by drawing rollers, and wound by a winder to obtain a 200-500 den TPU long fiber, the TPU long fiber is subjected to a ball bladder process to obtain the ball bladder layer.

### Claim 12 (depends on 10)

The manufacturing method of claim 10 wherein the step of making the ball bladder layer comprises a step of making a first high-resilience TPU layer, a high-airtightness TPU layer and a second high-resilience TPU layer, TPU particles are dried by a first dryer so that the moisture content is 300 ppm or below, and the TPU pellets are melted by a first extruder, the melting temperature of the first extruder is 160° C.-180° C., the DIE temperature is 180° C., and the first high-resilience TPU layer is made through a first metering pump.

### Claim 13 (depends on 12)

The manufacturing method of claim 12, wherein the step of making the ball bladder layer further comprises a step of drying TPU particles by a second dryer so that the moisture content is 300 ppm or below, and the TPU pellets are melted by a second extruder, the melting temperature of the second extruder is 160° C.-190° C., the DIE temperature is 180° C., and the high-airtightness TPU layer is made through a second metering pump.

### Claim 14 (depends on 13)

The manufacturing method of claim 13, wherein the step of making the ball bladder layer further comprises a step of drying TPU particles by a third dryer so that the moisture content is 300 ppm or below, and the TPU pellets are melted by a third extruder, the melting temperature of the third extruder is 160° C.-180° C., the DIE temperature is 180° C., and the second high-resilience TPU layer is made through a third metering pump.

### Claim 15 (depends on 14)

The manufacturing method of claim 14, wherein the step of making the ball bladder layer further comprises a step of cooling by using a first coating wheel to form a film, the high-airtightness TPU layer is disposed on the second high-resilience TPU layer, and the first high-resilience TPU layer is disposed on the high-airtightness TPU layer, the thickness composite ratio of the first high-resilience TPU layer to the high-airtightness TPU layer to the second high-resilience TPU layer is 1:2:1.

### Claim 16 (depends on 10)

The manufacturing method of claim 10, wherein the step of making the surface layer comprises a step of making an outer surface layer, a foamed latex layer and an unfoamed latex layer, TPU particles are dried with a fourth dryer so that the moisture content is 300 ppm or below, the TPU pellets are melted by a fourth extruder, the melting temperature of the fourth extruder is 185° C.-200° C., the DIE temperature is 185° C., and the outer surface layer is made through a fourth metering pump.

### Claim 17 (depends on 16)

The manufacturing method of claim 16, wherein the step of making the surface layer further comprises a step of drying TPU particles with a fifth dryer so that the moisture content is 300 ppm or below, the TPU pellets are melted by a fifth extruder, and 0.5-5.0% of a microsphere foaming agent is added, the melting temperature of the fifth extruder is 160° C.-190° C., the DIE temperature is 185° C., and the foamed latex layer is made through a fifth metering pump.

### Claim 18 (depends on 17)

The manufacturing method of claim 17, wherein the step of making the surface layer further comprises a step of drying TPU particles with a sixth dryer so that the moisture content is 300 ppm or below, the TPU pellets are melted by a sixth extruder, the melting temperature of the sixth extruder is 160° C.-180° C., the DIE temperature is 185° C., and the unfoamed latex layer is made through a sixth metering pump.

### Claim 19 (depends on 18)

The manufacturing method of claim 18, wherein the step of making the surface layer further comprises a step of cooling by using a second coating wheel to form a film, the foamed latex layer is disposed on the unfoamed latex layer, and the outer surface layer is disposed on the foamed latex layer, the thickness composite ratio of the outer surface layer to the foamed latex layer to the unfoamed latex layer is 1:8:1.