A Method for Enriching Precious Metals from Printed Circuit Board Incineration Ash from Molten Pool by Circulating Chlorination
AssigneeBeijing University of Technology
InventorsDean Pan, Yufeng Wu, Bin Li
Life of this patent
Estimating the term…
Loading patent…
AssigneeBeijing University of Technology
InventorsDean Pan, Yufeng Wu, Bin Li
Estimating the term…
The invention relates to the field of comprehensive recovery of valuable elements such as bromine, base metal and precious metal from incineration ash, especially relates to a method for enriching precious metals from printed circuit board incineration ash by bath smelting-chlorination circulation process. The process mainly comprises pretreatment of the printed circuit board Incineration ash and circulation-chlorination enrichment process for precious metals. The crude copper, crude zinc sulfate, bromine, lead chloride and precious metal enriched slag are obtained. Compared with the traditional process, it realizes the cycle enrichment of precious metals as well as avoids the loss of valuable metals and secondary pollution caused by tail liquid discharge.
1-6. (canceled)
A method for enriching precious metals from printed circuit board incineration ash by bath smelting-chlorination circulation process, comprising the steps of:
A method according to claim 1, wherein the primary roasting step is performed at a roasting temperature range of 200-270° C. and a roasting time range of 1-3 hours.
A method according to claim 1, wherein the secondary roasting step is performed at a roasting temperature range of 400-550° C. and a roasting time range of 0.5-2 hours;
A method according to claim 1, wherein in the chlorination and filtration step of chlorination enrichment process, the chlorination solution further comprises calcium chloride, sodium chloride and 30% hydrochloric acid, wherein the concentration of calcium chloride in the chlorination solution is in the range of 50-100 g/L, the concentration of sodium chloride in the chlorination solution is in the range of 200-300 g/L, the concentration of 30% hydrochloric acid in the chlorination solution is in the range of 200-400 g/L, the ratio between the chlorination solution and the chlorination raw material is 3:1-10:1 Liter:Kilogram, wherein the chlorination temperature is in the range of 65-95° C., and the chlorination time is in the range of 1-4 hours;
A method for enriching precious metals from printed circuit board incineration ash by bath smelting-chlorination circulation process in claim 1 comprising:
A method according to claim 1, comprising:
Dependencies are inferred from the claim text.